1-20 of 364 Search Results for

seam welding

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001365
EISBN: 978-1-62708-173-3
... Abstract Resistance seam welding (RSEW) is a process in which the heat generated by resistance to the flow of electric current in the work metal is combined with pressure to produce a welded seam. This article discusses the various classes of the RSEW process, namely roll spot welding...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005608
EISBN: 978-1-62708-174-0
... Abstract This article describes the process applications, advantages, and limitations of resistance seam welding. The fundamentals of lap seam welding are also reviewed. The article details the types of seam welds, namely, lap seam welds and mash seam welds, and the processing equipment used...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005640
EISBN: 978-1-62708-174-0
... with seam welding. It concludes with a discussion on the welding equipment and other factors associated with resistance spot and seam welding. aluminum alloys copper alloys electrode force low-carbon steel resistance spot welding seam welding stainless steel surface preparation weld lobe weld...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006514
EISBN: 978-1-62708-207-5
... Abstract The resistance welding processes commonly employed for joining aluminum are resistance spot welding, resistance seam welding, resistance roll welding, upset and flash welding for butt joining welding, and high-frequency resistance welding. This article discusses the general factors...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001441
EISBN: 978-1-62708-173-3
...), electron-beam welding (EBW), laser-beam welding (LBW), friction welding (FRW), resistance welding (RW), resistance spot welding (RSW), and resistance seam welding (RSEW). The article reviews the selection of shielding gases and filler metals for welding zirconium alloys. It concludes with a discussion...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001443
EISBN: 978-1-62708-173-3
... Abstract Resistance welding (RW) encompasses a group of processes in which the heat for welding is generated by the resistance to the flow of electrical current through the parts being joined. The three major resistance welding processes are resistance spot welding (RSW), resistance seam...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006510
EISBN: 978-1-62708-207-5
..., and susceptibility to solidification cracking and liquation cracking. It provides an overview on welding processes, including gas metal arc welding, gas tungsten arc welding, resistance spot and seam welding, laser beam welding, and various solid-state welding processes. A review on joint design is also included...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001384
EISBN: 978-1-62708-173-3
... Abstract This article begins with a discussion on the advantages and limitation of ultrasonic welding (USW). It describes variations of the USW process which can produce different weld geometries. These variations are helpful in producing spot welds, line welds, continuous seam welds, ring...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005607
EISBN: 978-1-62708-174-0
... for ultrasonic metal welding. It details the personnel requirements, advantages, limitations, and applications, namely, wire welds, spot welds, continuous seam welds, and microelectronic welds of ultrasonic metal welding. clamping force coalescence continuous seam welds high-frequency vibratory energy...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005625
EISBN: 978-1-62708-174-0
... resistance-welded joints. The various resistance-welded joints include spot welds, projection welds, seam welds, and butt welds. The article explains the relative contributions of the Joule, Peltier, and Thomson effects for typical RW scenarios. It concludes with information on the electrode “follow...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003207
EISBN: 978-1-62708-199-3
... Abstract This article presents a detailed account of the welding parameters, equipment needed, applications, advantages, limitations, and the process variables affecting various types of resistance welding operations, namely, resistance spot welding, resistance seam welding, resistance...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003207
EISBN: 978-1-62708-199-3
...Abstract Abstract This article presents a detailed account of the welding parameters, equipment needed, applications, advantages, limitations, and the process variables affecting various types of resistance welding operations, namely, resistance spot welding, resistance seam welding, resistance...
Book Chapter

Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005126
EISBN: 978-1-62708-186-3
... the tubes as they are produced on the machine. It describes the roll design for tube rolling and reviews the seam welding operations of pipe and tubing. The article discusses cross-sectional tolerances, the reshaping of round tubing, and factors that affect the quality, accuracy, and surface finish...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005583
EISBN: 978-1-62708-174-0
... is applied to produce a forged weld. High-frequency resistance welding is an automated process and is not adaptable to manual welding. High-frequency resistance welding was developed during the late 1940s and early 1950s to fill the need for high-integrity butt joints and seam welds in pipe and tubing...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005129
EISBN: 978-1-62708-186-3
...-welded blanks include: Laser Resistance mash seam High-frequency induction Electron beam (nonvacuum) Friction-stir welding (more recently considered for aluminum TWB) The type of weld joint selected for a specific application depends on a number of factors such as aesthetic...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003425
EISBN: 978-1-62708-195-5
.... Thermoplastic processing equipment Table 3 Thermoplastic processing equipment Process Description Raw material modification Weaving Tape is slit to 0.3 to 0.6 cm (0.1–0.2 in.) wide then woven to create a semidrapable form. Hand seaming/tacking Tape is butted together and seam welded...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005639
EISBN: 978-1-62708-174-0
... at ∼100 µm beam diameter. The moderately modified SEMs and small electron beam welders also have much better beam and/or part motion controls, which are capable of producing actual seam welds, rather than being restricted to spot welds. The situation with respect to laser microwelding is much better...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.9781627081740
EISBN: 978-1-62708-174-0
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005631
EISBN: 978-1-62708-174-0
... requirements on how the weld seam is presented to the laser beam. Some of the important joint geometries are illustrated in Fig. 1 and 2 , and Table 1 summarizes joint selection criteria for a few categories of joint design. Different types of joint design reported for LBW were reviewed by Shewell ( Ref 1...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005680
EISBN: 978-1-62708-198-6
... contact and reduced resistance, which leads to lower heat generated during welding. However, excessive electrode force can result in excessive indentation in work in the workpiece. Figure 6 shows the different types of resistance welding processes, including projection, butt, and seam welding...