1-20 of 117 Search Results for

rotary ultrasonic machine

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 January 1989
Fig. 3 Rotary ultrasonic machine tool More
Image
Published: 01 January 1989
Fig. 10 Parts machined by rotary ultrasonic machining More
Image
Published: 01 January 1989
Fig. 5 Diamond tools used in rotary ultrasonic machining More
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002159
EISBN: 978-1-62708-188-7
... Abstract The ultrasonic machining (USM) process consists of two methods, namely, ultrasonic impact grinding and rotary USM. This article lists the major ultrasonic components that are similar to both rotary USM and ultrasonic impact grinding. It also provides schematic representations...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003055
EISBN: 978-1-62708-200-6
... grinding and provides information on tooling, wheel selection, work material, and operational factors. It also discusses precision slicing and slotting, lapping, honing, and polishing as well as abrasive waterjet, electrical discharge, laser, and ultrasonic machining. abrasive machining ceramics...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005578
EISBN: 978-1-62708-174-0
... the process. The equipment for direct-drive and inertia machine tools is primarily the same. In general, a rotary friction welding machine tool consists of a drive motor for rotating a workpiece at high speed, a tailstock assembly for holding a stationary workpiece, a hydraulic ram for pressing...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001232
EISBN: 978-1-62708-170-2
... discussion on abrasive jet machining and ultrasonic machining. It concludes with a discussion on the four categories of factors that affect the abrasive finishing or machining: machine tool, work material, wheel selection, and operational. abrasive belt grinding abrasive belt polishing abrasive...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006467
EISBN: 978-1-62708-190-0
... of flaws encountered in the inspection of steel bars, including porosity, inclusions, scabs, cracks, seams, and laps. Inspection methods, such as magnetic-particle inspection. liquid penetrant inspection, ultrasonic inspection, and electromagnetic inspection, of steel bars are also described. The article...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005158
EISBN: 978-1-62708-186-3
... auxiliary horizontal axes (called u and v ). With four-axis control, the machine can tilt the wire to produce tapered work. Independent four-axis controls (machines with controlled vertical and rotary axes) are also available to allow production of top profiles that are independent of bottom profiles...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004010
EISBN: 978-1-62708-185-6
... forging or roll forming, disks are typically machined to a shape that is suitable for ultrasonic inspection. Roll formed titanium alloy disks can typically weigh 10 to 30% less than the equivalent forged component, depending on the complexity of the component geometry. The improved material utilization...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006936
EISBN: 978-1-62708-395-9
... Abstract Of the many different nondestructive evaluation (NDE) techniques, ultrasonic inspection continues to be the leading nondestructive method for inspecting composite materials, because measurements can be quantitative and the typical defect geometries and orientations lend themselves...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003045
EISBN: 978-1-62708-200-6
... Abstract Ultrasonic inspection is a nondestructive technique that is useful in both quality control and research applications for flaw detection in fiber-reinforced composite materials. This article describes ultrasonic nondestructive analysis by outlining its three basic types of scans...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006115
EISBN: 978-1-62708-175-7
.... The article summarizes the sieving methods for powders. The sieving methods include hand sieving, machine sieving, manual wet sieving, air jet sieving, sonic sifter, wet sieving by machine, the Seishin robot sifter, automated systems, and ultrasonic machine sieving. The article outlines the sieve types...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005715
EISBN: 978-1-62708-171-9
... requirements, coating function, part geometry, substrate metallurgy, structure, and thermal history. This article provides a detailed account of the various processes of surface preparation, namely, cleaning, roughening, dry abrasive grit blasting, and machining and macro roughening processes. It outlines...
Book Chapter

By J.F. Libsch
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001387
EISBN: 978-1-62708-173-3
... moving conveyor, rotary, or indexing device. In these systems, the operator serves primarily as an unskilled machine operator. Specialized complex assemblies (for example, electron tubes) that are brazed in controlled atmospheres may require skilled personnel with specialized training in induction...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002165
EISBN: 978-1-62708-188-7
...-the-electrode flushing, hole drilling beyond ten diameters is very difficult. These machines use brass or copper electrodes with negative polarity. Some machines use a guide bushing that is ultrasonically vibrated to aid flushing. Because of its low viscosity, water is the dielectric. The drilling speeds can...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003989
EISBN: 978-1-62708-185-6
... Radial forging machines, also referred to as rotary forging machines, are a modification of the traditional open-die press design that uses two sets of opposing dies, all of which apply deformation to the workpiece. Each pair of dies is arranged perpendicularly to the other as shown in Fig. 2 , which...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0005585
EISBN: 978-1-62708-170-2
... for grinding. (2) A diskshaped, coated abrasive product. abrasive flow machining. Removal of material by a viscous abrasive media flowing under pressure through or across a workpiece. abrasive jet machining. Material removal from a workpiece by impingement of fine abrasive particles that are entrained...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.9781627081702
EISBN: 978-1-62708-170-2
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004000
EISBN: 978-1-62708-185-6
..., including aluminum alloys and alloy steels, final forging design criteria for titanium closed-die forgings are typically balanced between forging producibility demands and total cost considerations, particularly intermediate and final component machining costs and overall metal recovery or yield...