Skip Nav Destination
Close Modal
By
Robert H. Heidersbach, James Brandt, David Johnson, John S. Smart, III, John S. Smart
Search Results for
precious metal alloys
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 141 Search Results for
precious metal alloys
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003776
EISBN: 978-1-62708-177-1
..., and copper. gold jewelry alloys intermetallic gold compounds iridium alloys metallographic preparation metallographic samples metallography microstructure platinum jewelry alloys platinum-aluminum-copper alloys platinum-base alloys precious metals ruthenium alloys shape memory alloys...
Abstract
This article explains how to prepare precious metal test samples for metallographic examination. It discusses cutting, mounting, grinding, polishing, and etching and addresses some of the challenges of working with small, relatively soft specimens. It includes dozens of example micrographs, comparing and contrasting the microstructural features of gold, platinum, iridium, palladium, and ruthenium-base alloys. It examines pure gold, intermetallic gold compounds, gold and platinum jewelry alloys, platinum-containing shape memory alloys, and alloys consisting of platinum, aluminum, and copper.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003150
EISBN: 978-1-62708-199-3
... Abstract Precious metals include gold, silver, and six platinum-group metals, namely, platinum, palladium, ruthenium, rhodium, osmium, and iridium. This article focuses on the consumption, trade practices, properties, product forms, and applications of these metals and their alloys. gold...
Book: Corrosion: Materials
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003829
EISBN: 978-1-62708-183-2
... “Properties of Precious Metals,” Properties and Selection: Nonferrous Alloys and Special-Purpose Materials , Volume 2, ASM Handbook , 1990. This will aid in assessing the relevance of any particular noble metal to a given application. Atomic, structural, and physical properties can also play an important...
Abstract
This article characterizes the corrosion resistance of precious metals, namely, ruthenium, rhodium, palladium, silver, osmium, iridium, platinum, and gold. It provides a discussion on the general fabricability; atomic, structural, physical, and mechanical properties; oxidation and corrosion resistance; and corrosion applications of these precious metals. The article also tabulates the corrosion rates of these precious metals in corrosive environment, namely, acids, salts, and halogens.
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006259
EISBN: 978-1-62708-169-6
... Abstract This article describes the annealing behavior of precious metals, namely, gold, silver, platinum, palladium, iridium, rhodium, ruthenium, and osmium. It discusses the annealing practices and their effect on the basic properties of common precious metal alloys. The article presents...
Abstract
This article describes the annealing behavior of precious metals, namely, gold, silver, platinum, palladium, iridium, rhodium, ruthenium, and osmium. It discusses the annealing practices and their effect on the basic properties of common precious metal alloys. The article presents the typical properties and compositions of silver-copper alloys and gold jewelry alloys such as colored gold alloys and white gold alloys.
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001454
EISBN: 978-1-62708-173-3
... Abstract Copper, copper alloys, and precious metals are probably the most easily brazed metals because of their resistance to oxidation at high temperatures. This article provides a brief discussion on the metallurgy of copper, copper alloys, and precious metals and discusses the filler metals...
Abstract
Copper, copper alloys, and precious metals are probably the most easily brazed metals because of their resistance to oxidation at high temperatures. This article provides a brief discussion on the metallurgy of copper, copper alloys, and precious metals and discusses the filler metals, brazing fluxes, joint clearance and design, and different brazing processes used in brazing of copper, copper alloys, and precious metals.
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006556
EISBN: 978-1-62708-290-7
... circulation than the burnout cycles for conventional waxes ( Ref 7 , 8 ). Deoxidizing the melt reduces gas bubble formation, which can create defects when the precious metal alloy encounters any carbonaceous residue from incomplete burnouts (Ref 9). Curing of the printed photocurable pattern...
Abstract
The additive manufacturing technologies in the casting of precious metals are divided into two groups: indirect metal methods and direct metal methods. Besides providing a process overview of both of these methods, the focus of this article is on the characteristics, process steps, applications, and advantages of direct metal methods, namely laser melting, material extrusion, binder jetting, material jetting, and vat photopolymerization methods.
Book Chapter
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001087
EISBN: 978-1-62708-162-7
... Abstract Precious metals are of inestimable value to modern civilization. This article discusses the resources and consumption, trade practices, and special properties of precious metals and its alloys, including ruthenium, rhodium, palladium, silver, osmium, iridium, platinum, and gold...
Abstract
Precious metals are of inestimable value to modern civilization. This article discusses the resources and consumption, trade practices, and special properties of precious metals and its alloys, including ruthenium, rhodium, palladium, silver, osmium, iridium, platinum, and gold, and tabulates the industrial applications of precious metals. It provides information on the commercial forms (wire, rod, sheet, strip, ribbon, and foil) and uses of precious metals, including semifinished products, precious metal powders, industrial uses, coatings, and jewelry.
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005670
EISBN: 978-1-62708-198-6
... on the ancient history of noble and precious metal use in dentistry is provided. The article discusses the use of direct gold dental filling materials, direct silver dental filling materials, traditional amalgam alloys, high-copper amalgam alloys, and gallium alloys in biomedical applications. It also provides...
Abstract
This article focuses on the use of noble and precious metals for biomedical applications. These include gold, platinum, palladium, ruthenium, rhodium, iridium, and osmium. The physical and mechanical properties of noble and precious metals are presented in tables. A brief discussion on the ancient history of noble and precious metal use in dentistry is provided. The article discusses the use of direct gold dental filling materials, direct silver dental filling materials, traditional amalgam alloys, high-copper amalgam alloys, and gallium alloys in biomedical applications. It also provides information on gold coatings and iridium oxide coatings for stents.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001252
EISBN: 978-1-62708-170-2
... of Cyanide? , Trans. Inst. Met. Finish. , Vol 69 ( No. 3 ), p 8 – 10 • “Bath for Electroplating of Precious Metal Alloys,” German Patent No. DE 2445538 , 1976 • Blair A. , Formulating High Speed Gold and Silver , Met. Finish. , May 1986 , p 13 – 15 • Blair...
Book Chapter
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005442
EISBN: 978-1-62708-196-2
... Abstract This article contains a table that lists the density of metals and alloys. It presents information on aluminum, copper, iron, lead, magnesium, nickel, tin, titanium, and zinc, an their respective alloys. Information on wrought alloys, permanent magnet materials, precious metals...
Abstract
This article contains a table that lists the density of metals and alloys. It presents information on aluminum, copper, iron, lead, magnesium, nickel, tin, titanium, and zinc, an their respective alloys. Information on wrought alloys, permanent magnet materials, precious metals, and rare earth metals is also listed.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004182
EISBN: 978-1-62708-184-9
... alloys, precious metals, and non-metals. The article also discusses the hydrogen blistering and stress-corrosion cracking of carbon steels in high-temperature HF and AHF. low-alloy steel carbon steel austenitic stainless steel nickel-rich austenitic stainless steel copper alloys corrosion...
Abstract
This article provides the corrosion data for materials in hydrofluoric acid (HF) and anhydrous hydrogen fluoride (AHF). These materials include carbon and low-alloy steels, austenitic stainless steels, nickel-rich austenitic stainless steels, nickel and nickel-base alloys, copper alloys, precious metals, and non-metals. The article also discusses the hydrogen blistering and stress-corrosion cracking of carbon steels in high-temperature HF and AHF.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003082
EISBN: 978-1-62708-199-3
... Abstract This article contains tables that present engineering data for the following metals and their alloys: aluminum, copper, iron, lead, magnesium, nickel, tin, titanium, zinc, precious metals, permanent magnet materials, pure metals, rare earth metals, and actinide metals. Data presented...
Abstract
This article contains tables that present engineering data for the following metals and their alloys: aluminum, copper, iron, lead, magnesium, nickel, tin, titanium, zinc, precious metals, permanent magnet materials, pure metals, rare earth metals, and actinide metals. Data presented include density, linear thermal expansion, thermal conductivity, electrical conductivity, resistivity, and approximate melting temperature. The tables also present approximate equivalent hardness numbers for austenitic steels, nonaustenitic steels, austenitic stainless steel sheet, wrought aluminum products, wrought copper, and cartridge brass. The article lists conversion factors classified according to the quantity/property of interest.
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001118
EISBN: 978-1-62708-162-7
... generalizations concerning the U.S. and world aluminum industries can be made: The aluminum industry today is truly international. Primary aluminum is produced in virtually every global region, and the metal produced competes in global markets. Aluminum alloy scrap is now traded internationally as well...
Abstract
Many nonferrous metals, including aluminum, nickel, copper, and others, are among the few materials that do not degrade or lose their chemical or physical properties in the recycling process. As a result, these metals can be recycled an infinite number of times. This article focuses on the recycling of nonferrous alloys, namely, aluminum, copper, magnesium, tin, lead, zinc, and titanium, providing details on the sources, consumption and classification of scrap, and the technological trends and developments in recycling.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003157
EISBN: 978-1-62708-199-3
..., and the method of attachment, all of which affect the size of the contact required for a specific application. To conserve precious metal, the contact materials, carrier material, and method of attachment must be optimized. Some high-strength, high-conductivity copper alloys are used for carriers because...
Abstract
Electrical contacts are metal devices that make and break electrical circuits. This article describes the property requirements such as electrical conductivity, mechanical properties, chemical properties, fabrication properties, and thermal properties of make-break arcing contacts. The article also focuses on brush contact materials and their interdependence factors for sliding contacts. In addition, the article discusses the properties, manufacturing methods, and applications of electrical contact materials, including wrought materials such as copper metals, silver metals, gold metals, precious metal overlays, tungsten, molybdenum, and aluminum, and composite materials. It concludes by discussing the composite manufacturing methods such as infiltration, press-sinter, press-sinter-repress process, press-sinter-extrude process, internal oxidation, and preoxidized-press-sinter-extrude process, and coprecipitation.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003222
EISBN: 978-1-62708-199-3
... Abstract This article focuses on the recycling of metals including iron and steel, stainless steel, superalloys, nickel, aluminum, copper, precious metals, lead, magnesium, tin, titanium, and zinc. It provides information on the identification and sorting of scrap metals and discusses...
Abstract
This article focuses on the recycling of metals including iron and steel, stainless steel, superalloys, nickel, aluminum, copper, precious metals, lead, magnesium, tin, titanium, and zinc. It provides information on the identification and sorting of scrap metals and discusses the equipment and procedures used for small-scale and large-scale scrapping operations.
Book Chapter
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001088
EISBN: 978-1-62708-162-7
..., and palladium and their corresponding alloys. chemical composition chemical properties electrical properties fabrication characteristics mechanical properties optical properties physical properties precious metals thermal properties Silver and Silver Alloys Commercially Pure Silver...
Abstract
This article discusses the chemical composition, fabrication characteristics, applications, mechanical properties, mass characteristics, thermal properties, electrical properties, optical properties, and chemical properties of precious metals, namely, silver, gold, platinum, and palladium and their corresponding alloys.
Book: Corrosion: Materials
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003834
EISBN: 978-1-62708-183-2
... with selectively clad (inlay) precious metals for low electrical contact resistance and high reliability. Clad metals can provide properties not available in a monolithic material at any cost. The best example is thermostat bimetals. An alloy with a high coefficient of thermal expansion is clad to an alloy...
Abstract
This article describes the principal cladding processes and methods for calculating properties of clad metals. It reviews the designing processes of clad metals to achieve specific requirements. The article discusses six categories of clad metal systems designed for corrosion control: noble metal clad systems, corrosion barrier systems, sacrificial metal systems, transition metal systems, complex multilayer systems, and clad diffusion alloys.
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001448
EISBN: 978-1-62708-173-3
... Abstract Ultrasonic welding (USW) is effectively used to join both similar and dissimilar metals with lap-joint welds. This article describes procedure considerations for the ultrasonic welding of specific material types. It reviews difficult-to-weld alloys, such as carbon and low-alloy steels...
Abstract
Ultrasonic welding (USW) is effectively used to join both similar and dissimilar metals with lap-joint welds. This article describes procedure considerations for the ultrasonic welding of specific material types. It reviews difficult-to-weld alloys, such as carbon and low-alloy steels, high-strength steels, and stainless steel, and provides information on the applications of weldable alloys such as aluminum alloys and copper alloys. The article concludes with a discussion on welding of dissimilar metal (nonferrous-to-nonferrous) combinations and its applications.
Book Chapter
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004109
EISBN: 978-1-62708-184-9
.... Early precious metal anodes were alloys that, after a short period of use, became enriched on the surface with the precious metal component. Anodes of this type are still used in harsh environments, such as Cook Inlet, Alaska, and the North Sea, where anode sleds weighing several tons are necessary...
Abstract
Cathodic protection (CP) is an electrochemical means of corrosion control widely used in the marine environment. This article discusses two types of CP systems: impressed current systems and sacrificial anode (passive) systems. It describes the anode materials used in these systems and the CP criteria. The article examines the design considerations and procedures involved in the CP of marine pipelines, offshore structures, and ship hulls. An illustration of sacrificial anode calculation is also provided.
Book: Thermal Spray Technology
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005745
EISBN: 978-1-62708-171-9
... of the areas associated with production and transfer of molten glass. Precious Metals Precious metals such as platinum and certain of their alloys are used extensively for long-term contact with molten glass. The industry is possibly the single largest consumer of platinum and is accustomed to measuring...
Abstract
This article reviews the use of thermal spray polymer coatings as a replacement for paints. It discusses the applications of the thermal spray forming process. The article also provides information on the applications of thermal spray in metal processing, textile and plastics, and ceramic and glass manufacturing industries.
1