1-20 of 129 Search Results for

polyethylene coated pipe

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006038
EISBN: 978-1-62708-172-6
... consisting of (1) fusion-bonded epoxy primer, (2) copolymer adhesive, and (3) high-density polyethylene outer wrap Fig. 34 Pipe coating configuration showing (1) butyl rubber primer and (2) extruded polyethylene outer layer Fig. 29 Application of a polyethylene pipe coating by cross-head...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004213
EISBN: 978-1-62708-184-9
.... and O'Beirne J. , Major Field Study Compares Pipeline SCC with Coatings , Oil Gas J ., Vol 90 ( No. 24 ), 1992 , p 39 19. Beavers J.A. , “Assessment of the Effects of Surface Preparation and Coating on the Susceptibility of Line Pipe to Stress Corrosion Cracking,” Pipeline Research...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006007
EISBN: 978-1-62708-172-6
... 39. Haimbl J. and Geiser J. , “Polyethylene Coatings in Europe: A Look Back on 30 Years of Experience,” Prevention of Pipeline Corrosion Conference, Pipe Line and Gas Industry and Pipes and Pipelines International ( Houston, TX ), Oct 31–Nov 2 , 1995 40. Vogt H.E.P...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006335
EISBN: 978-1-62708-179-5
... E E No Yes Yes Yes Yes Yes Scratch-resistant finish Polyethylene G E E E E E G F E F No No No Yes No Yes Coatings Styrene-butadiene E G E E E E G G E G No Yes Yes No Yes Yes General purpose Urethane G E G G E E E E G G Yes Yes Yes...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006027
EISBN: 978-1-62708-172-6
... on borosilicate glasses and other ceramics, ground to a powder for easier melting, can be applied. Polymer coatings, including polyethylene, polypropylene, nylon, polyethylene-tetrafluoroethylene copolymers, as well as thermoplastic acrylics and thermoset epoxies, can be thermally spray applied...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006040
EISBN: 978-1-62708-172-6
... track record of recommending the use of polyethylene encasement (wrapping the exterior of buried ductile iron pipe in polyethylene plastic) for soil–side corrosion protection. There are instances where soil aggressiveness is sufficiently high that the use of both external coatings and cathodic...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003015
EISBN: 978-1-62708-200-6
... or sheet extrusion, chill-roll film extrusion, pipe or tube extrusion, wire and cable coverings, extrusion coating, and profile extrusion, and provides some discussion on multiple-screw extruders. The article describes the dimensional accuracy of extrusion products, and lists common defects that occur...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003541
EISBN: 978-1-62708-180-1
... micrograph showing a yielded zone surrounding and preceding a fatigue crack in 0.25 mm (0.01 in.) thick polycarbonate sheet. 20× Fig. 11 Time-to-failure of high-density polyethylene pipes at different stresses and temperatures. Source: Ref 12 Fig. 8 Section from a polystyrene sample...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006059
EISBN: 978-1-62708-172-6
... or using protective coatings in municipal wastewater systems. References References 1. “Polyethylene Encasement for Ductile-Iron Pipe Systems,” AWWA C105, Appendix A, American Water Works Association , Dec 1 , 2005 2. Vesilind A. , Ed., Wastewater Treatment Plant Design...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003847
EISBN: 978-1-62708-183-2
... and storage of lower concentrations, <25% 60 Shore A hardness natural rubber Chlorobutyl blends  Storage of acid with trace amounts of organics Three-ply linings Semihard linings Chlorinated polyethylene-faced soft natural rubber  Spent hydrochloric acid Blended chlorobutyl Phosphoric...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003008
EISBN: 978-1-62708-200-6
...-styrenes, acrylics, high-density polyethylenes, reinforced polypropylenes, high-impact polystyrenes, polyvinyl chloride, styrene-acrylonitriles, and styrene-maleic anhydrides. engineering thermoplastics family characteristics industrial applications mechanical properties physical properties...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005745
EISBN: 978-1-62708-171-9
... processes Table 1 Selection of polymers applied as coatings via thermal spray processes Polymer Maximum temperature resistance °C °F Ethylene methacrylic acid copolymer (EMAA) 40–60 105–140 Polyethylene (PE) 40–80 105–175 Polypropylene (PP) 70 160 Nylon 6,6 (PA) 65 150...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004117
EISBN: 978-1-62708-184-9
... Protection of Polyethylene-Encased Ductile Iron Pipe,” Mater. Perform. , Vol 32 ( No. 8 ), 1993 , p 23 – 27 3. Eden D.A. and Etheridge A. , “Corrosion Monitoring as a Means of Effecting Control of CO 2 Corrosion,” Paper 01057, presented at Corrosion 2001 ( Houston, TX ), NACE...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004139
EISBN: 978-1-62708-184-9
... problems. A similar polyethylene tubing, although not cross linked, is also available commercially. Although not as strong as PEX, its strength is more than adequate for marine freshwater piping applications, and it is more flexible. Both materials are excellent piping materials for marine use in both hot...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002464
EISBN: 978-1-62708-194-8
... Low-density polyethylene (LDPE) 10–12 −120 110 High-density polyethylene (HDPE) 26–33 −120 135 Linear low-density polyethylene (LLDPE) 15–32 −120 125 Isotactic polypropylene (PP or i-PP) 31–37 −10 165 Cis-1,4-polyisoprene, natural rubber … −67 15–50 Trans...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003651
EISBN: 978-1-62708-182-5
.... Consideration of these factors during the planning stage helps the corrosion engineer to obtain the maximum amount of information with the minimum number of problems. References References 1. “ANSI Standard for Polyethylene Encasement for Ductile-Iron Pipe Systems,” C105/ A21.5-99, American Water...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004185
EISBN: 978-1-62708-184-9
... dehydrochlorination of CPVC. One CPVC pipe handling 28% NH 4 OH at ambient temperature failed after only 1 year in service ( Ref 43 ). If polyethylene is used to store concentrated aqueous ammonium solutions, there is a weight loss due to outward diffusion through the plastic. A solution of 27% NH 4 OH solution...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003021
EISBN: 978-1-62708-200-6
... 10.1002/pen.760292313 42. Atkinson J.R. and Ward I.M. , The Joining of Biaxially Oriented Polyethylene Pipes , Polym. Eng. Sci. , Vol 29 ( No. 23 ), 1989 , p 1638 – 1641 10.1002/pen.760292303 43. Williams R.G. , Development of a Novel Electrofusion System , Gas...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001469
EISBN: 978-1-62708-173-3
... J.R. and Ward I.M. , The Joining of Biaxially Oriented Polyethylene Pipes , Polym. Eng. Sci. , Vol 29 ( No. 23 ), 1989 , p 1638 – 1641 Electromagnetic Induction Welding 43. Chookazian SM. , Bonding Plastics by Induction Heating , SPE J. , Vol 26 , 1970 , p 49 – 53...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003827
EISBN: 978-1-62708-183-2
... are tabulated. The article discusses the in-process problems and procedures that are common but avoidable when processing beryllium and aluminum-beryllium composites. It also describes the types of coatings used on beryllium and aluminum-beryllium. These include chemical conversion coatings, anodized coatings...