EISBN: 978-1-62708-173-3
... Abstract This article commences with a brief description of the solidification characteristics and microstructures of martensitic precipitation hardening (PH) stainless steels. It reviews the welding parameters for types 17-4PH, 15-5PH, PH13-8 Mo, Custom 450, and Custom 455. The article...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000612
EISBN: 978-1-62708-181-8
... Abstract This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of precipitation-hardening stainless steels and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the cup-and-cone tension-overload...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005961
EISBN: 978-1-62708-168-9
..., and protective atmospheres used in heat treatment of iron-base precipitation-hardenable (PH) superalloys. It focuses on various factors to be considered in heat treating of PH stainless steels: cleaning prior to heat treatment, furnace atmospheres, time-temperature cycles, variations in cycles, and scale removal...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003203
EISBN: 978-1-62708-199-3
... (a) Cooling from the annealing temperature must be rapid, but it also must be consistent with limitations of distortion. Heat treatment of precipitation-hardening stainless steels Table 6 Heat treatment of precipitation-hardening stainless steels Alloy Condition code Solution anneal...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005673
EISBN: 978-1-62708-198-6
..., martensitic stainless steels, ferritic stainless steels, precipitation-hardening stainless steels, and duplex stainless steels. It contains a table lists common medical device applications for stainless steels. The article discusses the physical metallurgy, and physical and mechanical properties...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001046
EISBN: 978-1-62708-161-0
... Abstract This article discusses the composition, characteristics, and properties of the five groups of wrought stainless steels: martensitic stainless steels, ferritic stainless steels, austenitic stainless steels, duplex stainless steels, and precipitation-hardening stainless steels...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003812
EISBN: 978-1-62708-183-2
... steels, as defined by the crystallographic structure. These include ferritic stainless steels, austenitic stainless steels, martensitic stainless steels, and precipitation-hardening stainless steels. The mechanism of corrosion protection for stainless steels is reviewed. The article examines the effects...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003992
EISBN: 978-1-62708-185-6
... of austenitic stainless steels, martensitic stainless steels, precipitation-hardening stainless steels, and ferritic stainless steels. It concludes with a discussion on the heating and lubrication of dies. austenitic stainless steel cleaning dies ferritic stainless steel forgeability forging forging...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005977
EISBN: 978-1-62708-168-9
..., ferritic, austenitic, duplex (ferritic-austenitic), and precipitation-hardening stainless steels. It presents a checklist of characteristics to be considered in selecting the proper type of stainless steel for a specific application. The article also outlines the need to promote the formation...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002403
EISBN: 978-1-62708-193-1
...; 17-7PH, PH15-7Mo and AM355 are semiaustenitic precipitation hardening types; and A286 is an austenitic precipitation hardening type. Table 2 Typical tensile properties and fatigue limits of stainless steels Material Mechanical properties Ultimate tensile strength, ksi Tensile...