1-20 of 133 Search Results for

reinforced concrete pipes

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006040
EISBN: 978-1-62708-172-6
..., precast concrete cylinder pipe and reinforced concrete pipe, prestressed concrete tanks, and stainless steel. It provides information on the most common generic coating systems used for new steel tanks and water storage tanks. It concludes with a discussion of quality watch-outs when selecting or using...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006007
EISBN: 978-1-62708-172-6
... pipe coatings, base layer for three-layer pipe-coating systems, internal pipe linings, and corrosion coatings for concrete reinforcing steel (rebar). This article provides information on the chemistries of FBE, and discusses the application procedures for internal and external FBE pipe coating...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006059
EISBN: 978-1-62708-172-6
... Microbiologically Influenced Corrosion of Ferrous Metals, Stainless Steels, and Concrete Localized Corrosion of Stainless Steels Corrosion of Aluminum Alloys Corrosion of Copper and Copper Alloys Failure of Precast Concrete Cylinder Pipe and Reinforced Concrete Pipe Other Cast-in-Place Concrete...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003482
EISBN: 978-1-62708-195-5
... to provide external reinforcement for stress redistribution Fig. 6 Repair/strengthening of deck using (a) pultruded strips adhesively bonded to the concrete substrate, and (b) unidirectional fabric placed using wet lay-up Fig. 8 Damage due to prestressed concrete cylinder pipe burst...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004104
EISBN: 978-1-62708-184-9
.... Rapid destruction of the concrete and subsequent exposure of the aggregate and reinforcing steel can occur. A typical example of hydrogen-sulfide-induced corrosion that has progressed to the point of exposing the reinforcing steel in a gravity sewer pipe is shown in Fig. 1 . Stainless steel...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004190
EISBN: 978-1-62708-184-9
... was discontinued. Some of the nonpressurized internal equipment in continuous digesters have traditionally been constructed from type 304L stainless steel. This includes the central pipes, screens, and internal cone. Many of the nozzles in carbon steel digesters are also type 304L stainless steel...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006038
EISBN: 978-1-62708-172-6
... with an outer layer of polymer concrete Fig. 38 Two-layer abrasion-resistant overcoating system consisting of (1) fusion-bonded epoxy topcoat and (2) fusion-bonded epoxy primer Fig. 39 Components of a weight coat system including (1) corrosion-protective coating and (2) reinforced concrete...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003805
EISBN: 978-1-62708-183-2
... for stray return currents from electric rail systems, electrical grounding equipment, and CP systems on nearby pipes. Accelerating corrosion occurs at the point where the current leaves the pipe to the earth. The environment provided by good-quality concrete to steel reinforcement is one of high...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003051
EISBN: 978-1-62708-200-6
... processes and advanced manufacturing techniques are often used where these materials are employed. This article examines several traditional ceramics, including structural clay, whiteware, glazes, enamels, portland cements, and concrete. It also provides a detailed account of fabrication methods, properties...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004121
EISBN: 978-1-62708-184-9
... • Illig G. , Protecting Concrete Tanks in Water and Wastewater Treatment Plants , Water Eng. Manage. , Vol 145 ( No. 9 ), Sept 1998 , p 50 – 57 • Jones B.L. and Sansum A.J. , Review of Protective Coating Systems for Pipe and Structures in Splash Zones in Hostile Environments...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004168
EISBN: 978-1-62708-184-9
...Abstract Abstract Bridges and highways are core components of transportation system and range from pavements with earth, gravel, or stone covered by a thin bituminous surface course to a continually reinforced Portland cement concrete (PCC) roadway with or without a bituminous wear course...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004220
EISBN: 978-1-62708-184-9
... Marine 686 27.0 Cape Canaveral, FL (beach) Marine 1070 42.0 Source: Ref 1 Recommended maximum water-soluble chloride levels in concrete mix (prior to service) for different reinforced concrete exposures Table 2 Recommended maximum water-soluble chloride levels in concrete mix...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003637
EISBN: 978-1-62708-182-5
... Water-saturated clay-type soils of near-neutral pH with decaying organic matter and a source of SRB Water treatment Heat exchangers and piping Sewage handling and treatment Concrete and reinforced-concrete structures Highway maintenance Culvert piping Buildings and stoneworks Ancient...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006062
EISBN: 978-1-62708-172-6
... corrosion protection for steel structures, piping, and miscellaneous hardware such as hanger rods, fasteners, conduit, piping (exterior), and so on. Stainless steel and fiberglass-reinforced plastic (FRP) tanks and piping and concrete structures and surfaces are usually not included. Unless the maintenance...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006782
EISBN: 978-1-62708-295-2
... concrete wall debris identified by x-ray diffraction Table 2 Composition of deteriorating concrete wall debris identified by x-ray diffraction Compounds Composition, wt% Sample A Sample B Sample C Sample D CaCO 3 (calcite) 44.8 3.6 72.9 … CaO (lime...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003655
EISBN: 978-1-62708-182-5
... Management In addition to the previous examples dealing with probe locations, the following examples illustrate various monitoring techniques. Example 4: Smart Reinforced Concrete Structures Example 5: Atmospheric Corrosion in Aircraft Example 6: Electrochemical Noise Probes in Chemical Plants...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001014
EISBN: 978-1-62708-161-0
... E4340 6448 6150 6274 8620 Landing gears 6322 8740 6382 4140 6415 E4340 Propellers, spiders, hubs, and barrels 6415 E4340 Springs 6450 6150 Dimensions of deformed and plain concrete-reinforcing bars of standard sizes Table 7 Dimensions of deformed and plain...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006014
EISBN: 978-1-62708-172-6
.... Fig. 3 White metal surface blast cleaned in accordance with SSPC-SP 5. Courtesy of KTA-Tator, Inc. Fig. 10 Calcium chloride test on concrete floor. Courtesy of KTA-Tator, Inc. Fig. 8 Corrosion of steel reinforcement in concrete. Courtesy of KTA-Tator, Inc. Fig. 9...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004161
EISBN: 978-1-62708-184-9
.... and Butalia T.S. , Use of High Volume Fly Ash Mixes in Preventing Corrosion in Concrete , International Ash Utilization Symposium , University of Kentucky , accessed at http://www.flyash.org , January 2005 Selected References Selected References • Cuddon A.C. and Allen C...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003697
EISBN: 978-1-62708-182-5
... applications. Ceramic anodes, also called mixed metal oxide anodes, are the newest materials available for anodes. They are supplied either as oxide coatings on transition metal substrates or as bulk ceramics. Their use as cathodic protection anodes for protecting reinforcing steel in concrete is new...