1-20 of 600

Search Results for properties of refractory metals

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006123
EISBN: 978-1-62708-175-7
... Abstract This article focuses on the selection, properties, and applications of powder metallurgy refractory metals and their alloys, including tungsten, molybdenum, tantalum, niobium, and rhenium. molybdenum niobium powder metallurgy refractory metals rhenium tantalum tungsten...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003151
EISBN: 978-1-62708-199-3
... oxidizing aerospace applications. This article discusses the properties, processing, applications, and classes of refractory metals and its alloys, namely molybdenum, tungsten, niobium, tantalum and rhenium. It also provides an outline of the coating processes used to improve their oxidation resistance...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001079
EISBN: 978-1-62708-162-7
... temperatures and lowest vapor pressures of all metals. The refractory metals are readily degraded by oxidizing environments at moderately low temperatures, a property that has restricted the applicability of the metals in low-temperature or nonoxidizing high-temperature environments. Protective coating systems...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005167
EISBN: 978-1-62708-186-3
... Abstract This article describes the formability and surface contamination of the refractory metals such as niobium, tantalum, molybdenum, tungsten, and titanium-zirconium-molybdenum alloys. It reviews the factors that affect mechanical properties and formability during rolling and heat...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001456
EISBN: 978-1-62708-173-3
... titanium, zirconium, and beryllium, have in common the ability to form stable oxides at elevated temperatures. These diverse groups of metals have a wide range of mechanical and physical properties ( Table 1 ). Selected physical properties of reactive and refractory metals Table 1 Selected physical...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006133
EISBN: 978-1-62708-175-7
... for common metal cutting operations; thus equipment must be more rigid and have greater torque to ensure optimal results. Carbide and, on occasion, cast cobalt tools give acceptable tool life and cutting properties. Tool sharpness is critical to cut refractory metals cleanly. Worn tools can tear the material...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003840
EISBN: 978-1-62708-183-2
... coatings, concrete, refractories, and ceramics. Indeed, sometimes the demarcation between nonmetals and metals is not distinct, because some nonmetals may duplicate properties found in metals. Sometimes, the interaction of nonmetallic materials with environments, both how the properties of the nonmetallic...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003841
EISBN: 978-1-62708-183-2
... decarburization vessel. After secondary refining, the molten metal is transported to a tundish for casting. Each furnace is lined with refractory materials. Usually, a practice called zoning is used, where refractories with different properties are used in different areas of the same vessel to resist...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001426
EISBN: 978-1-62708-173-3
... temperatures, a property that has restricted the applicability of the metals in low-temperature or nonoxidizing high-temperature environments. This article is limited to a discussion of special metallurgical considerations during the fusion welding of refractory metal alloys. These alloys are discussed...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003051
EISBN: 978-1-62708-200-6
... and advanced manufacturing techniques are often used where these materials are employed. This article examines several traditional ceramics, including structural clay, whiteware, glazes, enamels, portland cements, and concrete. It also provides a detailed account of fabrication methods, properties...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006091
EISBN: 978-1-62708-175-7
..., properties, and performance of electrical contacts based on PM or hybrid composite technologies with refractory metals and compounds. These metals and compounds include tungsten, molybdenum, carbide-based composites, and silver-base composites. The article explains composite manufacturing methods, namely, PM...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003221
EISBN: 978-1-62708-199-3
... Abstract This article discusses surface engineering of nonferrous metals including aluminum and aluminum alloys, copper and copper alloys, magnesium alloys, nickel and nickel alloys, titanium and titanium alloys, zirconium and hafnium, zinc alloys, and refractory metals and alloys. It describes...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006121
EISBN: 978-1-62708-175-7
.... The effects of processing conditions on the physical and chemical properties of tungsten, molybdenum, tantalum, niobium, and rhenium powders are reviewed. chemical properties molybdenum powders niobium powders physical properties powder production refractory metal powders rhenium powders tantalum...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 31 January 2025
DOI: 10.31399/asm.hb.v13b.a0007042
EISBN: 978-1-62708-183-2
...), and the needed properties to be used at various temperatures and temperature gradients, all of which is dependent on the “know-how” of the manufacturer to produce the proper microstructure. Refractories and structural ceramics are generally thought to be inert and corrosion resistant (as compared to metallic...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003551
EISBN: 978-1-62708-180-1
... those chemical and physical properties that make them applicable for structures, or as components of systems, that are exposed to environments above 538 °C (1000 °F).” Nowadays, refractories are made of not only oxides and nonoxide compounds (carbides, nitrides, and carbons), but also of metallic...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003180
EISBN: 978-1-62708-199-3
... Abstract Characteristics of stainless steel that affect its formability include yield strength, tensile strength, and ductility, in addition to the effect of work hardening on these properties. This article discusses the forming process of stainless steel, heat-resistant alloys and refractory...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005198
EISBN: 978-1-62708-187-0
... and in a wide variety of traditional and specialized shapes. There is no direct impingement of the flame on the metal, and the heat loss to the outside is limited by the refractory walls. However, the energy efficiency of the crucible furnace can be low (7 to 19%), with over 60% of the heat loss attributed...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.9781627081832
EISBN: 978-1-62708-183-2
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002463
EISBN: 978-1-62708-194-8
... application at quite high temperatures in many oxidizing and reducing environments. Ceramics are usually thermal and electrical insulators, but unlike metals these properties can often be varied independently with composition and microstructure control. Materials such as aluminum nitride and beryllia can show...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005193
EISBN: 978-1-62708-187-0
... in nonferrous alloys. In almost all instances of metal casting, they are considered to be detrimental to the performance of the cast component. For example, mechanical properties can be adversely influenced by inclusions, which act as stress raisers. There is no set pattern for the effect, but some...