Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006795
EISBN: 978-1-62708-295-2
... industries. This article describes the processes involved in erosion of ductile materials, brittle materials, and elastomers. Some examples of erosive wear failures are given on abrasive erosion, liquid impingement erosion, cavitation, and erosion-corrosion. In addition, the article provides information on...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003030
EISBN: 978-1-62708-200-6
... Manufactured Carbon and Graphite Bearing and Seal Materials” ( Ref 15 ), was developed for a specific class of materials but offers a general reporting format that may be useful to anyone concerned with friction and wear testing. The suggested reporting format includes a description of the test device and test...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006789
EISBN: 978-1-62708-295-2
... Wear processes and relevant tribosystems Wear process Examples of relevant tribosystems Sliding wear Sliding bearings; cam and tappets; guides; seals; piston rings; disc-pad braking system; forming dies; cutting tools Fretting wear Riveted joints, bolted flanges, shrink fits, all in...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006829
EISBN: 978-1-62708-295-2
... Abstract Fretting is a wear phenomenon that occurs between two mating surfaces; initially, it is adhesive in nature, and vibration or small-amplitude oscillation is an essential causative factor. Fretting generates wear debris, which oxidizes, leading to a corrosion-like morphology. This...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005678
EISBN: 978-1-62708-198-6
... (UHMWPE). The principal physical properties and tribological characteristics of these materials are summarized. The article discusses the pin-on-disk experiments and pin-on-plate experiments for determining friction and wear characteristics. It details the use of various types of joint simulators, such as...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005677
EISBN: 978-1-62708-198-6
... Abstract This article reviews the friction and wear of various dental materials that have been studied by fundamental wear measurements, simulated service wear measurements, and clinical measurements. The materials include dental amalgam, composite restorative materials, pit and fissure...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003976
EISBN: 978-1-62708-185-6
... window seals ( Ref 82 ). Westheide ( Ref 101 ) also carried out similar studies on protective wear-resistant coatings for upsetting dies. A qualitative comparison of various coatings is provided in Table 9 . Hard chromium plating and TiC coatings via CVD were found to have excellent wear resistance...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003104
EISBN: 978-1-62708-199-3
... wear debris and the introduction of nonmetallic particles through imperfect seals. Other combinations include rolling with sliding and lubricated-nonlubricated situations. It is often difficult to compare published wear data obtained by different investigators, either because some of the...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001281
EISBN: 978-1-62708-170-2
... lamp 215 mm diam, 30 8 1 2 in. diam, 1 1 4 5557–1125 Buff, chemical brighten Sulfuric acid (a) Seal Atmospheric exposure Canopy track 760 mm T-extrusion 30-in. T-extrusion 7075 Machine Hard None Resist wear, sea air Gelatin molds 150–205 mm overall 6–8 overall...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005350
EISBN: 978-1-62708-187-0
... Abstract This article illustrates the basic components of dry and wet hearth reverberatory furnace. It discusses stack melters that are used for aluminum metal casting, as they are efficient in sealing the furnace and using the flue gases to preheat the charge materials. The article describes...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003065
EISBN: 978-1-62708-200-6
... gives a detailed account of production, properties and application of fiberglass, optical fibers, glass spheres and ceramic glasses, and describes the forms, classification, compositions and properties of glass/metal and glass-ceramic/metal seals. fiberglass forming glass melting glass spheres...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003848
EISBN: 978-1-62708-183-2
... Abstract Elastomers belong to a group of materials known as polymers that acquire their properties and strength from their molecular weight, chain entanglements, and crystalline regions. This article focuses on the use of elastomers as seals and describes its performance capabilities from the...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001320
EISBN: 978-1-62708-170-2
... productivity of carbide, cermet, and ceramic cutting tool materials used in machining operations. The useful life of cutting tools may be limited by a variety of wear processes, such as crater wear, flank wear or abrasive wear, builtup edge, depth-of-cut notching, and thermal cracks. The article provides...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003061
EISBN: 978-1-62708-200-6
... that make use of wear resistance include dies for hot extrusion of metal rods and tubes, inserts for tablesetting, and paper lapping dies, seals, and bearings. The information in this article is largely taken from the following articles in Ceramics and Glasses, Volume 4, Engineered Materials...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003225
EISBN: 978-1-62708-199-3
... degree of wear. Typical components include bearings, gears, seals, guides, piston rings, splines, brakes, and clutches. Wear of these components can range from mild, polishing-type attrition to rapid, severe removal of material with accompanying surface roughening. Whether or not wear constitutes failure...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003152
EISBN: 978-1-62708-199-3
... Abstract Cemented carbides belong to a class of hard, wear-resistant, refractory materials in which the hard carbide particles are bound together, or cemented, by a ductile metal binder. Cermet refers to a composite of a ceramic material with a metallic binder. This article discusses the...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003838
EISBN: 978-1-62708-183-2
... Abstract Cemented carbides are extremely important in corrosion conditions in which high hardness, wear resistance, or abrasion resistance is required. This article describes the effect of binder composition and carbide addition on corrosion behavior of cemented carbides. It lists the examples...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003842
EISBN: 978-1-62708-183-2
... information on high-temperature applications, wear properties, and the microscopic analyses of advanced ceramics. microscopic analysis advanced ceramics ceramic matrix composites high-temperature oxidation mechanical properties oxide ceramics wear properties CERAMICS are generally stable to...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001311
EISBN: 978-1-62708-170-2
... powders, are worn away by, for example, blades. A good seal is maintained by partial wear of the coating and essentially no blade-tip wear occurs. Plasma-sprayed anti-fretting-wear coatings for titanium alloys, usually of tungsten carbide-cobalt, are also widely used. Another major use of sprayed...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003057
EISBN: 978-1-62708-200-6
.... The article describes testing methods such as room and high-temperature strength test methods, proof testing, fracture toughness measurement, and hardness and wear testing. It also explains methods for determining thermal expansion, thermal conductivity, heat capacity, and emissivity of ceramics and...