Skip Nav Destination
Close Modal
Search Results for
physical testing
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 1902
Search Results for physical testing
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Image
Published: 01 January 2005
Fig. 38 Physical modeling of the wedge-forging test. (a) Preform geometry. (b) Plan view, longitudinal section, and transverse section of forged plasticine wedge sample. Source: Ref 74
More
Image
in The Application of Thermodynamic and Material Property Modeling to Process Simulation of Industrial Alloys
> Metals Process Simulation
Published: 01 November 2010
Fig. 17 Comparison of the spiral test result, based on the physical properties calculated from JMatPro for alloy ADC12 of low and high specification. Courtesy of UES Software Asia, generated using ProCast
More
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003523
EISBN: 978-1-62708-180-1
... presented subsequently follows the basic approach of the scientific method as used in the physical sciences. This includes the definition of the problem, collection of data, analysis of data, development of a hypothesis, and testing and selection of the appropriate hypothesis. Often, investigations...
Abstract
This article focuses on the general methods and approaches from the perspective of a reconstruction analyst and includes discussions relevant to materials failure analysts at the incident scene. The elements of accident reconstruction are described. These have conceptual similarity with the principles for failure analysis of material incidents that are less complex than a large-scale accident. The article provides a brief review of some general concepts on the use of modeling which can be a very powerful tool for information pertaining to the reconstruction of an accident where the model can be a physical, mathematical, or logical representation of a physical system or process.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003441
EISBN: 978-1-62708-195-5
... Abstract This article describes the most significant tests to characterize the properties of constituent materials. It discusses the chemical, physical, and mechanical tests for determining the properties of reinforcement fibers and fabrics. The article provides information on some of the basic...
Abstract
This article describes the most significant tests to characterize the properties of constituent materials. It discusses the chemical, physical, and mechanical tests for determining the properties of reinforcement fibers and fabrics. The article provides information on some of the basic materials used for thermoset and thermoplastic resin matrices. It reviews the identification of the individual characteristics of thermoset and thermoplastic resin along with the test methods normally used for their determination. The article contains a table that lists properties and tests for uncured and cured thermoset-matrix resins and prepregs.
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006772
EISBN: 978-1-62708-295-2
... the information collected. Testing of the hypothesis may be done by cognitive reasoning, modeling techniques, or actual experimentation. The need for modeling or physical testing depends on the circumstances of each individual accident. The difficulty of recreating an accident is often underestimated...
Abstract
Failure analysis is generally defined as the investigation and analysis of parts or structures that have failed or appeared to have failed to perform their intended duty. Methods of field inspection and initial examination are also critical factors for both reconstruction analysts and materials failure analysts. This article focuses on the general methods and approaches from the perspective of a reconstruction analyst. It describes the elements of accident reconstruction, which have conceptual similarity with the principles for failure analysis of material incidents that are less complex than a large-scale accident. The approach presented is that the analysis and reconstruction is based on the physical evidence. The article provides a brief review of some general concepts on the use and limitations of advanced data acquisition tools and computer modeling. Legal implications of destructive testing are discussed in detail.
Book Chapter
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005540
EISBN: 978-1-62708-197-9
... Abstract Simulation programs are becoming more effective tools in reducing the need for physical testing and the avoidance of costly downstream problems by solving the problems upfront in the early development stage. This article provides a brief review of the history and applied analysis...
Abstract
Simulation programs are becoming more effective tools in reducing the need for physical testing and the avoidance of costly downstream problems by solving the problems upfront in the early development stage. This article provides a brief review of the history and applied analysis of simple forming operations. It focuses on metal stamping simulation based on the finite-element methods or model (FEM) with emphasis on software tools using the three-dimensional FEM technology. The article discusses two aspects of particular importance in finite-element analysis of sheet forming and springback analysis: the type of solution algorithm/governing equation and the type of element. The article provides information on various models for material yield criteria.
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003518
EISBN: 978-1-62708-180-1
... an investigation of documentation and a series of physical tests. This Volume focuses on the definition of and requirements for a professionally performed failure analysis of a physical object or structure. However, many of the concepts for investigation that are described in this Section have much greater...
Abstract
Failure analysis is a process that is performed to determine the causes or factors that have led to an undesired loss of functionality. This article describes some of the factors and conditions that might be considered when approaching a failure analysis problem. It focuses on the key principles, objectives, practices, and procedures of failure analysis. The article provides guidelines on the preparation of a protocol for a failure analysis. It also demonstrates the proper approaches to failure analysis.
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006754
EISBN: 978-1-62708-295-2
..., someone should determine if the correct material was used and if it was processed properly. This often requires both an investigation of documentation and a series of physical tests. This Volume focuses on the definition of and requirements for a professionally performed failure analysis of a physical...
Abstract
Failure analysis is a process that is performed in order to determine the causes or factors that have led to an undesired loss of functionality. This article is intended to demonstrate proper approaches to failure analysis work. The goal of the proper approach is to allow the most useful and relevant information to be obtained. The discussion covers the principles and approaches in failure analysis work, objectives and scopes of failure analysis, the planning stages for failure analysis, the preparation of a protocol for a failure analysis, practices used by failure analysts, and procedures of failure analysis.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003440
EISBN: 978-1-62708-195-5
.... Typical types of composite test matrices are shown in Table 1 . Typical types of composite test matrices Table 1 Typical types of composite test matrices Constituent physical properties Constituent mechanical properties Prepreg physical properties Lamina physical properties Lamina...
Abstract
A test plan specifies material properties to be evaluated, selects test methods, eliminates options offered by standard test methods by selecting specific specimen and test configurations, and defines success criteria. This article discusses various testing objectives that affect the execution of testing programs. The testing objectives include development of test matrices, testing standards, specimen preparation, environmental conditioning, instrumentation and data acquisition, failure modes, and data interpretation and recording.
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006762
EISBN: 978-1-62708-295-2
... preparation is required prior to writing a report, regardless of the format. The author must compile all information generated during the investigation and review the data. Many investigators find it helpful to assemble all pertinent data, such as photographs, spectra, and mechanical and physical test results...
Abstract
As a failure investigation progresses, the time arrives when the data and results of the various testing and analyses are compiled, compared, and interpreted. Data interpretation should be relatively straightforward for results that align well. However, interpretation can be challenging when results from various tests seem contradictory or inconclusive. Regardless, conclusions must eventually be drawn from the data. This article discusses the processes involved in reviewing data, formulating conclusions, failure analysis report preparation and writing, and providing recommendations and follow-up with appropriate personnel to prevent future failures.
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002445
EISBN: 978-1-62708-194-8
..., and physical. It also presents information on the simulation and testing carried out to evaluate the design behavior. computer-aided electrical/electronic design electrical phases functional phases hydraulic system mechanical system physical phases DESIGN AND ANALYSIS of electrical/electronic...
Abstract
Design and analysis of electrical/electronic systems and components tends to be different from the corresponding process for most mechanical and hydraulic systems. This article provides an overview of three overlapping phases followed in electrical design: functional, electrical, and physical. It also presents information on the simulation and testing carried out to evaluate the design behavior.
Book: Powder Metallurgy
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006086
EISBN: 978-1-62708-175-7
... used mechanical methods include water and gas atomization, milling, mechanical alloying, and electrolysis. Some chemical methods include reduction of oxides. This article provides information on the reliable techniques for powder characterization and testing to evaluate the chemical and physical...
Abstract
Various powder production processes allow precise control of the chemical composition and physical characteristics of powders and allow tailoring of specific attributes for targeted applications. Metal powders are produced by either mechanical methods or chemical methods. The commonly used mechanical methods include water and gas atomization, milling, mechanical alloying, and electrolysis. Some chemical methods include reduction of oxides. This article provides information on the reliable techniques for powder characterization and testing to evaluate the chemical and physical properties of metal powders, both as individual particles and in bulk forms.
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006374
EISBN: 978-1-62708-192-4
.... The article concludes with information on physical and chemical testing of brakes and toxicity of brake formulation and regulations. aircraft brake linings aircraft brakes automotive brakes brake pads cast iron casting chemical testing disk brakes drum brakes friction physical testing...
Abstract
This article focuses on friction and wear of automotive and aircraft brakes. It provides a comparison of friction and wear behaviors, frictional characteristics, and frictional performance of the friction materials. The article describes the components of brake friction materials and the classifications of brake lining materials. It discusses the effect of formulation compositions and manufacturing processes and the effect of braking operation conditions. The article provides information on aircraft brake linings, which operate under a wide range of kinetic energy conditions. The morphology effect of graphite on automotive brake drum and disk is explained. The article also describes the characteristics of specific wear rates for both normal and local cast iron in automotive brake drums and disk rotors. It provides information on noises, vibrations, and harshness caused by brake pads. The article concludes with information on physical and chemical testing of brakes and toxicity of brake formulation and regulations.
Book Chapter
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006738
EISBN: 978-1-62708-210-5
... Abstract This datasheet provides information on composition limits, processing effects on physical and mechanical properties, and fabrication characteristics of high-strength forging alloy 7076. alloy composition aluminum alloy 7076 fabrication characteristics high-strength forging...
Abstract
This datasheet provides information on composition limits, processing effects on physical and mechanical properties, and fabrication characteristics of high-strength forging alloy 7076.
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003286
EISBN: 978-1-62708-176-4
... Abstract This article provides the theoretical background for understanding many of the physical processes relevant to mechanical testing methods, experimental results, and analytical approaches described in this volume. creep testing stress-relaxation testing creep deformation Stress...
Abstract
This article provides the theoretical background for understanding many of the physical processes relevant to mechanical testing methods, experimental results, and analytical approaches described in this volume.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003439
EISBN: 978-1-62708-195-5
... allowables Related subjects are discussed in the next article in this Section, “Test Program Planning,” which is followed by additional articles on specific types of tests. Differences Between Testing of Composites and Testing of Isotropic Materials The physics of composites testing may appear...
Abstract
Composites are complex engineered materials that often behave differently than common isotropic materials. Before testing a composite material, or before ordering or supervising such testing, the responsible party should review certain considerations. This article provides an overview of such considerations, namely, the differences between the testing of composites and testing of isotropic materials, role of certification agencies and importance of their involvement, building-block approach to composites testing, determining the purpose of testing, normalizing results, and statistical data reduction.
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005686
EISBN: 978-1-62708-198-6
... that combines the review and evaluation of existing data from all sources with, when necessary, the selection and application of additional tests. The evaluation starts with an assessment of the physical and chemical characteristics of the materials, history of clinical use or human exposure data, and any...
Abstract
This article provides a background to the biological evaluation of medical devices. It discusses what the ISO 10993 standards require for polymeric biomaterials and presents examples of qualitative and quantitative tests that can be used to satisfy these requirements. The article describes infrared (IR) and thermal analyses that are used extensively to fingerprint polymeric materials. It also presents a discussion on the chemical characterization and risk assessment of extracts. Background information on risk assessments of extracts is also included. The four basic steps that are commonly used in the risk assessment process are discussed. These include hazard identification, dose-response assessment, and exposure assessment, and risk characterization.
Book Chapter
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006714
EISBN: 978-1-62708-210-5
... Abstract This datasheet provides information on key alloy metallurgy, and processing effects on physical and mechanical properties of the extrusion alloy 6042. It provides a comparison of characteristics of the alloy 6042 with related alloys and tempers. extrusion alloy 6042 mechanical...
Abstract
This datasheet provides information on key alloy metallurgy, and processing effects on physical and mechanical properties of the extrusion alloy 6042. It provides a comparison of characteristics of the alloy 6042 with related alloys and tempers.
Book Chapter
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006583
EISBN: 978-1-62708-210-5
... Abstract This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and applications of Al-Mg die-casting alloy 518.0. A figure presents die cast aluminum casting rotating-beam fatigue curve for 518.0-F alloy. aluminum alloy...
Abstract
This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and applications of Al-Mg die-casting alloy 518.0. A figure presents die cast aluminum casting rotating-beam fatigue curve for 518.0-F alloy.
Book: Powder Metallurgy
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006068
EISBN: 978-1-62708-175-7
... the two types of quality assurance testing measures for powder metallurgy stainless steels: tests for powder contamination and tests of chemical and physical properties. annealing chemical properties drying gas atomization lubricating physical properties powder characteristics powder...
Abstract
This article provides information on the process details that differ from general water atomization of metals as they relate to basic and engineering properties that are specific to stainless steel powders. The discussion focuses on the compacting-grade stainless steel powders. The process details include raw materials, melting method, and control of physical and chemical powder characteristics. The article describes the gas atomization of stainless steel powders and processes that are done after water atomization: drying, screening, annealing, and lubricating. It also discusses the two types of quality assurance testing measures for powder metallurgy stainless steels: tests for powder contamination and tests of chemical and physical properties.