1-20 of 1418

Search Results for protective lining

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003684
EISBN: 978-1-62708-182-5
... Abstract Inorganic chemical-setting ceramic linings are one of the most widely used construction materials in designing the protective linings for industrial installations. Monolithic linings can be applied by cast or gunite (shotcreting) methods over steel or concrete as well as brick...
Image
Published: 01 January 2003
Fig. 11 Magnesium anode used to cathodically protect glass-lined steel water heater More
Book Chapter

By Harry R. Hanson
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003608
EISBN: 978-1-62708-182-5
... that is cathodically protected, if a foreign pipeline crosses or passes close to the protected pipeline, current from the cathodic protection system can gather onto the foreign pipeline and then be discharged from the foreign line when it crosses or comes close to the protected pipeline. This is particularly true...
Book Chapter

By Dudley J. Primeaux, II
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006047
EISBN: 978-1-62708-172-6
... Abstract Two-component polyurea elastomeric coating/lining systems are the newest technology in the protective coating/lining industry and a wide variety of applications have been developed. These include coating/lining applications over concrete, geotextile membranes, various metals...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006009
EISBN: 978-1-62708-172-6
... and vinyl ester coatings, namely, curing systems, thixotropic agents and fillers. It exemplifies polyester and vinyl ester coating, lining and flooring systems that are used for top-to-bottom protection of industrial plants and equipment. The article also highlights the concerns to be addressed when using...
Book Chapter

By Kenneth B. Tator
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006027
EISBN: 978-1-62708-172-6
... Abstract This article provides a brief discussion on the common types of overlayers that can be used on a metal surface to protect it from corrosion. These overlayers include phosphate, chromate, and chromate-free conversion coatings; hot dip galvanizing; cementitious linings; glass...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004121
EISBN: 978-1-62708-184-9
.... These include protective coatings and linings, cathodic protection, advanced materials selection and design, water treatment, equipment inspection and monitoring, and below-grade moisture mitigation. cathodic protection corrosion control corrosivity equipment inspection advanced materials selection...
Book Chapter

By Russell D. Kane
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004210
EISBN: 978-1-62708-184-9
... and gas gathering lines at bends and joints or in flow-control valves and wellhead equipment by produced sand is probably the other most common occurrence of erosion in oil and gas production. Erosion-Corrosion Strictly speaking, in erosion-corrosion, only the protective corrosion product film...
Book Chapter

By E. Bud Senkowski
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006035
EISBN: 978-1-62708-172-6
... the following tests that replicate immersion conditions on installed linings: ASTM D6943, “Standard Practice for Immersion Testing of Industrial Protective Coatings” ( Ref 6 ) NACE TM0174-2002, “Laboratory Methods for the Evaluation of Protective Coatings and Lining Materials on Metallic Substrates...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006016
EISBN: 978-1-62708-172-6
... and installation of the protective coating/lining system. Prior to beginning surface-preparation operations, many specifications will require a presurface-preparation inspection to verify the correction of fabrication defects and removal of surface contamination such as grease, oil, cutting compounds, lubricants...
Book Chapter

By Kenneth B. Tator
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003691
EISBN: 978-1-62708-182-5
... of the Environmental Protection Agency and the Occupational Safety and Health Administration as well as the corresponding Code of Federal Regulation numbers. coating lining material surface preparation THE TOTAL NATIONAL YEARLY COST of metallic corrosion in the United States was estimated at $275 billion...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006059
EISBN: 978-1-62708-172-6
... or internal protective coatings or linings other than the cement mortar coating or concrete core included in their original manufacture. The ductile iron option (up to 110 cm, or 42 in., in diameter) typically includes internal cement mortar or epoxy linings and external polyethylene encasement for corrosion...
Book Chapter

By E. Bud Senkowski, Kenneth B. Tator
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003695
EISBN: 978-1-62708-182-5
... as a Protective Lining Since 1839, when Charles Goodyear discovered the process known as vulcanization , whereby a soft, amorphous mass of natural rubber cross-linked into a resilient, elastomeric material with excellent elongation, modulus, and tensile strength, rubber has been used as a material...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003549
EISBN: 978-1-62708-180-1
... in the environment; change in the alloy or heat treatment; change in design; use of galvanic protection; use of inhibitors; use of nonmetallic coatings and liners; application of metallic coatings; use of surface treatments, thermal spray, or other surface modifications; corrosion monitoring; and preventive...
Image
Published: 30 August 2021
Fig. 18 Metal consumption over time for an alloy forming a protective scale under various turbine cycling conditions. The solid black line indicates metal consumption in a thermal cycling regime, with each parabola representing oxidation after effective loss of the protective oxide layer More
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006040
EISBN: 978-1-62708-172-6
... for associated pump stations and piping, as discussed subsequently. Earthen-berm reservoirs are typically lined with sheet linings composed of polyethylene or other types of thermoplastic or synthetic rubber to prevent water leakage. Most concrete reservoirs are not coated for corrosion protection, because...
Image
Published: 01 January 2003
Fig. 1 Schematic of a chemical-resistant dual-lining system that provides double protection to the substrate in the form of a flexible membrane and a rigid surface layer. The flexible corrosion-resistant membrane is applied in direct contact with steel or concrete substrates More
Book Chapter

By Hiroyuki Tanabe
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003809
EISBN: 978-1-62708-183-2
... Abstract This article describes the paint systems generally used to protect steel structures, steel sheet, and bridges from corrosion, and how they deter corrosion. It provides a discussion on the basic design criteria of steel structures for corrosion protection. The article also explains...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003840
EISBN: 978-1-62708-183-2
... and uses of these materials. ceramics organic coatings concrete elastomers nonmetallic materials plastics protective coatings refractories thermosetting resins resin-matrix composites rubber linings WHEN PEOPLE THINK OF CORROSION, they sometimes attribute such degradation to only...
Book Chapter

By W. Brian Holtsbaum
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004115
EISBN: 978-1-62708-184-9
... to: Cathodic protection (CP) ( Ref 3 , 4 , 5 ) High voltage dc (HVDC) power lines ( Ref 6 ) Transit systems ( Ref 1 , 7 , 8 , 9 ) Direct current operated mining equipment Electric railways Welding, both onshore and offshore ( Ref 10 ) Electroplating or battery-charging equipment...