Published: 01 January 2005
Fig. 5 Spur gear forgings made by precision flashless forging More
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003986
EISBN: 978-1-62708-185-6
... of the key factors that impact the precision forging process. It provides information on the achievable tolerances and presents examples of precision forging. A discussion on forging of bevel gears/spiral bevel gears is also presented. axle shafts bevel gears precision flashless forging precision...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004037
EISBN: 978-1-62708-185-6
... corrosion in service. Examples of parting line designs that enhance resistance to stress corrosion are given in the following section. Parting Line and Seamless (Flashless) Cylindrical Forgings Cylindrical forgings commonly have a straight parting line located in a diametral plane. For typical hammer...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003183
EISBN: 978-1-62708-199-3
..., precision forging, and cold forging. computer-aided design die design forging processes materials selection types of hammers types of presses Hammers and Presses for Forging FORGING MACHINES fall into three categories according to their method of operation. Mechanical forging presses...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003973
EISBN: 978-1-62708-185-6
...-blow dwell time, quantity of blows, etc.) can be engineered for best control of adiabatic heating, die chilling, strain, strain rate, recrystallization, and grain growth. The engineered processing steps are precisely controlled by the computerized forging hammer controls, which also allow...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005144
EISBN: 978-1-62708-186-3
... and the lubricants used in the processes. It discusses the various forming processes of magnesium alloys. These include press-brake forming, deep drawing, manual and power spinning, rubber-pad forming, stretch forming, drop hammer forming, and precision forging. cold forming deep drawing drop hammer forming...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.9781627081962
EISBN: 978-1-62708-196-2
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.9781627081993
EISBN: 978-1-62708-199-3