Published: 01 January 1989
Fig. 22 Effect of blank size on the major and pitch diameters of 1038 steel screws with thread length of 6.4 mm ( 1 4 in.). See the table accompanying Fig. 16 for screw details and threading conditions. All dimensions in figure given in inches. More
Image
Published: 01 January 2005
Fig. 22 Effect of blank size on the major and pitch diameters of 1038 steel screws with thread length of 6.4 mm ( 1 4 in.). See the table accompanying Fig. 16 for screw details and threading conditions. All dimensions in figure given in inches More
Image
Published: 01 January 2001
Fig. 24 S - N curve comparing blind fasteners with screws and nutplates in composite laminate More
Image
Published: 30 August 2021
Fig. 33 Bend in one of the fractured bone screws More
Image
Published: 15 June 2019
Fig. 33 Screws, nuts, bolts, and machine tooling produced from aluminum and free-machining alloys such as 6262 and 2011-T6. Courtesy of Cox Manufacturing and Elkins Machine & Tool Company More
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001018
EISBN: 978-1-62708-161-0
... of 0.55% C that are intended for use under the service conditions mentioned above. Guidelines are also discussed for the selection of steels for bolts (including cap screws), studs (including U-bolts), and nuts for service at the temperature range mentioned above and for service between 200 and 370 °C...