...) is a process by which a suitable powder or mixture of powders is compacted under the opposing forces of a pair of rolling mill rolls to form a continuous green strip that is further densified and strengthened by sintering and rerolling. This article discusses the basic principle, process considerations...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003039
EISBN: 978-1-62708-200-6
... Winding Machines Tensioners Ovens Prepreg (Commercial) Wet Rerolled Wet Winding Round Cylindrical Helical Winding Polar Winding Hoop Patterns Water-Soluble Mandrels Spider/Plaster Mandrels Tubular Steel Mandrels Nonremovable Metal Liners Specialized Mandrels...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003416
EISBN: 978-1-62708-195-5
...), wet rerolled, and wet winding. Prepregs Wet Rerolled Wet Winding In helical winding, the mandrel rotates more or less continuously while the fiber feed carriage traverses back and forth at a speed regulated to generate the desired helical angle. The normal winding pattern provides...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005286
EISBN: 978-1-62708-187-0
... Powder Twin-roll strip casting ( Fig. 11 ) is a continuous process in which molten metal is introduced through refractory or ceramic spout tips into the gap between counterrotating water-cooled rolls, producing strip at conventional reroll gages (3.18 to 11.4 mm, or 0.125 to 0.450...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006485
EISBN: 978-1-62708-207-5
... strip casting ( Fig. 11 ) is a continuous process in which molten metal is introduced through refractory or ceramic spout tips into the gap between counterrotating water-cooled rolls, producing strip at conventional reroll gages (3.18 to 11.4 mm, or 0.125 to 0.450 in.) that typically serve as stock...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001057
EISBN: 978-1-62708-162-7
... molten alloy directly to reroll gages ( Fig. 5 ). Strip casters employ counterrotating water-cooled cylinders or rolls to solidify and partially work coilable gage reroll stock in line. Slab casters of either twin-belt or moving block design cast stock typically 19 mm (0.75 in.) in thickness which...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004018
EISBN: 978-1-62708-185-6
... showing a shear band in rolled iron. Rolling strain, ε=2. Micron marker is parallel to the rolling direction. Original magnification 12,000×. Courtesy of D.J. Willis Fig. 16 70-30 brass, rolled 60%, etched, scratched parallel to rolling plane normal, and rerolled 10%. Old shear bands do...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001053
EISBN: 978-1-62708-161-0
... as to lie reasonably flat in charging box 27 Rail, steel No. 1 Standard section tee rails, original weight of 25 kg/m (50 lb/yd) or more; 3 m (10 ft) long and more. Suitable for rerolling into bars and shapes. Free from bent and twisted rails; frog, switch, and guard rails; or rails with split heads...
Book Chapter

Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005125
EISBN: 978-1-62708-186-3
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004163
EISBN: 978-1-62708-184-9
... surfaces is possible. The wrap needs to be extended into the shell/end cap seam and the entire thickness rerolled to seal off leaks. Figure 19 shows an AL409 muffler wrap after 27,400 km (17,000 miles) of driving, with internal leakage around the rolled head causing exterior corrosion of the protective...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005145
EISBN: 978-1-62708-186-3
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006276
EISBN: 978-1-62708-169-6
... pierced and rerolled Annealed tempers (d) O10 Cast and annealed (homogenized) O11 As-cast and precipitation heat treated O20 Hot forged and annealed O25 Hot rolled and annealed O30 Hot extruded and annealed O31 Extruded and precipitation heat treated O40 Hot pierced...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001011
EISBN: 978-1-62708-161-0
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001105
EISBN: 978-1-62708-162-7
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006527
EISBN: 978-1-62708-207-5
... by this process. Some parts can be rolled to a specified diameter in one operation. When high-strength alloys are being formed to relatively small radii, one or more reroll operations are required. In stretch bending, opposing tensile forces are applied to a workpiece wrapped around a bending form. Bending...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005139
EISBN: 978-1-62708-186-3
... starting and stop-off tabs. Trim tabs. Hammer weld to induce compressive stress, using an air hammer at 310 kPa (45 psi). Restore roundness of cylinder by rerolling several times in three-roll former. Form bead on one end of cylinder, in four passes in an edger. Roll flange on opposite end...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003131
EISBN: 978-1-62708-199-3
... pierced M45 As-hot pierced and rerolled Annealed tempers (d) O10 Cast and annealed (homogenized) O11 As-cast and precipitation heat treated O20 Hot forged and annealed O25 Hot rolled and annealed O30 Hot extruded and annealed O31 Extruded and precipitation heat treated...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.9781627081856
EISBN: 978-1-62708-185-6
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001065
EISBN: 978-1-62708-162-7
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.9781627081979
EISBN: 978-1-62708-197-9