1-20 of 555 Search Results for

safety and environmental considerations

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003828
EISBN: 978-1-62708-183-2
... of hydride corrosion of uranium are discussed. The article provides information on environmentally assisted cracking, protective coatings, and surface modification of uranium and its alloys. It also summarizes the environmental, safety, and health considerations for their use. atmospheric corrosion...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001245
EISBN: 978-1-62708-170-2
... information on the quality control of nickel plating. It concludes with a review of the environmental, health, and safety considerations associated with nickel plating. deposit properties electroforming health and safety considerations multilayer coating nickel plating process considerations...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003044
EISBN: 978-1-62708-200-6
.... The article also discusses the test procedures, recommended configurations, test specimen considerations, and safety requirements considered in the four major types of mechanical testing of polymer-matrix composites: tensile test, compression test, flexural test, and shear test. compression test...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001222
EISBN: 978-1-62708-170-2
... the mechanisms of alkaline cleaning, such as saponification, displacement, emulsification and dispersion, and metal oxide dissolution. The article concludes with information of the safety and environmental considerations in the usage of alkaline cleaners. alkaline cleaner composition alkaline cleaning...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001258
EISBN: 978-1-62708-170-2
..., nickel-manganese alloys, and nickel chromium binary and ternary alloys. It also includes information on the environmental, health, and safety considerations for these nickel-base alloys. health and safety considerations nickel alloy plating nickel-chromium plating nickel-cobalt plating nickel...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001225
EISBN: 978-1-62708-170-2
.... It provides an overview of the basic design and safety considerations of the salt bath equipment and describes the environmental impact of molten salt bath cleaning. casting cleaning environmental impact flame spray removal glass removal molten salt bath cleaning paint stripping personnel safety...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001246
EISBN: 978-1-62708-170-2
... and processing equipment and discusses the properties, advantages, limitations, and principal applications of iron plating. It also describes the environmental, health, and safety considerations of iron plating. electrolytes health and safety considerations iron plating iron plating equipment IRON...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005776
EISBN: 978-1-62708-165-8
... procedures, as well as the equipment used (salt bath furnaces) and safety precautions to be undertaken during the liquid nitriding process. It describes the different types of liquid nitriding process, namely, liquid pressure nitriding, aerated bath nitriding, and liquid nitrocarburizing. Environmental...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003445
EISBN: 978-1-62708-195-5
... a “building-block” testing approach ( Fig. 3 ), in which environmental effects are addressed at the analysis, coupon, structural element, subcomponent, component, and full-scale levels. The sums of these levels of analyses and tests must be consolidated in such a way as to validate the consideration...
Book Chapter

By Greg Kress
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003392
EISBN: 978-1-62708-195-5
..., and environmental constraints. mechanical properties composites repeatability cost size damage tolerance durability environmental constraints design criteria DESIGN CRITERIA are the decisive quantified goals that a product must attain. A product needs to achieve a certain level of safety, cost...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003691
EISBN: 978-1-62708-182-5
... of the Environmental Protection Agency and the Occupational Safety and Health Administration as well as the corresponding Code of Federal Regulation numbers. coating lining material surface preparation THE TOTAL NATIONAL YEARLY COST of metallic corrosion in the United States was estimated at $275 billion...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002439
EISBN: 978-1-62708-194-8
..., producibility, maintainability, environmental impact, quality, unit cost, and so on. In terms of safety, consideration of hazards and their elimination must start with the first concept of the design of the product and be carried through the entire life cycle. As Hunter ( Ref 7 ) says: “This must include...
Series: ASM Handbook
Volume: 24A
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.hb.v24A.a0006960
EISBN: 978-1-62708-439-0
... Abstract This article provides an overview of the concepts of environmental, health, and safety (EH&S) risk incidents, then discusses these concepts relative to additive manufacturing (AM): the multiple intrants, process parameters, and equipment, as well as the resulting products...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001240
EISBN: 978-1-62708-170-2
... fluids grinding grinding fluid selection grinding waste disposal safety and environmental considerations FINISHING METHODS can include a wide variety of processes such as lapping, polishing, tumbling, and loose media. However, in keeping with metalworking tradition and for the purposes...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006137
EISBN: 978-1-62708-175-7
... and using common sintering atmosphere gases are explosion, fire, toxicity, and asphyxiation. atmosphere supply systems inspection maintenance safety and environmental concerns sintering atmosphere generators sintering atmospheres SINTERING ATMOSPHERES (endothermic gas, exothermic gas...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001322
EISBN: 978-1-62708-170-2
..., Occupational Safety and Health Administration, Title 29 Code of Federal Regulations , Part 1910.1027, 14 Sept 1992 5. Ryan W. and Schrader R. , An Ounce of Toxic Pollution Prevention , National Environmental Law Center , Jan 1993 6. Style R. , Are State Laws Motivating...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001376
EISBN: 978-1-62708-173-3
... the safety standards and regulations before proceeding ( Ref 13 ). Noise and Vibration Abatement The sound and ground vibration generated during EXW can be considerable. Common methods for noise abatement include performing the operation in a highly remote geographic location, in a mine or bunker...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005717
EISBN: 978-1-62708-171-9
... Abstract The hazards associated with thermal spray deposition processes include ultraviolet and infrared radiation; acoustical noise; and by-product production in the forms of nitrous oxides, ozone, fumes, and dust. The most important consideration in health and safety is to use the engineered...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005759
EISBN: 978-1-62708-171-9
..., and safety considerations. These guidelines are written within the context of the prevailing internationally accepted practices and standards, as well as United States laws and regulations. They are intended to have worldwide application. It is incumbent upon each individual, company, or institution...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002436
EISBN: 978-1-62708-194-8
.... With the increased emphasis on safety, reliability, and achieving mission objectives, design teams must incorporate risk/hazard considerations in their designs. Figure 1 is a flow chart that shows the integration of risk and hazard analysis in the overall design process. Even if designers or design managers...