1-20 of 236 Search Results for

platinum powder

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 30 September 2015
Fig. 1 Simple toggle press used by Wollaston for making platinum powder compacts More
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006017
EISBN: 978-1-62708-175-7
... Abstract Powder metallurgy (PM) has been called a lost art. Long before furnaces were developed that could approach the melting point of metal, PM principles were used. This article provides an overview of the major historical developments of various methods of platinum powder production...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001317
EISBN: 978-1-62708-170-2
..., impregnation, ion exchange, and precipitation. Catalyst carriers are usually high-surface-area inorganic materials with complex pore structures, into which catalytic materials such as palladium, platinum, cobalt, chromium oxide, and vanadium pentoxide are deposited using these procedures. The article also...
Book Chapter

Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001087
EISBN: 978-1-62708-162-7
... (0.010 to 0.025 in.) wall thickness and as single lengths about 150 mm (6 in.) long. Base metal tube is available with an outer cladding or an inner lining of platinum, gold, silver, or any of the commercial precious metal alloys. Precious Metal Powders Precious metal powders are produced...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003150
EISBN: 978-1-62708-199-3
... to produce shinier, smooth films; spherical particles more often result in dull-appearing surfaces. Platinum, palladium, 40Pt-20Pd-40Au, 10Pt-20Pd-70Au, 7.5Pt-22.5Pd-70Au, and 75Au-25Pd powders have been used for electronic purposes. Trials are usually necessary to determine the most suitable powder from...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006556
EISBN: 978-1-62708-290-7
... commercial sources for gas-atomized platinum alloy powders ( Ref 20 , 21 ). Recent developments in crucible-less atomization (electrode induction gas atomization, plasma wire, and plasma powder spheroidization) may have the potential to make AM-grade platinum alloy powder, but they have not been put...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005670
EISBN: 978-1-62708-198-6
... Abstract This article focuses on the use of noble and precious metals for biomedical applications. These include gold, platinum, palladium, ruthenium, rhodium, iridium, and osmium. The physical and mechanical properties of noble and precious metals are presented in tables. A brief discussion...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006018
EISBN: 978-1-62708-175-7
... Abstract Metal powders are used as fuels in solid propellants, fillers in various materials, such as polymers or other binder systems, and for material substitution. They are also used in food enrichment, environmental remediation market, and magnetic, electrical, and medical application areas...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003829
EISBN: 978-1-62708-183-2
... Abstract This article characterizes the corrosion resistance of precious metals, namely, ruthenium, rhodium, palladium, silver, osmium, iridium, platinum, and gold. It provides a discussion on the general fabricability; atomic, structural, physical, and mechanical properties; oxidation...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001097
EISBN: 978-1-62708-162-7
.... A transient open circuit occurs when some of the built-up powder falls into the contact area. Controlled experiments have shown that the type of contact metal influences the amount of polymer formed. The greatest amount of polymer is formed on the platinum metals; lesser amounts are formed on gold...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003157
EISBN: 978-1-62708-199-3
... contact applications. Fabrication Properties Contact materials should have the capability of being welded, brazed, or otherwise joined to backing materials. In addition, they should have sufficient malleability to enable them to be shaped, or they should be capable of being formed by powder...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001254
EISBN: 978-1-62708-170-2
... Abstract The electroplating of platinum-group metals (PGMs) from aqueous electrolytes for engineering applications is limited principally to palladium and, to a lesser extent, to platinum, rhodium, and thin layers of ruthenium. This article provides a discussion on the plating operations...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003776
EISBN: 978-1-62708-177-1
... micrographs, comparing and contrasting the microstructural features of gold, platinum, iridium, palladium, and ruthenium-base alloys. It examines pure gold, intermetallic gold compounds, gold and platinum jewelry alloys, platinum-containing shape memory alloys, and alloys consisting of platinum, aluminum...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005745
EISBN: 978-1-62708-171-9
... or applying extra material to the desired location. In addition, reports have shown that functionalized polyethylene polymers, such as ethylene methacrylic acid copolymer and ethylene acrylic acid, can be applied in high humidity as well as at temperatures below freezing. Polymer Powders and Process...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001098
EISBN: 978-1-62708-162-7
... be observed from Eq 3 that thermal emf is a bulk property. It is independent of the resistance, and hence of the diameter, of the wire. The thermoelectric property of an electrical conductor is usually expressed in millivolts against a common reference. Platinum 67, because of its purity and excellent...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001088
EISBN: 978-1-62708-162-7
... Abstract This article discusses the chemical composition, fabrication characteristics, applications, mechanical properties, mass characteristics, thermal properties, electrical properties, optical properties, and chemical properties of precious metals, namely, silver, gold, platinum...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001094
EISBN: 978-1-62708-162-7
... by fabricating parts using powder metallurgical techniques and heat treating with essentially the same treatment as that used for cast parts. Typical properties are given in Tables 3 and 4 and the demagnetization curve is shown in Fig. 8 . Platinum-cobalt magnets have been replaced by rare-earth materials...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001454
EISBN: 978-1-62708-173-3
... composition, the shape and dimension of the parts to be joined, and the intended application. Gold, silver, and the platinum group metals are well known for their resistance to oxidation at high temperatures. Not only does this characteristic make the precious metals desirable in industrial and medical...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006123
EISBN: 978-1-62708-175-7
... Abstract This article focuses on the selection, properties, and applications of powder metallurgy refractory metals and their alloys, including tungsten, molybdenum, tantalum, niobium, and rhenium. molybdenum niobium powder metallurgy refractory metals rhenium tantalum tungsten...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003158
EISBN: 978-1-62708-199-3
..., and great versatility of application. Thermocouples are grouped into two broad categories, namely, standard thermocouples, including five base-metal thermocouples and three noble-metal thermocouples that have been given letter designations, and nonstandard thermocouples, including iridium-rhodium, platinum...