Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003592
EISBN: 978-1-62708-182-5
... Abstract Electrode potential is a key parameter in the thermodynamic and kinetic processes that drive aqueous corrosion. This article discusses the complexities associated with measuring electrode potential and explains where and how to use reference electrodes to improve measurement accuracy...
Book Chapter

Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003799
EISBN: 978-1-62708-183-2
... Abstract This article discusses a tool for the conversion of measurements made against various reference electrodes at different temperatures. It reviews different electrode potential temperature coefficients, namely, isothermal temperature coefficient and thermal temperature coefficient...
Image
Published: 01 January 2003
Fig. 3 Schematic of silver-silver chloride and calomel reference electrodes. Source: Ref 12 More
Image
Published: 01 January 2003
Fig. 6 Diagram of potential conversion between reference electrodes. SHE, standard hydrogen electrode; CuSO 4 , copper-copper sulfate electrode. SHE, standard hydrogen electrode More
Image
Published: 01 January 2003
Fig. 2 Experimental electrochemical reference electrodes to simultaneously measure sodium and oxygen activities and thereby, melt basicity. (a) Ag/Ag + electrode. (b) ZrO 2 electrode. Source: Ref 3 , 5 , 6 More
Image
Published: 01 January 1986
Fig. 3 Schematic of reference electrodes. (a) Single junction. (b) Double junction More
Image
Published: 01 January 2003
Fig. 3 Probe installation in ballast tank with zinc anodes, reference electrodes, and data logger. Source: Ref 11 More
Image
Published: 01 January 2003
Fig. 27 Example 3 . Placement of reference electrodes More
Image
Published: 15 December 2019
Fig. 28 Schematics of reference electrodes. (a) Single junction. (b) Double junction More
Image
Published: 01 January 2006
Fig. 5 Basic E log I test. CSE, copper/copper-sulfate reference electrode; dc, direct current. More
Image
Published: 01 January 2003
Fig. 2 Schematic of a copper/copper sulfate reference electrode More
Image
Published: 01 January 2003
Fig. 9 Copper-saturated copper sulfate reference electrode More
Image
Published: 01 January 2003
Fig. 3 Test cell for flat sheet electrodes. CE, counter electrode; RE, reference electrode; WE, working electrode More
Book Chapter

By Mark A. Arnold
Series: ASM Handbook Archive
Volume: 10
Publisher: ASM International
Published: 01 January 1986
DOI: 10.31399/asm.hb.v10.a0001740
EISBN: 978-1-62708-178-8
... membrane electrodes, and discusses important elements that must be considered in addition to the potentiometric membrane electrode to ensure proper electrode response. These elements are reference electrodes, temperature controls, recording of the potential with respect to time, electrode storages...
Book Chapter

By Kurt H. Stern
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003581
EISBN: 978-1-62708-182-5
...: reference electrodes and indicator electrodes. It explains that corrosion in molten salts can be caused by the solubility of the metal in the salt, particularly if the metal dissolves in its own chloride. The article describes the factors that affect the corrosion of titanium, namely, the titanium chloride...
Image
Published: 01 January 2003
Fig. 6 R sn (ω) versus frequency compared to two times the impedance | Z (ω)| versus frequency for iron in 1 M Na 2 SO 4 at pH 4 with a “noisy” iron reference electrode. Impedance measurements performed in a two-electrode cell with two iron electrodes produced 2| Z (ω)|. R sn (ω More
Image
Published: 01 January 2003
Fig. 3 Schematic of an anodic protection system. One or more cathodes, a reference electrode, a potential sensing and controlling circuit, and a dc power supply are required for each anodic protection system. The vessel wall is made the anode of the circuit by current forced between More
Book Chapter

By Drew Hevle, Angel Kowalski
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004112
EISBN: 978-1-62708-184-9
... potentials. Additional relevant characteristics of the voltmeter are range, resolution, and accuracy. Reference Electrodes The choice of reference electrodes is determined by the environment in which the electrode is placed. For onshore surveys the most commonly used is the copper/copper-sulfate...
Book Chapter

By Carl E. Locke, Jr.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003696
EISBN: 978-1-62708-182-5
... that exhibit very interesting behavior when subjected to anodic polarization. This behavior can be studied with an experimental setup, which is shown in block-diagram fashion in Fig. 1 . When the potential of the working electrode relative to the reference electrode is controlled and shifted in the more...
Book Chapter

By Ernest W. Klechka, Jr.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004113
EISBN: 978-1-62708-184-9
... should be part of the operating procedures for the AST or UST. The size, type, and location of anodes and reference electrodes are determined during design. Potential interference with external liners (for product release control) and buried piping should be considered. Electrical interference...