1-20 of 1646

Search Results for resistance-ratio test

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001115
EISBN: 978-1-62708-162-7
... test methods used to characterize purity. Tables list the values for resistance ratios of zone-refined metals and their corresponding chemical compositions, and provide an example of the detection of impurities to concentrations in the parts per billion range, utilizing a combination of the glow...
Book Chapter

By J. Gilbert Kaufman
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006457
EISBN: 978-1-62708-210-5
... range of aluminum alloys based on notch-yield ratios measured in accordance with ASTM E 602 are illustrated in Fig. 13 . Fig. 13 Notch-yield ratio vs. tensile yield strength for wrought aluminum alloys (transverse direction). Source: Ref 33 Tear Resistance The other test widely used...
Book Chapter

By Doru M. Stefanescu
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006308
EISBN: 978-1-62708-179-5
... of automotive gray cast irons designated by the tensile strength-Brinell hardness ratio Properties determined on as-cast test bar B (30.5 mm, or 1.2 in. diam) SAE grade Brinell hardness, HB Microstructure (a) Minimum transverse load Minimum deflection Minimum tensile strength (TS) TS/HB (b) kN...
Book Chapter

By S. Lampman
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002403
EISBN: 978-1-62708-193-1
...% NaCl solutions at 105 °C (220 °F). Test data from U-bend also confirm good SCC resistance in chloride environments ( Ref 1 , 2 ), although SCC of the ferritics has been reported in applications such as: Type 434, type 430, and Fe-18Cr-2Mo in lithium chloride solutions Sensitized type 446...
Book Chapter

By Charles V. White
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001002
EISBN: 978-1-62708-161-0
... for machine components that must resist wear. castability gray iron impact resistance machinability microstructure pressure tightness section sensitivity test bar properties wear resistance CAST IRONS are alloys of iron, carbon, and silicon in which more carbon is present than can...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002398
EISBN: 978-1-62708-193-1
... structures. With more demanding structural applications, the fatigue and fracture resistance of castings is of considerable interest to designers of castings. In the past, material selection and product design were based on the results of tension tests, stress-life fatigue tests, and impact tests...
Book Chapter

Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006344
EISBN: 978-1-62708-179-5
... are dependent on the relevant wall thickness. The SAE International standard J431 ( Ref 7 ) classifies sand-molded gray cast irons used by the automotive and allied industries. It defines iron grades by a test bar tensile strength/Brinell hardness ratio, hardness grades by hardness alone, and casting grades...
Book Chapter

By Harvey P. Hack
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003663
EISBN: 978-1-62708-182-5
... and mass loss of certain model components. Although less expensive than full-scale component testing, physical scale modeling has many of the disadvantages of component testing. In addition, a great inaccuracy in conductivity scaling stems from the fact that the polarization resistance of the materials...
Book Chapter

By Hugh Baker
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003086
EISBN: 978-1-62708-199-3
..., and the fatigue strength of the material must be reported for a given number of cycles (as well as the stress ratio for the test and the stress-concentration factor if the specimen contains a notch). For steels, however, the curve breaks off and becomes essentially horizontal at some stress level called...
Image
Published: 01 January 1990
Fig. 10 Comparison of the oxidation-sulfidation resistance of MA ODS alloys with that of superalloys IN-738 and IN-100. Tested in a burner rig for 500 h at 925 °C (1700 °F) using an air-to-fuel ratio that varied from 27:1 to 21:1. JP-5 fuel contained 0.3% S. Temperature test cycle consisted More
Book Chapter

Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006346
EISBN: 978-1-62708-179-5
... from rotating-bending tests Table 7 Fatigue strengths and endurance ratios for five compacted graphite irons from rotating-bending tests Matrix structure Graphite type (a) Tensile strength Fatigue strength Fatigue-endurance ratio Hardness, HB MPa ksi MPa ksi As-cast ferrite...
Book Chapter

Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006339
EISBN: 978-1-62708-179-5
... in fatigue, with a notch sensitivity ratio (ratio of notched to unnotched endurance limits) ranging from 1.2 to 1.6 for the notch geometry tested. Conventional ferritic and pearlitic ductile irons have a notch sensitivity of approximately 1.6, and steels with fatigue strengths similar to ADI exhibit notch...
Book Chapter

By Cindy O'Malley, Carly McGee, Valerie Sherbondy
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006063
EISBN: 978-1-62708-172-6
... established, a simple solvent-resistance test performed by rubbing the surface of a coating with a cloth wet by solvent can be performed as a qualitative assessment of cure when a quantitative analysis is not required. The qualitative assessment of cure based on solvent resistance indicates proper coating...
Image
Published: 01 January 2005
Fig. 63 Comparison of the corrosion resistance of MA 6000 and MA 956 with that of other superalloys. Tested in a burner rig for 312 h using a 30-to-1 air-to-fuel ratio. Fuel contained 0.3% S and 5 ppm seawater, and specimens were held at temperature for 58 min of each hour, then cooled 2 min More
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003108
EISBN: 978-1-62708-199-3
... using test bars machined from 25 mm (1 in.) keel blocks. (a) 0.2% offset. (b) 0.0375% offset. (c) Calculated from tensile modulus and Poisson's ratio in tension Fig. 4 Tensile properties of ductile iron versus hardness. Mechanical properties were determined on specimens taken from...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006403
EISBN: 978-1-62708-192-4
... tribological action on a component (e.g., piston ring/cylinder liner; bearing shell/shaft). The contact-area-to-wear-track ratio is an important factor in developing suitable methods for testing. Fig. 4 Basic contact conditions for (a) conformal and (b) counterformal contact, with Hertzian contact...
Book Chapter

By Russell D. Kane
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003611
EISBN: 978-1-62708-182-5
... and manganese has been varied, although aluminum additions and diffusion coatings have shown particular promise in being able to set up a barrier to carbon ingress, thereby increasing resistance to carburization. Studies of alloy ratio of nickel and chromium have shown that alloys based on 50:50 nickel...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006098
EISBN: 978-1-62708-175-7
... properties Poisson's ratio powder metallurgy rearview mirror brackets sensor boss stainless steel powder thermal conductivity thermal diffusivity thermal expansion coefficient AN IMPORTANT CRITERION in the selection of stainless steel is the need for resistance to corrosion in the environment...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006913
EISBN: 978-1-62708-395-9
... and defines terms used in connection with testing and specification of plastics for electrical applications. arc resistance electrical applications electrical properties electrical testing plastics PLASTICS have become extremely popular among electrical product manufacturers. Prior...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006544
EISBN: 978-1-62708-210-5
... is better than 2024-O for forming by stretching, whereas 2024-O is better for forming by bending. Indexes of formability from tensile tests of several wrought aluminum alloys Table 5 Indexes of formability from tensile tests of several wrought aluminum alloys Alloy and temper Ratio of yield...