Skip Nav Destination
Close Modal
By
Carolyn Carradero Santiago, Eric MacDonald, Jose Coronel, Dominic Kelly, Ryan Wicker ...
By
Lucas W. Koester, Leonard J. Bond, Peter C. Collins, Hossein Taheri, Timothy Bigelow
By
Adrian Pierorazio, Nicholas E. Cherolis, Michael Lowak, Daniel J. Benac, Matthew T. Edel
Search Results for
satellite components
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 100 Search Results for
satellite components
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001086
EISBN: 978-1-62708-162-7
... specifically for optical components is satellite imaging systems. Because the large mirrors used in aerospace optics must retain precise geometry throughout complex loading spectra, no differentiation was drawn between grades used for optical instruments and those used for inertial-guidance instruments...
Abstract
Beryllium is a metal with an unusual combination of physical and mechanical properties that make it particularly effective in optical components, precision instruments, and specialized aerospace applications. Almost all of the beryllium in use is a powder metallurgy (P/M) product. Beginning with an overview of the mining and refining processes of beryllium, this article discusses powder production and consolidation methods, beryllium grades and their designations, and the protective measures that have been enacted to reduce exposure to beryllium.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001260
EISBN: 978-1-62708-170-2
... to extend the lifetime of printing press components that are subject to sliding-wear damage. Other applications of electroplated multiple-layer thin films that are being explored include the use of Cu/Ag and Cu/Co alloys for high-temperature applications in rocket thrust aligners, where protective...
Abstract
Multiple-layer alloy electrodeposition involves the formation of an inhomogeneous alloy consisting of lamellae of different composition. This article reviews the process description, engineering parameters, characterization, and applications of multiple-layer alloys. Pulsed-current plating and pulsed-potential plating are also discussed.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003165
EISBN: 978-1-62708-199-3
...) are required. In addition to these grades, I-70 was developed for optical components in satellite imaging systems and optical grade O-50 was developed for infrared optical instruments. Table 1 gives compositions of instrument/optical grades. Beryllium Alloys Beryllium is too reactive to accept...
Abstract
Beryllium possesses an unusual combination of physical and mechanical properties, suiting it for specialized applications where its relatively high cost can be justified. It has very low density, a moderately high melting point, high elastic modulus, and good electrical and thermal conductivity. The article describes structural, instrument, and optical grade beryllium and the corresponding compositional ranges. It also discusses processing and product forms as well as factors affecting corrosion resistance. The article concludes with a short note on health and safety considerations when handling beryllium.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003475
EISBN: 978-1-62708-195-5
... on launch vehicle upper stages and satellites. A brief description of key applications, including solid rocket motor casings, payload fairings, and payload support (adapter) structures, is presented subsequently. Solid Rocket Motors Space motor components must be highly reliable and lightweight...
Abstract
This article discusses composites for unmanned space vehicles and provides an overview of key design drivers, challenges, and environment for use of composites in spacecraft, launch vehicles, and missiles. It describes the design allowable properties of composite materials. The article provides information on the specific state-of-the-art applications of composite materials for spacecraft missiles and launch vehicles. A discussion on the key applications, including solid rocket motor casings, payload fairings, and payload support structures, is presented.
Book Chapter
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006558
EISBN: 978-1-62708-290-7
... photopolymerization and thermoplastic extrusion 3D printing have been used to create geometrically complex dielectric structures that serve as an electrical device substrate. During interruptions in these processes, ink deposition can provide a network of conductive paths to connect electronic components, create...
Abstract
This article provides an overview of the implementation of wire embedding with ultrasonic energy and thermal embedding for polymer additive manufacturing, discussing the applications and advantages of the technique. The mechanical and electrical performance of the embedded wires is compared with that of other conductive ink processes in terms of electrical conductivity and mechanical strength.
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001091
EISBN: 978-1-62708-162-7
... for defense applications. Gallium arsenide is about ten times more resistant to radiation than silicon. This resistance is essential in satellite operations in space, where components are exposed to damaging radiation from the sun. Gallium arsenide circuits also can operate at higher temperatures than can...
Abstract
Gallium-base components can be found in a variety of products ranging from compact disk players to advanced military electronic warfare systems, owing to the factor that it can emit light, has a greater resistance to radiation and operates at faster speeds and higher temperatures. This article discusses the uses of gallium in optoelectronic devices and integrated circuits and applications of gallium. The article discusses the properties and grades of gallium arsenide and also provides information on resources of gallium. The article talks about the recovery techniques, including recovery from bauxite, zinc ore and secondary recovery process and purification. The article briefly describes the fabrication process of gallium arsenide crystals. Furthermore, the article gives a short note on world supply and demand of gallium and concludes with research and development on gallium arsenide integrated circuits.
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006560
EISBN: 978-1-62708-290-7
... parts. Fig. 4 Metal printed satellite component with lattice structure from Thales Alenia Space. Source: Ref 30 . Reprinted from https://www.metal-am.com/large-scale-metal-lattice-structure-complex-satellite-part/ , copyright 2016 Thales Alenia Space, by permission from Thales Alenia Space...
Abstract
This article introduces the design and manufacturing implications of additive manufacturing (AM) on part characteristics as well as on design opportunities and on manufacturing practices, supply chains, and even business models. In addition, it describes how they relate to the fundamental nature of AM processes and discusses the characteristics and purposes of AM processes and the parts they fabricate.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003367
EISBN: 978-1-62708-195-5
... they have found wide applications in electronics, printed circuit boards, satellite and aerospace structural composites, and low-dielectric and radar applications. They can be formulated for use as high-performance adhesives, syntactic foams, honeycomb, and fiber- reinforced composites and are often found...
Abstract
Cyanate ester resins are a family of high-temperature thermosetting resins that bridge the gap in thermal performance between engineering epoxy and high-temperature polyimides. This article discusses the chemistry, properties and characteristics of the cyanate ester resins. It describes the processing procedures for the cyanate ester resins and provides information on properties for selected applications, such as space applications, radomes, and printed circuit boards.
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006357
EISBN: 978-1-62708-192-4
... carried out. Applying a theory to a condition that is considerably different from that which was used to derive the particular theory is likely to lead to an erroneous outcome. In a way, the applicable theory of wear is very much a function of the operating condition of the pair of components...
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003409
EISBN: 978-1-62708-195-5
...Abstract Abstract The prepreg hand lay-up process is a versatile, reliable, cost-effective, and high quality process for fabricating large or small components. This article discusses the technique characteristics and applications of the process. It describes the stages involved in the process...
Abstract
The prepreg hand lay-up process is a versatile, reliable, cost-effective, and high quality process for fabricating large or small components. This article discusses the technique characteristics and applications of the process. It describes the stages involved in the process of lay-up, namely, lay-up definition, ply-kit cutting, layup, debulking, and preparation for curing. The article concludes with a discussion on the component properties and design guidelines of the prepreg hand lay-up process.
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001080
EISBN: 978-1-62708-162-7
... for structural components on aircraft ranging from the Boeing 707, to the supersonic SR-71 Blackbird reconnaissance aircraft, to space satellites and missiles. Jet Engine Components Jet engine components ( Ref 8 ). Titanium fan disks ( Fig. 4 ), turbine blades and vanes, and structurals are commonly used...
Abstract
Titanium has been recognized as an element with good mechanical and physical properties, alloying characteristics, and corrosion resistance. Providing an outline of general characteristics and types of titanium alloys, this article discusses the contemporary technology of titanium along with its market developments. It also discusses the application of titanium and titanium alloys in corrosive environments and in aerospace and automotive industries. The article describes the developments in titanium processing and materials technologies, which include the development of sponge production and melting processes, oxide dispersion-strengthened alloys by powder metallurgy techniques, titanium-base intermetallic compounds, and titanium-matrix composites.
Book Chapter
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005142
EISBN: 978-1-62708-186-3
... systems, and precision satellite and airborne optical components. Structural grades find application as satellite superstructures, antenna booms, and optical support structures. Table 1 lists the compositions of four grades of vacuum hot pressed beryllium. Compositions of four grades of vacuum hot...
Abstract
This article describes the effect of temperature, composition, strain rate, and fabrication history on the results obtained in the forming of beryllium as well as the safety measures required. It provides information on the equipment, tooling, dies, and workpieces used for forming beryllium. The article discusses the role of lubrication, blank development, tool designs, and strain rates, in deep drawing. It also provides information on the tooling and applications of three-roll bending, stretch forming, and spinning.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003350
EISBN: 978-1-62708-195-5
... to MMCs. In each of these systems, the matrix is typically a continuous phase throughout the component. The second level of classification refers to the reinforcement form—particulate reinforcements, whisker reinforcements, continuous fiber laminated composites, and woven composites (braided...
Abstract
This article begins with a brief history of composite materials and discusses its characteristics. It presents an introduction to the constituents, product forms, and fabrication processes of composite materials. The article concludes with a discussion on the applications of organic-matrix, metal-matrix, and ceramic-matrix composites.
Book Chapter
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006465
EISBN: 978-1-62708-190-0
... components, such as porosity, inclusions, cracking, and residual stress, that can be avoided by using vendor recommended process parameters and approved materials. It describes the development of process-structure-property-performance modeling. The article explains the practical considerations...
Abstract
Additive manufacturing (AM) is the process of joining materials to make parts from three-dimensional (3D) model data, usually layer upon layer, as opposed to subtractive manufacturing and formative manufacturing methodologies. This article discusses various defects in AM components, such as porosity, inclusions, cracking, and residual stress, that can be avoided by using vendor recommended process parameters and approved materials. It describes the development of process-structure-property-performance modeling. The article explains the practical considerations in nondestructive evaluation for additively manufactured metallic parts. It also examines nondestructive testing (NDT) inspection and characterization methods for each of the manufacturing stages in their natural order. The article provides information on various inspection techniques for completed AM manufactured parts. The various electromagnetic and eddy current techniques that can be used to detect changes to nearsurface geometric anomalies or other defects are also discussed. These include ultrasonic techniques, radiographic techniques, and neutron imaging.
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001465
EISBN: 978-1-62708-173-3
... for the same reasons welding is popular on earth. Welding applications in space are similar to those on earth in that they both involve the need to assemble structural components that will exhibit sufficient strength, endurance, and reliability during their service lives. In addition, ease of repair of welded...
Abstract
Welding as an assembly process has become increasingly more attractive to designers of space structures because of its sufficient strength, endurance, reliability during their service lives, and ease of repair. This article reviews a variety of applications for welding in space and low-gravity environments and describes the unique aspects of the space environment. It compares the applicable welding processes, namely, electron-beam welding, laser-beam welding, and gas-tungsten arc welding and examines the metallurgy of low-gravity welds. Steps taken to ensure the continued development of welding technology in space are also discussed.
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006650
EISBN: 978-1-62708-213-6
... the +1/2 and −1/2 levels (central transition), which are those typically measured by NMR, can be detected using RF-based methods. Other transitions, called satellite transitions, also are made possible through the Zeeman effect, including those for higher-order spin states such as 3/2 and 5/2, depending...
Abstract
This article focuses on the application of solid-state nuclear magnetic resonance (NMR) spectroscopy in materials science, especially for inorganic and organic polymer solids. It begins with a discussion on the general principles of NMR, providing information on nuclear spin descriptions and line narrowing and spectral resolution and describing the impact of magnetic field on nuclear spins and the factors determining resonance frequency. This is followed by a description of various systems and equipment necessary for NMR spectroscopy. A discussion on general sampling for solid-state NMR, sample-spinning requirements, and extraneous signals is then included. Various factors pertinent to accurate calibration of the NMR spectrum are also described. The article provides information on some of the parameters both beneficial and problematic for processing NMR data. It ends with a description of the applications of NMR in glass science and ceramics.
Book Chapter
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006804
EISBN: 978-1-62708-329-4
... pieces can be very significant ( Ref 1 ). Fig. 2 Horizontal vessel that experienced a boiling liquid expanding vapor explosion. Source: Ref 1 Explosion Damage Indicators In failure and incident investigations, component and equipment damage is often used to determine the location...
Abstract
This article addresses the effects of damage to equipment and structures due to explosions (blast), fire, and heat as well as the methodologies that are used by investigating teams to assess the damage and remaining life of the equipment. It discusses the steps involved in preliminary data collection and preparation. Before discussing the identification, evaluation, and use of explosion damage indicators, the article describes some of the more common events that are considered in incident investigations. The range of scenarios that can occur during explosions and the characteristics of each are also covered. In addition, the article primarily discusses level 1 and level 2 of fire and heat damage assessment and provides information on level 3 assessment.
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006681
EISBN: 978-1-62708-213-6
... and Hardware In general, it is still possible to use a relatively complicated instrument such as a TEM without detailed knowledge of its hardware components. Modern electron microscopes consist of a set of complex components, including an electron source, electromagnetic lenses, recording devices, and so...
Abstract
Transmission electron microscopy (TEM) approach enables essentially simultaneous examination of microstructural features through imaging from lower magnifications to atomic resolution and the acquisition of chemical and crystallographic information from small regions of the thin specimen. This article discusses fundamentals of the technique, especially for solving materials problems. Background information is provided to help understand basic operations and principles, including instrumentation, the physics of signal generation and detection, image formation, electron diffraction, and spectrometry techniques with data analysis.
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009084
EISBN: 978-1-62708-177-1
... ( Ref 3 , 5 ). Heat Effects on Composite Material Surfaces The proper selection of the matrix material for the environment in which a component is to be used is critical so that long-term durability of the part is maintained. If the temperature to which the composite is exposed in service...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005339
EISBN: 978-1-62708-187-0
... for lightweight and higher-strength components ( Ref 1 , 2 , 3 , 4 , 5 , 6 ). MMCs are engineered combinations of two or more materials (one of which is a metal or alloy) in which tailored properties, not achievable in monolithic metals or alloys, are achieved by systematic combinations of different...
Abstract
Metal matrix composites (MMCs) can be synthesized by vapor phase, liquid phase, or solid phase processes. This article emphasizes the liquid phase processing where solid reinforcements are incorporated in the molten metal or alloy melt that is allowed to solidify to form a composite. It illustrates the three broad categories of MMCs depending on the aspect ratio of the reinforcing phase. The categories include continuous fiber-reinforced composites, discontinuous or short fiber-reinforced composites, and particle-reinforced composites. The article discusses the two main classes of solidification processing of composites, namely, stir casting and melt infiltration. It describes the effects of reinforcement present in the liquid alloy on solidification. The article examines the automotive, space, and electronic packaging applications of MMCs. It concludes with information on the development of select cast MMCs.