Fig. 10 Pushpin testing. (a) Pushpin test setup using the Gleeble. UAM, ultrasonic additive manufacturing. Source: Ref 12 . (b) Schematic of the pushpin test showing specimen dimensions. More
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006574
EISBN: 978-1-62708-290-7
... with a discussion on the process fundamentals and process parameters of UAM. It then describes metallurgical aspects in UAM. The article provides a detailed description of a wide range of mechanical characterization techniques of UAM, namely tensile testing, peel testing, and pushpin testing. The article ends...