Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003683
EISBN: 978-1-62708-182-5
... Abstract Porcelain enamels are glass coatings applied primarily to products or parts made of sheet steel, cast iron, or aluminum to improve appearance and to protect the metal surface. This article provides information on the types and properties of the porcelain enamels and frits for porcelain...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001279
EISBN: 978-1-62708-170-2
... Abstract Porcelain enamels are glass coatings applied primarily to products or parts made of sheet steel, cast iron, and aluminum to improve appearance and to protect the metal surface. This article describes the types of porcelain enamels, and details enamel frits for these materials...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006528
EISBN: 978-1-62708-207-5
... Abstract Porcelain enamel is a fusion bonded glass coating that resists chemical and abrasive attack, provides thermal and electrical insulation, and improves aesthetic qualities. It is used on cast iron as well as steel and aluminum alloys. This article provides a review of the porcelain...
Image
Published: 01 January 2003
Fig. 1 Corrosion of a porcelain enamel in boiling water and boiling mineral acids. Source: Ref 2 More
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003217
EISBN: 978-1-62708-199-3
... and their application. It also provides information on weld-overlay and thermal spray coating, porcelain enameling, and the preparation of enamel frits for steels. The article closes by describing methods and materials for ceramic coating. ceramic coatings chemical conversion coatings continuous...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006027
EISBN: 978-1-62708-172-6
... and porcelain enamels; electroplating; thermal spray coatings; and rubber linings. cementitious linings chromate conversion coating chromate-free conversion coating electroplating glasses hot dip galvanizing phosphate conversion coating porcelain enamels rubber linings thermal spray coating...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003094
EISBN: 978-1-62708-199-3
... applications that require the mechanical properties normally obtained by heat treatment. Steel sheet is coated in coil form before fabrication either by the steel mills or by specialists called coil coaters. Porcelain enamels are glass coatings applied primarily to products or parts made of sheet steel, cast...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006335
EISBN: 978-1-62708-179-5
... coating, cladding, porcelain enameling, and thermal spray. Organic coatings have a wide variety of properties, but their primary use is for corrosion resistance combined with a pleasing colored appearance. The article discusses the various types of organic coatings applied to cast irons. Practically any...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001303
EISBN: 978-1-62708-170-2
... life when resistance to corrosion, wear, and erosion is required. The common methods include electroplating, electroless plating, hardfacing, weld cladding, surface hardening, porcelain enameling, and organic coatings. cast iron conversion coatings corrosion resistance ductile iron...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001308
EISBN: 978-1-62708-170-2
..., electroless plating, porcelain enameling, and shot peening. abrasive blast cleaning acid etching alkaline etching aluminum aluminum alloys anodizing barrel finishing buffing chemical brightening chemical cleaning chemical conversion coating chemical etching cleaning coating electroless...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001304
EISBN: 978-1-62708-170-2
..., hot-dip coating processes, electrogalvanizing, electroplating, metal cladding, organic coatings, zinc-rich coatings, porcelain enameling, thermal spraying, hardfacing, vapor-deposited coatings, surface modification, and surface hardening via heat treatment. alloy steel cadmium plating carbon...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003049
EISBN: 978-1-62708-200-6
... Abstract This article provides an overview of the types, properties, and applications of traditional and advanced ceramics and glasses. Principal product areas for traditional ceramics include whitewares, glazes, porcelain enamels, structural clay products, cements, and refractories. Advanced...
Image
Published: 01 January 1994
Fig. 14 Enamel/metal expansion and stress patterns. Linear expansion and stress in a composite of acid-resistant cover-coat porcelain enamel and low-carbon steel More
Image
Published: 01 January 1997
Fig. 1 Estimated worldwide sales of ceramics. Does not include sales of glass products, which is estimated to be approximately $58 billion (1996). (a) Sales of traditional/industrial ceramics (1996). (b) Distribution of whiteware sales (1992). (c) Distribution of porcelain enamel sales (1992 More
Image
Published: 01 January 1994
Fig. 7 Process for preparing heat-treatable aluminum alloys for porcelain enameling No. Type Composition of solution Operating temperature Cycle time, min Constituent wt% °C °F 1 Alkaline cleaner (a) (b) (b) 60–82 140–180 2–5 2 Oxide removal Chromic acid More
Image
Published: 01 January 1994
Fig. 10 Process for preparing heat-treatable aluminum alloys for porcelain enameling No. Type Composition of solution Operating temperature Cycle time, min Constituent wt% °C °F 1 Alkaline cleaner (a) (b) (b) 60–82 140–180 2–5 2 Oxide removal Chromic acid More
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003051
EISBN: 978-1-62708-200-6
... and texture of the glaze, that are not available with competitive materials. Sanitaryware Sanitaryware, in its broadest sense, includes all products associated with residential and commercial bathrooms and facilities. Following this definition, such things as bathtubs (porcelain enameled and plastic...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0005585
EISBN: 978-1-62708-170-2
.... The clustering together of a few or many particles, whiskers, or fibers, or a combination thereof, into a larger solid mass. aging. (1) The storage of porcelain enamel slips or powders before use. (2) The change occurring in porcelain enamel slips or powders with the lapse of time. (3) In heat treatment...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.9781627081702
EISBN: 978-1-62708-170-2
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001316
EISBN: 978-1-62708-170-2
... a glaze. When the substrate is a metal, the coating is called a porcelain enamel. When the substrate is a glass, the coating is called a glass enamel. This article focuses on ceramic coatings for ceramic and glass substrates. Porcelain enameling is discussed in a separate article in the Section “Dip...