1-20 of 149 Search Results for

rhodium

Sort by
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006199
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which rhodium (Rh) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Image
Published: 01 January 1986
Fig. 14 Compton scatter for rhodium tube from iron and plastic More
Image
Published: 01 January 1990
Fig. 8 Thermal emf of iridium-rhodium/iridium thermocouples. Adapted from Ref 9 More
Image
Published: 01 January 1990
Fig. 93 Reflectance of rhodium as a function of wavelength. Sources: Ref 316 , 317 More
Image
Published: 15 December 2019
Fig. 19 Compton scatter for rhodium tube from iron and plastic More
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005670
EISBN: 978-1-62708-198-6
... Abstract This article focuses on the use of noble and precious metals for biomedical applications. These include gold, platinum, palladium, ruthenium, rhodium, iridium, and osmium. The physical and mechanical properties of noble and precious metals are presented in tables. A brief discussion...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003829
EISBN: 978-1-62708-183-2
... Abstract This article characterizes the corrosion resistance of precious metals, namely, ruthenium, rhodium, palladium, silver, osmium, iridium, platinum, and gold. It provides a discussion on the general fabricability; atomic, structural, physical, and mechanical properties; oxidation...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001254
EISBN: 978-1-62708-170-2
... Abstract The electroplating of platinum-group metals (PGMs) from aqueous electrolytes for engineering applications is limited principally to palladium and, to a lesser extent, to platinum, rhodium, and thin layers of ruthenium. This article provides a discussion on the plating operations...
Image
Published: 31 December 2017
Fig. 15 Micrographs of wear tracks on single-crystal SiC {0001} surface after ten passes of rhodium and titanium pins in ultrahigh vacuum: (a) Rhodium pin; hexagonal cracking. (b) Titanium pin; hexagonal pit. Vacuum pressure, 10 –8 Pa; room temperature More
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006259
EISBN: 978-1-62708-169-6
... Abstract This article describes the annealing behavior of precious metals, namely, gold, silver, platinum, palladium, iridium, rhodium, ruthenium, and osmium. It discusses the annealing practices and their effect on the basic properties of common precious metal alloys. The article presents...
Book Chapter

Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001087
EISBN: 978-1-62708-162-7
... Abstract Precious metals are of inestimable value to modern civilization. This article discusses the resources and consumption, trade practices, and special properties of precious metals and its alloys, including ruthenium, rhodium, palladium, silver, osmium, iridium, platinum, and gold...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003150
EISBN: 978-1-62708-199-3
... Abstract Precious metals include gold, silver, and six platinum-group metals, namely, platinum, palladium, ruthenium, rhodium, osmium, and iridium. This article focuses on the consumption, trade practices, properties, product forms, and applications of these metals and their alloys. gold...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003158
EISBN: 978-1-62708-199-3
..., and great versatility of application. Thermocouples are grouped into two broad categories, namely, standard thermocouples, including five base-metal thermocouples and three noble-metal thermocouples that have been given letter designations, and nonstandard thermocouples, including iridium-rhodium, platinum...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006209
EISBN: 978-1-62708-163-4
... - Tantalum)” : in the article “Ni (Nickel) Binary Alloy Phase Diagrams.” “Rh-Ta (Rhodium - Tantalum)” : in the article “Rh (Rhodium) Binary Alloy Phase Diagrams.” “Ru-Ta (Ruthenium - Tantalum)” : in the article “Ru (Ruthenium) Binary Alloy Phase Diagrams.” “Si-Ta (Silicon - Tantalum...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006216
EISBN: 978-1-62708-163-4
...)” in the article “Pt (Platinum) Binary Phase Diagrams.” “Re-V (Rhenium - Vanadium)” in the article “Re (Rhenium) Binary Phase Diagrams.” “Rh-V (Rhodium - Vanadium)” in the article “Rh (Rhodium) Binary Phase Diagrams.” “Ru-V (Ruthenium - Vanadium)” in the article “Ru (Ruthenium) Binary Phase...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006215
EISBN: 978-1-62708-163-4
...)” in the article “Pu (Plutonium) Binary Alloy Phase Diagrams.” “Re-U (Rhenium - Uranium)” in the article “Re (Rhenium) Binary Alloy Phase Diagrams.” “Rh-U (Rhodium - Uranium)” in the article “Rh (Rhodium) Binary Alloy Phase Diagrams.” “Ru-U (Ruthenium - Uranium)” in the article “Ru (Ruthenium...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006204
EISBN: 978-1-62708-163-4
... - Selenium)” in the article “Pd (Palladium) Binary Alloy Phase Diagrams.” “Pr-Se (Praseodymium - Selenium)” in the article “Pr (Praseodymium) Binary Alloy Phase Diagrams.” “Rb-Se (Rubidium - Selenium)” in the article “Rb (Rubidium) Binary Alloy Phase Diagrams.” “Rh-Se (Rhodium - Selenium...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006213
EISBN: 978-1-62708-163-4
... (Phosphorus - Titanium) ” in the article “P (Phosphorous) Binary Alloy Phase Diagrams.” “Pd-Ti (Palladium - Titanium) ” in the article “Pd (Palladium) Binary Alloy Phase Diagrams.” “Pt-Ti (Platinum - Titanium) ” in the article “Pt (Platinum) Binary Alloy Phase Diagrams.” “Rh-Ti (Rhodium...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001261
EISBN: 978-1-62708-170-2
... 0.200 Cobalt 0.014 Copper 0.013 Gallium 0.014 Gold 0.006 Indium 0.009 Iridium 0.069 Iron 0.025 Lead 0.006 Mercury 0.008 Nickel acid 0.047 Nickel alkaline 0.017 Nickel, black 0.025 Nickel, natural 0.025 Palladium 0.019 Platinum 0.015 Rhodium...
Book Chapter

Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006541
EISBN: 978-1-62708-183-2
... coating M Brass, low copper; bronze, low copper Metallic coating N Brass, high copper; bronze, high copper Metallic coating O Copper, high nickel Metallic coating P Nickel, cobalt Metallic coating Q Titanium Anodized R Silver Plating S Palladium, rhodium, gold, platinum...