Published: 01 December 1998
Fig. 5 Schematic of salt bath furnace. Agitated molten salt bath with sludge settling zone More
Image
Published: 01 January 1994
Fig. 2 Cutaway view of a salt bath furnace incorporating an agitated molten salt bath and a sludge settling zone More
Image
Published: 30 September 2014
Fig. 9 Internally heated salt bath furnace with submerged electrodes. This furnace has a modified brick lining for use with carburizing salts. More
Image
Published: 01 December 1998
Fig. 5 Internally heated salt bath furnace with submerged electrodes. This furnace has a modified brick lining for use with carburizing salts. More
Image
Published: 30 September 2014
Fig. 9 Salt bath furnace. Courtesy of Borel Swiss AG More
Image
Published: 30 September 2014
Fig. 3 Ventilation of a salt bath furnace with (a) a capture hood and (b) a canopy hood. The capture hood in (a) requires a ventilation rate of 200 m 3 /min (7120 ft 3 /min), whereas the canopy hood in (b) requires a larger ventilation rate of 905 m 3 /min (32,000 ft 3 /min). All dimensions More
Image
Published: 30 September 2014
Fig. 5 Internally heated salt bath furnace with immersed electrodes and ceramic tiles More
Image
Published: 30 September 2014
Fig. 7 Metal pot, immersed-electrode salt bath furnace for ferrous tempering and isothermal annealing—see table for standard sizes Typical standard sizes Temperature range Working dimensions Input, kW Heating capacity (A) Length (B) Width (C) Depth °C °F mm in. mm More
Image
Published: 30 September 2014
Fig. 8 Metal pot, immersed-electrode salt bath furnace for liquid carburizing, cyaniding, and carbonate baths—see table for standard sizes Typical standard sizes Temperature range Working dimensions Input, kW Heating capacity (A) Length (B) Width (C) Depth °C °F mm More
Image
Published: 01 December 1998
Fig. 4 Internally heated salt bath furnace with immersed electrodes and ceramic tiles More
Image
Published: 30 September 2014
Fig. 4 Externally heated salt bath furnaces for liquid carburizing More
Image
Published: 01 December 1998
Fig. 3 Externally heated salt bath furnaces for liquid carburizing More
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005958
EISBN: 978-1-62708-168-9
... Abstract This article provides a detailed discussion on the heating equipment used for austenitizing, quenching, and tempering tool steels. These include salt bath furnaces, controlled atmosphere furnaces, fluidized-bed furnaces, and vacuum furnaces. The article discusses the types of nitriding...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005776
EISBN: 978-1-62708-165-8
... procedures, as well as the equipment used (salt bath furnaces) and safety precautions to be undertaken during the liquid nitriding process. It describes the different types of liquid nitriding process, namely, liquid pressure nitriding, aerated bath nitriding, and liquid nitrocarburizing. Environmental...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005815
EISBN: 978-1-62708-165-8
.... The article discusses the embrittlement problems associated with tempering. Four types of equipment are used for tempering, namely, convection furnaces, salt bath furnaces, oil bath equipment and molten metal baths. Special procedures for tempering are briefly reviewed. cracking dimensional change...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005929
EISBN: 978-1-62708-166-5
...: the first type uses atmosphere austenitizing followed by salt quench and the second type employs austenitizing salt baths with rapid transfer to the quench salt. The article provides a detailed account on the construction, advantages and disadvantages, and limitations of isothermal quenching furnaces...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003198
EISBN: 978-1-62708-199-3
... Abstract Batch furnaces and continuous furnaces are commonly used in heat treating. This article provides a detailed account of various heat treating equipment and its furnace types, including salt bath equipment (externally heated, immersed-electrode and submerged-electrode furnaces...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001225
EISBN: 978-1-62708-170-2
... of heat treatment salt bath furnaces. However, the actual process equipment is unique. Two main distinctions between heat treatment/heat transfer salts and cleaning salts are that the cleaning salts are chemically active and the byproduct generation in cleaning baths is potentially much greater. Both...
Image
Published: 01 January 1993
Fig. 1 Principal types of furnaces used for molten-salt-bath dip-brazing applications. (a) and (b) externally heated; (c) and (d) internally heated More
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005957
EISBN: 978-1-62708-166-5
... safety requirements of these furnaces. batch-type furnaces ceramic fibers continuous-type furnaces fluidized-bed furnaces heat exchangers heat treating furnaces salt bath furnaces FURNACES ARE ONE OF THE MOST VERSATILE TYPES of industrial appliances that span many different areas of use...