Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006548
EISBN: 978-1-62708-290-7
... for commercialization of AM technologies, moving into the third segment of AM historical development, modern AM. This period of AM development is characterized by AM without the use of a computer. The oldest of the three main areas of AM development is photosculpture. Figure 1 shows the photosculpture studio...