EISBN: 978-1-62708-210-5
... Abstract Alloy 354.0 was designed especially for premium engineered casting applications requiring high-tensile properties and elongation. This datasheet provides information on key alloy metallurgy, fabrication characteristics, processing effects on physical and mechanical properties, and...
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005287
EISBN: 978-1-62708-187-0
... principles in casting. The article concludes with information on premium engineered castings that provide higher levels of quality and reliability than in conventionally produced castings. aluminum casting alloys centrifugal casting die casting lost foam casting gravity casting investment casting...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003127
EISBN: 978-1-62708-199-3
... factors affecting the selection of casting process and the general designation system for aluminum alloys. It provides useful information on mechanical test methods, selection of proper test specimens for accurate test methods, characteristics of premium engineered castings, and advantages of hot...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006555
EISBN: 978-1-62708-210-5
... 0.10 Zn 0.10 max 0.10 max 0.10 max Other (each), max 0.05 0.05 0.05 Other (total), max 0.15 0.15 0.15 Al bal bal bal Typical physical and tensile mechanical properties are given in Tables 2 and 3 . Alloys A206.0 and B206.0 are produced as premium engineered casting...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006572
EISBN: 978-1-62708-210-5
... Abstract Alloy 362.0, low-iron premium die-casting alloy, is made from recycled secondary metal scrap and was developed to have equivalent or better mechanical properties than Silafont-36 and/or Aural-2. This datasheet provides information on key alloy metallurgy, processing effects on physical...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006554
EISBN: 978-1-62708-210-5
... properties for specimens taken from commercial castings of premium engineered Alloy A201.0-T7 Property Designated location Undesignated location Class 1 and 2 strength Class 10 strength Class 11 strength Ultimate strength, MPa (ksi) 414 (60) 414 (60) 386 (56) Yield strength, MPa (ksi...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001082
EISBN: 978-1-62708-162-7
... premium investment cast and hot isostatic pressed parts. As indicated previously ( Table 5 ), substantial work has been done in recent years to modify the microstructure of cast parts to produce fatigue properties either equivalent or superior to the best wrought-annealed products. Figure 11(a) compares...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005331
EISBN: 978-1-62708-187-0
... approximately 0.70% Mg, beyond which either no further strengthening occurs or matrix softening takes place. Common premium-strength compositions in the aluminum-silicon family employ magnesium in the range of 0.40 to 0.070% (see the section “Premium Engineered Castings” in this article). Binary aluminum...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002407
EISBN: 978-1-62708-193-1
...) castings combine a number of conventional casting procedures in a selective manner to provide premium strength, soundness, dimensional tolerances, surface finish, or a combination of these characteristics. As a result, premium engineered castings typically have somewhat higher fatigue resistance than...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005337
EISBN: 978-1-62708-187-0
... tubes, missile wings, and hot gas nozzles. As the more precise investment casting technology developed and the commercial use of HIP became a reality in the mid-1970s, titanium casting applications quickly expanded into critical airframe ( Fig. 12 ) and gas turbine engine ( Fig. 13 ) components. The...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006329
EISBN: 978-1-62708-179-5
.... Pig iron is considered a premium charge material because of its uniformity of composition and size, and it is free of detrimental tramp elements. In the early years, pig iron was the predominant charge component for ensuring quality iron with sufficient carbon content and low quantities of detrimental...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006548
EISBN: 978-1-62708-210-5
... Abstract This article aims to comprehensively review and summarize the material properties and engineering data for aluminum alloy castings and their many applications. The discussion focuses on conventional sand, permanent mold, and die castings as well as the premium engineered versions of...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001061
EISBN: 978-1-62708-162-7
... spacing to some extent, the only efficient way of ensuring fine spacing is use of rapid cooling. Fig. 3 Tensile properties versus dendrite cell size for four heats of aluminum alloy A356-T62 plaster cast plates In premium engineered castings and in many other casting applications, careful...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006524
EISBN: 978-1-62708-207-5
... also are grouped into various types of application categories, such as pistons, rotors, and premium castings. The major factors that influence alloy selection for casting applications include the casting process to be used, casting design, required properties, and economic (and availability...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003508
EISBN: 978-1-62708-180-1
... for failures of the first type, and the founder the second. No such distinction should be drawn. The key to serviceable castings is communication between the designer and the foundry engineers. Foundrymen are an invaluable source of information on just what can be produced in cast form, both in terms...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003121
EISBN: 978-1-62708-199-3
... pans; typewriter frames; engine parts 332.0 Automotive and heavy-duty pistons; pulleys, sheaves 333.0 Gas meter and regulator parts; gear blocks; pistons; general automotive castings 354.0 Premium-strength castings for the aerospace industry 355.0 Sand: air compressor pistons; printing...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001057
EISBN: 978-1-62708-162-7
... pattern and mold or die design. Premium engineered castings display extreme integrity, close dimensional tolerances, and consistently controlled mechanical properties in the upper range of existing high-strength capabilities for selected alloys and tempers. Fig. 6 U.S. casting shipments from 1978...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003007
EISBN: 978-1-62708-200-6
... match structure in equal sections. Super-premium thermoplastics compete on cost basis. Brass or bronze Cast Machined Usually, for saltwater resistance. Several thermoplastics and thermoset materials compete successfully. Magnesium Cast Machined For light weight requirement. Several plastics...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002484
EISBN: 978-1-62708-194-8
... metal to feed shrinkage that occurs during solidification. There are a number of excellent summaries of principles of good casting design ( Ref 6 , 7 , 8 ), and a comprehensive booklet was published on design of premium quality aluminum alloy castings ( Ref 9 ). This latter publication also includes...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002178
EISBN: 978-1-62708-188-7
...) 0.13 (0.005) S4, S5 (M2, M3) 82 (270) 95 (315) 0.20 (0.008) P20, M20 (C-6) 130 (425) 0.20 (0.008) CP20, CM20 (CC-6) 2.5 (0.100) 18 (60) 0.30 (0.012) S4, S5 (M2, M3) 64 (210) 75 (245) 0.40 (0.015) P30, M30 (C-6) 95 (315) 0.30 (0.012) CP30, CM30 (CC-6) (a) Any premium high...