..., and thermal processes. Thermoplastic-matrix composites are recycled by regrinding, compounding/blending and reprocessing. The article concludes with discussion on the properties of recycled composite fibers. blending industrial waste disposal polymer-matrix composites recycling regrinding...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003424
EISBN: 978-1-62708-195-5
... plated, brazed diamond, diamond coated carbide, and polycrystalline cutting tools. The article also describes cutting tool materials that are used for peripheral milling, face milling, and the trimming of polymer-matrix composites. machining carbon fiber-reinforced epoxy epoxy thermoset composite...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003401
EISBN: 978-1-62708-195-5
..., preimpregnated reinforcement is used, together with high-performance polymer foam and honeycomb cores, and the composite matrix is crosslinked under vacuum and at elevated temperature, sometimes even in an autoclave. In this case, the main driver is performance enhancements. In aerospace applications, hand...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003426
EISBN: 978-1-62708-195-5
... Abstract Good hole-drilling processes are key to joining composite parts with other composite parts or with metal parts. This article discusses the considerations for drilling polymer-matrix composites. It describes the use of power-feed drill motors and automated drilling/fastener installation...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003447
EISBN: 978-1-62708-195-5
... Abstract This article discusses the materials and properties of polymer-matrix composites to characterize each generic material according to its composition and method of manufacture. It contains a table that lists the key physical, mechanical, thermal, and electrical properties, and in-service...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003489
EISBN: 978-1-62708-195-5
... bonding cleaning composite repair core splicing epoxy adhesive hot forming mechanical forming polymer-matrix composites trimming ADHESIVE BONDING frequently is used to assemble composite components into larger structures. In addition, finished components that are damaged during assembly...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003031
EISBN: 978-1-62708-200-6
...-reinforced composites matrix resins organic matrices polymer-matrix composites reinforcements A COMPOSITE MATERIAL can be defined as a macroscopic combination of two or more distinct materials, having a recognizable interface between them. However, because composites are usually used...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003043
EISBN: 978-1-62708-200-6
... Abstract The structural efficiency of a composite structure is established by its joints and assembly. Adhesive bonding, mechanical fastening, and fusion bonding are three types of joining methods for polymer-matrix composites. This article provides information on surface treatment...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003045
EISBN: 978-1-62708-200-6
... and terminate at the back-surface reflection. These periodic reflections are produced by the matrix pockets formed in the interstitial spaces of the weave and oscillate with a period proportional to the weave spacing. Matrix-rich regions between the plies of a composite material produce interlaminar echoes...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003046
EISBN: 978-1-62708-200-6
... for Advanced Composite Structures, Adhesives and Sealants, Volume 3, Engineered Materials Handbook, ASM International, 1990, p 821–828 M.M. Schwartz, Joining of Composite Matrix Materials, ASM International, 1994, p 69–77 References References 1. “Guidance Materials for the Design...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003042
EISBN: 978-1-62708-200-6
... Abstract This article describes the use of conventional machining techniques, laser cutting and water-jet cutting for producing finished composite parts. It explains two representative polymer-matrix composites--graphite and aramid composites--and discusses the machining and drilling problems...
Image
Published: 01 January 1997
Fig. 13 General classification of processes for polymer-matrix composites More
Image
Published: 01 January 2001
Fig. 1 Damage to fiber reinforced polymer-matrix composites resulting from different impact severity. (a) Low-energy impact. (b) Medium-energy impact. (c) High-energy impact More
Image
Published: 01 January 2001
Fig. 4 Relation of polymer-matrix composites to the overall use of hydrocarbons More
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006478
EISBN: 978-1-62708-190-0
... Abstract This article introduces the principal methodologies and some advanced technologies that are being applied for nondestructive evaluation (NDE) of fiber-reinforced polymer-matrix composites. These include acoustic emission, ultrasonic, eddy-current, computed tomography, electromagnetic...
Image
Published: 15 December 2019
Fig. 48 Microstructure of fiberglass-reinforced polymer-matrix composite I-beam viewed using Nomarski DIC. Nothing is visible in bright field. More
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003381
EISBN: 978-1-62708-195-5
..., processing, and diffusion on hygrothermal behavior of polymer-matrix composites and provides an outline on general considerations in assessing them. It discusses the hygrothermal testing and conditioning of polymer-matrix composites to assess fundamental hygrothermal behavior. The article provides...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003490
EISBN: 978-1-62708-195-5
... Abstract This article highlights the selected applications of advanced polymer-matrix composites, metal-matrix composites, and ceramic matrix composites. advanced polymer-matrix composites metal-matrix composites ceramic matrix composites APPLICATIONS of advanced composite...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003423
EISBN: 978-1-62708-195-5
... Abstract This article provides a summary of the concepts discussed in the articles under the Section “Post-Processing and Assembly” ASM Handbook, Volume 21: Composites. polymer-matrix composites ceramic-matrix composites metal-matrix composites post processing ONE OF THE PRIMARY...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003480
EISBN: 978-1-62708-195-5
... Abstract This article presents an overview of advanced composites, namely, polymer matrix composites, metal-matrix composites, ceramic-matrix composites, and carbon-matrix composites. It also provides information on the properties and applications of the composites in thermal management...