1-20 of 334 Search Results for

plastic plasma treatment

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001319
EISBN: 978-1-62708-170-2
... Abstract This article provides an overview of plasma surface treatments for plastics. It covers the equipment and methods used in plasma processing, providing detailed explanations of the plasma discharge reactions and how they affect surface state and topography. It also provides information...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005130
EISBN: 978-1-62708-186-3
... and the sheet bends away from the plasma. Additionally, the total thickness of the sheet is heated thoroughly, a relatively great plastic strain is produced by the thermal cycle and after cooling, the convex shaped is maintained, as shown in Fig. 4b . Fig. 4 Schematic of temperature distribution...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003043
EISBN: 978-1-62708-200-6
... preparation for the adhesive bonding of plastics because it involves no solvents, chemical fumes, disposal problems, or heat that could harm the plastic surface. The plasma reacts to a depth of 0.01 to 0.1 μm ( Ref 8 ). The effect of plasma treatment is to reduce the contact angle (a function of surface...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005745
EISBN: 978-1-62708-171-9
...Abstract Abstract This article reviews the use of thermal spray polymer coatings as a replacement for paints. It discusses the applications of the thermal spray forming process. The article also provides information on the applications of thermal spray in metal processing, textile and plastics...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005958
EISBN: 978-1-62708-168-9
... and nitrocarburizing. atmosphere furnaces austenitizing fluidized-bed furnaces gas nitriding heat treatment plasma nitriding quenching salt bath furnaces salt bath nitrocarburizing tempering tool steel vacuum furnaces THE HEAT TREATMENT of tool steels covers an extremely wide variety of different...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002466
EISBN: 978-1-62708-194-8
...Abstract Abstract Surface treatments are used in a variety of ways to improve the material properties of a component. This article provides information on surface treatments that improve service performance so that the design engineer may consider surface-engineered components as an alternative...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005672
EISBN: 978-1-62708-198-6
... blasting, and shot blasting. A laser technique has also been tried ( Ref 4 ). Chemical methods include degreasing, etching, anodizing, using adhesion promoters (accelerators and primers), and flame, corona, and plasma treatments. Additional information on surface treatments for various plastics and metals...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005707
EISBN: 978-1-62708-171-9
... into the plasma and deposited onto the substrate. This continuing bombardment increases nucleation and improves adhesion. Gas scattering is the major factor in ensuring uniform coating distribution. Applications of ion plating include optical coatings on glass and plastic, coating of electrical contacts...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006419
EISBN: 978-1-62708-192-4
.... However, due to the high achievable particle temperature, the process is especially well-suited for ceramic coatings. In combination with a far-off powder delivery and less plasma energy, even plastics can be processed. Typical applications include: The variety of useable materials makes...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003976
EISBN: 978-1-62708-185-6
... for forging dies. 1, abrasive wear; 2, thermal fatigue; 3, mechanical fatigue; 4, plastic deformation. Source: Ref 2 Fig. 26 Thickness of various coatings and surface treatments. PVD, physical vapor deposition; CVD, chemical vapor deposition. Source: Ref 49 Abstract Abstract...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001441
EISBN: 978-1-62708-173-3
... the welding operation. Taping a plastic bag over the part to be welded and sealing the bag at the point where the welding cables enter the bag will simulate an enclosed chamber when helium is introduced into the bag system as a shielding gas. Preweld heat treatment is not required. Postweld stress relief...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005706
EISBN: 978-1-62708-171-9
...-fed flame spray, wire- or rod-fed flame spray, electric arc spray, plasma arc spray, vacuum plasma spray, high-velocity oxyfuel spray, detonation gun deposition, and cold spray, and their advantages. It provides details on the microstructural characteristics of thermal spray coatings. The article also...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005977
EISBN: 978-1-62708-168-9
... Stratospheric Electroplating Ni, Cu, Cr (e.g., hexavalent Cr salts) Heavy metals, water management Plasma nitriding Nil … Physical vapor deposition Nil … Vacuum treatments (coating, spraying, etc.) Nil … Acid pickling H 2 SO 4 , HNO 3 Water quality, acid rain Quench hardening Oil...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001440
EISBN: 978-1-62708-173-3
...-welding processes that are used for joining titanium and titanium alloys. The processes include gas-tungsten arc welding (GTAW), gas-metal arc welding (GMAW), plasma arc welding (PAW), electron-beam welding (EBW), laser-beam welding (LBW), friction welding (FRW), and resistance welding (RW). The article...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003690
EISBN: 978-1-62708-182-5
.... , Arc Plasma Technology in Materials Science , Springer- Verlag , 1972 , 206 pages 10.1007/978-3-7091-8293-2 2. Ballard W.E. , Metal Spraying and Flame Deposition of Ceramics and Plastics , 4th ed. , Griffin , London, U.K. , 1963 3. Pawlowski L. , The Science...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005728
EISBN: 978-1-62708-171-9
... information on how the materials themselves respond to the various test methods. The article focuses on the test methods themselves, including those test parameters that can be varied and the influence of each on the results obtained. coating characterization coating testing liquid precursor plasma...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001306
EISBN: 978-1-62708-170-2
... Trends in Surface Treatment of Tools Used for Plastics Processing , Thyssen Edelstahl Tech. Ber. , special issue, May 1990 , p 82 – 99 15. Sundquist H.A. , Sirvio E.H. , and Kurkinen M.T. , Wear of Metalworking Tools Ion Plated With Titanium Nitride , Met. Tech. , Vol 10...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005939
EISBN: 978-1-62708-168-9
.... , Metallurgical Study of Low-Temperature Plasma Carbon Diffusion Treatments for Stainless Steels , Surf. Coat. Technol. , Vol 60 , 1993 , p 416 – 423 10.1016/0257-8972(93)90124-7 7. Stevenson P. et al. , The Effect of Process Parameters on the Plasma Carbon Diffusion Treatment of Stainless...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006273
EISBN: 978-1-62708-169-6
... with Nitrogen Ion Implantation and Plasma Treatment , Nucl. Instrum. Methods Phys. Res. B , Vol 59–60 , 1991 , p 920 – 924 10.1016/0168-583X(91)95733-T 5. Chen H.-Y. , Stock H.-R. , and Mayr P. , Plasma-Assisted Nitriding of Aluminum , Surf. Coat. Technol. , Vol 64 , 1994 , p...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.9781627081702
EISBN: 978-1-62708-170-2