Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003571
EISBN: 978-1-62708-180-1
... failure of an antifriction bearing, a nylon driving gear, and a polyoxymethylene gear wheel. antifriction bearing cohesive wear elastomers glassy thermoplastics interfacial wear lubricant mechanical properties nylon nylon driving gear plastics polyoxymethylene gear wheel semicrystalline...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003572
EISBN: 978-1-62708-180-1
... 1 , 2 , 3 , 4 , 5 , 6 , 7 , 8 , 9 , 10 , 11 ). Table 1 Tribo-potential of polymers and composites for variety of applications Composite material Tribological applications Maximum tribological regime Neat and short fiber reinforced composites (SFRP) Seals, gears...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003005
EISBN: 978-1-62708-200-6
... structure is desired. Typical applications for CG iron include bed plates for large diesel engines, crank cases, gearbox and turbocharger housings, connecting forks, bearing brackets, pulleys for truck servo drives, sprocket wheels, and eccentric gears. Because the thermal conductivity of CG iron...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.9781627082006
EISBN: 978-1-62708-200-6