Skip Nav Destination
Close Modal
Search Results for
plastic mounts
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 191 Search Results for
plastic mounts
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003021
EISBN: 978-1-62708-200-6
... A press that clamps the sections together during the heating and subsequent cooling cycles A brass electrode or die that is mounted on an aluminum plate, which applies the electrical energy directly to the plastic ( Ref 48...
Abstract
This article discusses the classification of the attachment and joining methods in plastics, including mechanical fastening, adhesive bonding, solvent bonding, and welding. It describes the mechanical fastening techniques used to join both similar and dissimilar materials with machine screws or bolts, nuts and washers, molded-in threads, self-threading screws, rivets, spring-steel fasteners, press fits, and snap fits. The article explains solvent bonding used for thermoplastic parts, and tabulates the solvent types used with various plastics. It also describes the surface preparation of plastics, chemical treatment for adhesion, and tabulates the adhesive types for bonding plastics to plastics and plastics to nonplastics. The article briefly describes the welding processes of thermoplastics, including fusion welding (hot-tool, hot gas, extrusion, and focused infrared), friction welding (vibration, spin, and ultrasonic), and electromagnetic welding (resistance, induction, dielectric, and microwave). It concludes with the evaluation of welds using destructive and nondestructive testing.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003026
EISBN: 978-1-62708-200-6
... Abstract In terms of their electrical properties, plastics can be divided into thermosetting and thermoplastic materials, some of which are conductive or semiconductive. This article provides detailed information on factors that affect the property of plastics. It discusses the major test...
Abstract
In terms of their electrical properties, plastics can be divided into thermosetting and thermoplastic materials, some of which are conductive or semiconductive. This article provides detailed information on factors that affect the property of plastics. It discusses the major test methods used to determine the following dielectric properties of plastics: dielectric breakdown voltage, dielectric strength, dielectric constant, dissipation factor, arc tracking resistance, insulation resistance, volume, and surface resistivity or conductivity. The test specifications and conditions, recommended by several U.S. and foreign testing organizations for characterizing the electrical properties of plastic materials are listed. The article describes the influence of these properties on selection of plastics for insulation application. An outline of the electromagnetic shielding and testing methods of electromagnetic interference are also provided. Designations, electrical properties, and applications of elastomers are tabulated.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003028
EISBN: 978-1-62708-200-6
... the test specimen. When the light source is off, the water spray exposes the specimen to 100% humidity conditions, similar to what a plastic would experience outdoors at night. This weatherometer also uses a black panel temperature control. This control consists of a temperature sensor mounted on a...
Abstract
This article describes weathering and environmental factors that contribute to degradation in plastics, including temperature variations, moisture, sunlight, oxidation, microbiologic attack, and other environmental elements. It presents a general overview of aging factors, their effects on plastic materials, and the accelerated test methods that can be used to estimate the reaction of a plastic component during actual use. The article focuses on the determination of service temperature as it indicates the ability of a material to retain a certain property, when exposed to elevated temperatures for an extended period of time. It concludes by describing various degradation processes, namely, thermal degradation, thermal oxidative degradation, photooxidative degradation, environmental corrosion, and chemical corrosion and discussing the ways of detecting these degradation processes.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003007
EISBN: 978-1-62708-200-6
... Abstract Engineering plastics offer unique product benefits based on physical properties, or combinations of physical properties, that allow vastly improved product performance. Providing an overview of the general characteristics and the mechanical and environmental stress response of...
Abstract
Engineering plastics offer unique product benefits based on physical properties, or combinations of physical properties, that allow vastly improved product performance. Providing an overview of the general characteristics and the mechanical and environmental stress response of engineering plastics, this article discusses various factors, including thermal, mechanical and electrical properties, environmental factors, and material cost that are important in the selection of engineering plastics for specific applications.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003244
EISBN: 978-1-62708-199-3
... and control desired. Only the portion of the specimen to be polished should be in contact with the electrolyte. Small specimens may be mounted by conventional molded-plastic-mounting procedures, for ease in handling for mechanical preparation and subsequent electropolishing. Electrical...
Abstract
This article describes the methods and equipments involved in the preparation of specimens for examination by light optical microscopy, scanning electron microscopy, electron microprobe analysis for microindentation hardness testing, and for quantification of microstructural parameters, either manually or by the use of image analyzers. Preparation of metallographic specimens generally requires five major operations: sectioning, mounting, grinding, chemical polishing, and etching. The article provides information on the principles of technique selection in mechanical polishing, and describes the procedures, advantages, and disadvantages of electrolytic and chemical polishing. It also provides a detailed account of procedures, precautions, and composition for preparation and handling of etchants.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003245
EISBN: 978-1-62708-199-3
..., temperature, and pressure of mounting are similar to those for phenolics, but they produce a superior mount with better edge retention. Phenolics are badly degraded by hot etchants, while thermosetting epoxy holds up well. Plastics that cure at room temperature, such as acrylics, polyesters, and epoxy...
Abstract
Proper sectioning of the surface to be examined is a very important step in preparing steel specimens. The first step in preventing damage to the metallurgical structure is to minimize the amount of sectioning that is done. This article discusses the various metallographic techniques, namely mounting, grinding, polishing, and etching involved in the microstructural analysis of carbon and alloy steels, case hardening steels, cast iron, ferrous powder metallurgy alloys, wrought and cast stainless steels, tool materials, steel castings, iron-chromium-nickel heat-resistant casting alloys and different product forms of steels.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003247
EISBN: 978-1-62708-199-3
...-Mg alloys: 5 xxx series and casting alloys 4, 2, or 1 Al-Mg-Si alloys: 6 xxx series and casting alloys 4, 2, or 1 Al-Cu-Mg-Zn alloys: 7 xxx series and casting alloys 1 (a) Also, welds and brazed joints made with the use of these alloys as filler metals Mounting in a plastic...
Abstract
This article describes the metallographic technique for nonferrous metals and special-purpose alloys. These include aluminum alloys, copper and copper alloys, lead and lead alloys, magnesium alloys, nickel and nickel alloys, magnetic alloys, tin and tin alloys, titanium and titanium alloys, refractory metals and alloys, zinc and zinc alloys, and wrought heat-resisting alloys. The preparation of specimens for metallographic technique includes operations such as sectioning, mounting, grinding, polishing, and etching of nonferrous metals and alloys. The article contains tables that list the etchants for macroscopic examination and microscopic examination of nonferrous metals and special-purpose alloys.
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006765
EISBN: 978-1-62708-295-2
... performed with the scanning electron microscope (SEM) over the same magnification range as the LM, but examination with the latter is more efficient. This article describes the major operations in the preparation of metallographic specimens, namely sectioning, mounting, grinding, polishing, and etching. The...
Abstract
Metallographic examination is one of the most important procedures used by metallurgists in failure analysis. Typically, the light microscope (LM) is used to assess the nature of the material microstructure and its influence on the failure mechanism. Microstructural examination can be performed with the scanning electron microscope (SEM) over the same magnification range as the LM, but examination with the latter is more efficient. This article describes the major operations in the preparation of metallographic specimens, namely sectioning, mounting, grinding, polishing, and etching. The influence of microstructures on the failure of a material is discussed and examples of such work are given to illustrate the value of light microscopy. In addition, information on heat-treatment-related failures, fabrication-/machining-related failures, and service failures is provided, with examples created using light microscopy.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003025
EISBN: 978-1-62708-200-6
... Abstract Mechanical properties are often the most important properties in the design and selection of engineering plastics. Temperature, molecular structure, crystallinity, viscoelasticity, and effects of environment, fillers and reinforcements are considered as the basic factors affecting the...
Abstract
Mechanical properties are often the most important properties in the design and selection of engineering plastics. Temperature, molecular structure, crystallinity, viscoelasticity, and effects of environment, fillers and reinforcements are considered as the basic factors affecting the mechanical properties of engineering plastics. The testing methods for determining mechanical properties, including stress-strain test, modulus-directed tensile test, strength test, strength-directed tensile test, impact test, and dynamic mechanical test are discussed.
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006660
EISBN: 978-1-62708-213-6
... Abstract The electron backscatter diffraction (EBSD) technique has proven to be very useful in the measurement of crystallographic textures, orientation relationships between phases, and both plastic and elastic strains. This article focuses on backscatter diffraction in a scanning electron...
Abstract
The electron backscatter diffraction (EBSD) technique has proven to be very useful in the measurement of crystallographic textures, orientation relationships between phases, and both plastic and elastic strains. This article focuses on backscatter diffraction in a scanning electron microscope and describes transmission Kikuchi diffraction. It begins with a discussion on the origins of EBSD and the collection of EBSD patterns. This is followed by sections providing information on EBSD spatial resolution and system operation of EBSD. Various factors pertinent to perform an EBSD experiment are then covered. The article further describes the processes involved in sample preparation that are critical to the success or usefulness of an EBSD experiment. It also discusses the applications of EBSD to bulk samples and the development of EBSD indexing methods.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001264
EISBN: 978-1-62708-170-2
... electroless nickel coatings on composites and plastics. aluminum alloys composites copper alloys electroless nickel baths electroless nickel plating electroless nickel plating equipment electroless nickel-boron coatings electroless nickel-phosphorus coatings fatigue strength ferrous alloys...
Abstract
Electroless nickel plating is used to deposit nickel without the use of an electric current. This article provides an overview of the solution composition and characteristics of the electroless nickel bath. It focuses on the metallurgical, mechanical and physical properties of electroless nickel-phosphorus coatings and electroless nickel-boron coatings. The effect of electroless nickel coatings on the fatigue strength of steel is also described. The article includes information on the recommended pretreatment procedures for different ferrous alloys, aluminum alloys, and copper alloys. It presents a detailed account of the equipment and various processes—including bulk and barrel plating—involved in electroless nickel plating, and discusses hydrogen relief methods. The article includes a comprehensive table on nickel plating applications, and concludes with information on electroless nickel coatings on composites and plastics.
Book Chapter
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006673
EISBN: 978-1-62708-213-6
... various criteria to be considered for specimen preparation and calibration of TGAs. The use of thermogravimetric analysis data in the assessment of failure analysis of plastics and the combined usage of TGA with other techniques to understand the changes in the sample are also covered. The article...
Abstract
Thermogravimetric analysis (TGA) is a thermal analysis technique that measures the amount and rate of change in the weight of a material as a function of temperature or time in a controlled atmosphere. This article provides a detailed account of the concepts of TGA, covering the various criteria to be considered for specimen preparation and calibration of TGAs. The use of thermogravimetric analysis data in the assessment of failure analysis of plastics and the combined usage of TGA with other techniques to understand the changes in the sample are also covered. The article provides examples of applications and provides information on the interpretation of TGA.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003187
EISBN: 978-1-62708-199-3
... Abstract Fundamental to the machining process, is the metal-cutting operation, which involves extensive plastic deformation of the work piece ahead of the tool tip, high temperatures, and severe frictional conditions at the interfaces of the tool, chip, and work piece. This article explains...
Abstract
Fundamental to the machining process, is the metal-cutting operation, which involves extensive plastic deformation of the work piece ahead of the tool tip, high temperatures, and severe frictional conditions at the interfaces of the tool, chip, and work piece. This article explains that the basic mechanism of chip formation is shear deformation, which is controlled by work material properties such as yield strength, shear strength, friction behavior, hardness, and ductility. It describes various chip types, as well as the cutting parameters that influence chip formation. It also demonstrates how the service life of cutting tools is determined by a number of wear processes, including tool wear, machining parameters, and tool force and power requirements. It concludes by presenting a comprehensive collection of formulas for turning, milling, drilling, and broaching, and its average unit power requirement.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001265
EISBN: 978-1-62708-170-2
... electroless copper in various applications. This article provides information on the bath chemistry and deposit properties of electroless copper and discusses the applications of electroless copper plating, such as printed wiring boards, decorative plating-on-plastic, electromagnetic interference shielding...
Abstract
Electroless, or autocatalytic, metal plating is a nonelectrolytic method of deposition from solution that can be plated uniformly over all surfaces, regardless of size and shape. The plating's ability to plate onto nonconductors is an advantage that contributes to the choice of electroless copper in various applications. This article provides information on the bath chemistry and deposit properties of electroless copper and discusses the applications of electroless copper plating, such as printed wiring boards, decorative plating-on-plastic, electromagnetic interference shielding, and hybrid and other advanced applications. It describes two commercial processes, pretreatment and post-treatment. The article reviews the solutions used, controls and control equipment, and performance criteria of electroless copper plating. It concludes with information on the environmental and safety issues associated with electroless copper plating.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003014
EISBN: 978-1-62708-200-6
... Abstract Injection molding is a process of forcing or injecting a fluid plastic material into a closed mold. The process generally has the advantages of being more readily automated and of permitting finer part details. Injection-molding compounds are thermoplastic or thermosetting materials...
Abstract
Injection molding is a process of forcing or injecting a fluid plastic material into a closed mold. The process generally has the advantages of being more readily automated and of permitting finer part details. Injection-molding compounds are thermoplastic or thermosetting materials and their composites that are specifically formulated for the injection-molding process. This article discusses the injection molding process, which includes the two basic categories of thermoplastic and thermoset injection molding, and lists the common thermoplastic and thermoset molding compounds and applications. It also describes the operation of the different types of injection molding machines as well as mold design and process controls. The article also describes the selection of injection-moldable thermosets, and provides an overview of part performance, properties, blowing agents, and aesthetic concerns related to thermoplastic structural-foam injection molding.
Book Chapter
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005677
EISBN: 978-1-62708-198-6
... sealants, dental cements, porcelain and plastic denture teeth, dental feldspathic porcelain and ceramics, endodontic instruments, periodontal Instruments, and orthodontic wires. The article describes the correlations of properties, such as hardness, fracture toughness, and wear. It discusses wear mechanism...
Abstract
This article reviews the friction and wear of various dental materials that have been studied by fundamental wear measurements, simulated service wear measurements, and clinical measurements. The materials include dental amalgam, composite restorative materials, pit and fissure sealants, dental cements, porcelain and plastic denture teeth, dental feldspathic porcelain and ceramics, endodontic instruments, periodontal Instruments, and orthodontic wires. The article describes the correlations of properties, such as hardness, fracture toughness, and wear. It discusses wear mechanism such as sliding adhesive wear, two-body abrasion, three-body abrasion, erosion, and fatigue.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003009
EISBN: 978-1-62708-200-6
... Abstract Advanced thermoplastics are stiff, moldable plastics that compete with traditional engineering thermoplastics and thermosets owing to their good tensile, compressive, impact, and shear strength, electrical properties, and corrosion resistance. This article discusses commercial forms...
Abstract
Advanced thermoplastics are stiff, moldable plastics that compete with traditional engineering thermoplastics and thermosets owing to their good tensile, compressive, impact, and shear strength, electrical properties, and corrosion resistance. This article discusses commercial forms, family characteristics, properties and applications of the following advanced thermoplastics: homopolymer and copolymer acetals, fluoropolymers, ionomers, polyamides, polyamide-imides, polyarylates, polyketones, polyaryl sulfones, polybutylene terephthalates, polycarbonates, polyether-imides, polyether sulfones, polyethylene terephthalates, thermoplastic polyimides, liquid crystal polymers, polyphenylene ether blends, polyphenylene sulfides, and polysulfones.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003053
EISBN: 978-1-62708-200-6
... possible to their final shape. The article also provides useful information on drying methods, shrinkage, and defects as well as the removal of organic processing aids such as dispersants, binders, plasticizers, and lubricants. ceramic forming process drying green machining organics removal...
Abstract
Ceramic-forming processes usually start with a powder which is then compacted into a porous shape, achieving maximum particle packing density with a high degree of uniformity. This article compares and contrasts several forming processes, including mechanical consolidation, dry pressing, cold isostatic pressing, slip casting, tape casting, roll compaction, extrusion, and injection molding. It describes the advantages, equipment and tooling, and material requirements of green machining, the machining of ceramics in an unfired state with the intent of producing parts as close to as possible to their final shape. The article also provides useful information on drying methods, shrinkage, and defects as well as the removal of organic processing aids such as dispersants, binders, plasticizers, and lubricants.
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006767
EISBN: 978-1-62708-295-2
... elastic fracture mechanics analysis, with some mention of elastic-plastic fracture mechanics analysis. The article describes the probabilistic aspects of fatigue and fracture. Information on crack-growth simulation of the material is also provided. crack-growth simulation elastic-plastic fracture...
Abstract
This article describes concepts and tools that can be used by the failure analyst to understand and address deformation, cracking, or fracture after a stress-related failure has occurred. Issues related to the determination and use of stress are detailed. Stress is defined, and a procedure to deal with stress by determining maximum values through stress transformation is described. The article provides the stress analysis equations of typical component geometries and discusses some of the implications of the stress analysis relative to failure in components. It focuses on linear elastic fracture mechanics analysis, with some mention of elastic-plastic fracture mechanics analysis. The article describes the probabilistic aspects of fatigue and fracture. Information on crack-growth simulation of the material is also provided.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003005
EISBN: 978-1-62708-200-6
... materials, including ferrous alloys, nonferrous alloys, ceramics, cermets and cemented carbides, engineering plastics, polymer-matrix composites, metal-matrix composites, ceramic-matrix and carbon-carbon composites, and reviews their general property characteristics and applications. It describes the...
Abstract
The selection of engineered materials is an integrated process that requires an understanding of the interaction between materials properties, manufacturing characteristics, design considerations, and the total life cycle of the product. This article classifies various engineered materials, including ferrous alloys, nonferrous alloys, ceramics, cermets and cemented carbides, engineering plastics, polymer-matrix composites, metal-matrix composites, ceramic-matrix and carbon-carbon composites, and reviews their general property characteristics and applications. It describes the synergy between the elements of the materials selection process and presents a general comparison of material properties. Finally, the article provides a short note on computer aided materials selection systems, which help in proper archiving of materials selection decisions for future reference.