1-7 of 7 Search Results for

prepriming techniques

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 December 2008
Fig. 1 Prepriming techniques for (a) the basin, using a stopper, (b) the basin and sprue, and (c) the whole filling system. All of the prepriming methods can use devices such as mechanical valves or fusible bursting discs. More
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005221
EISBN: 978-1-62708-187-0
... features of the system. entrainment defects naturally pressurized filling system gravity-poured castings prepriming techniques filters mold-filling designs FILLING the casting cavity with molten metal can be accomplished in various ways. Filling methods differ among the various casting...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001012
EISBN: 978-1-62708-161-0
..., and service life of the host material. The article covers metallic coatings, including zinc, aluminum, zinc-aluminum alloys, tin, and terne; pretreatment or phosphate coatings; and preprimed and painted finishes based on organic coatings. aluminum coatings aluminum-zinc alloy coatings hot dip process...
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0009017
EISBN: 978-1-62708-187-0
... generation are increased. Techniques for prepriming and countergravity flow are discussed in the article “Filling and Feeding System Concepts.” Pressurized versus Unpressurized Systems The difference between these two systems is in the choice of the location of the flow-controlling constriction...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003094
EISBN: 978-1-62708-199-3
... are used primarily in consumer goods. These applications require materials that are serviceable under a wide variety of conditions and that are especially adaptable to low-cost techniques of mass production into articles having good appearance. Therefore, these products must incorporate, in various degrees...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006492
EISBN: 978-1-62708-207-5
... is somewhat rough, depending on the fabrication techniques used. These and other highly localized aluminum oxide layer surface variabilities can cause different physical, chemical, and electrochemical behavior, which, in a moist marine or chemical environment, has the potential to initiate or accelerate...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.9781627081993
EISBN: 978-1-62708-199-3