1-20 of 219

Search Results for reinforced thermoset plastics

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

By J.R. Crum
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004181
EISBN: 978-1-62708-184-9
.... The article illustrates the effect of HCl on nonmetallic materials such as natural rubber, neoprene, thermoplastics, and reinforced thermoset plastics. It also tabulates the corrosion of various metals in dry hydrogen chloride. carbon steel chlorine zirconium alloy steel austenitic stainless steel...
Book Chapter

By Peter Elliott
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003702
EISBN: 978-1-62708-182-5
... various corrosion-resistant materials, including ferrous and nonferrous metals and alloys, thermoplastics, reinforced thermosetting plastics, nonmetallic linings, glass, carbon and graphite, and catalyzed resin coatings. It examines an unusual form of intergranular corrosion known as exfoliation, which...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003845
EISBN: 978-1-62708-183-2
... thermosetting resins. The article concludes with a discussion on the curing system of thermosetting resins. furan fabrication fiberglass-reinforced plastic equipment polyester epoxy vinyl-ester phenolic thermosetting resins MANY FACTORS contribute to the corrosion-resistant effectiveness...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003010
EISBN: 978-1-62708-200-6
... Abstract A thermosetting resin, or thermoset, is a synthetic organic polymer that cures to a solid, infusible mass by forming a three-dimensional network of covalent chemical bonds. Significant applications include construction and thermoset engineering plastics. This article discusses...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003002
EISBN: 978-1-62708-200-6
... and carbon-and glass-reinforced engineering thermoplastics. Values are also provided for chemical resistance ratings for selected plastics and metals, and hardness of selected elastomers. chemical resistance ratings elastomers engineering tables hardness materials characterization techniques...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006935
EISBN: 978-1-62708-395-9
... reinforcement. molecular orientation plastics processing process selection reinforcement thermoplastics thermosetting plastics MANUFACTURING PROCESS selection is a critical step in plastics product design. Failure to select a viable process during initial design stages can dramatically increase...
Book Chapter

Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003370
EISBN: 978-1-62708-195-5
... operation, one 1.2 m (4 ft) SMC machine can produce 11 × 10 9 g (25 × 10 6 lb) of molding compound per year. Bulk Molding Compounds Bulk molding compounds, or fiber-reinforced thermoset molding compounds, represent the original engineering plastic materials. Phenolic molding compounds reinforced...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003032
EISBN: 978-1-62708-200-6
... contoured planes, can also be woven with more threads per inch to achieve a high density. Satin weaves are used to best advantage in the reinforced plastic field, especially for prepregs for aircraft and missiles. Satin weave fabrics require more threads per inch to retain stability and are generally...
Book Chapter

Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003447
EISBN: 978-1-62708-195-5
... planes, can also be woven with more threads per inch to achieve a high density. Satin weaves are used to best advantage in the reinforced plastic field, especially for prepregs for aircraft and missiles. Satin weave fabrics require more threads per inch to retain stability and are generally produced...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003034
EISBN: 978-1-62708-200-6
... fiber type formulation matrix type BULK MOLDING COMPOUNDS, or fiber-reinforced thermoset molding compounds, represent the original engineering plastic materials. Phenolic molding compounds reinforced with cellulose fibers were developed by L. Baekeland early in this century. Fiberglass...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003471
EISBN: 978-1-62708-195-5
... and fillers) complicates the process. Energy Recovery Processes for Recycling of Thermoset Composites Like unreinforced plastics, composites have an appreciable energy content (although the frequently inorganic reinforcement phase significantly lowers the specific heat content). For example...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006922
EISBN: 978-1-62708-395-9
.... This article reviews the numerous considerations that are equally important to help ensure that part failure does not occur. It provides a quick review of thermoplastic and thermoset plastics. The article focuses primarily on thermoset materials that at room temperature are below their glass transition...
Book Chapter

By Vishu Shah
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006916
EISBN: 978-1-62708-395-9
... to the enhancement and retention of the overall strength of a fiber-reinforced plastic part. If fibers are intended to act as reinforcement and not as filler, and if the goal is to improve mechanical properties, it is important that they do not break up, bunch up, and reduce in length during processing...
Book Chapter

By Steven R. Nutt
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003351
EISBN: 978-1-62708-195-5
... they account for more than 80% of all matrices in reinforced plastics and essentially all matrices used in advanced composites. The most widely used thermosetting resins are the polyesters, which are most often combined with E-glass. This combination accounts for the bulk of the fiber-reinforced plastics (FRP...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003014
EISBN: 978-1-62708-200-6
... Abstract Injection molding is a process of forcing or injecting a fluid plastic material into a closed mold. The process generally has the advantages of being more readily automated and of permitting finer part details. Injection-molding compounds are thermoplastic or thermosetting materials...
Book Chapter

By Peter Martin
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006925
EISBN: 978-1-62708-395-9
... bond between adjacent carbon atoms ( Fig. 4 ). Three-dimensional covalent bonding is typified by cross linking that occurs when thermoset plastics are cured. Differences in chemical bonding are the reasons for the differences between thermoplastics and thermosets. Thermoplastics are invariably composed...
Book Chapter

By B. Tomas Åström
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003419
EISBN: 978-1-62708-195-5
... reinforcing fiber ideally should be surrounded by matrix without any voids. Fully polymerized thermoplastics have very high molecular weights, meaning that their melt viscosities are at least two orders of magnitude higher than melt viscosities for thermosets, which makes impregnation significantly more...
Book Chapter

By Joseph E. Sumerak, Jeffrey D. Martin
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003417
EISBN: 978-1-62708-195-5
... is the ability to use the widest variety of reinforcement types, forms, and styles with a broad selection of thermosetting resins and fillers. Virtually no other composite process offers as much materials versatility as pultrusion. Reinforcements can be placed precisely where they are needed for mechanical...
Book Chapter

Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003487
EISBN: 978-1-62708-195-5
...-wound reinforced at which the molecules have signi cant mo- tain thermosetting resins in which the material plastics, a winding pattern so designed that the bility, permitting them to reorient to a con g- is still soluble in certain liquids, and may be stresses in all laments are equal. uration having...
Book

Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.9781627081955
EISBN: 978-1-62708-195-5