1-20 of 70

Search Results for oxyacetylene brazing

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

By G. Fisher, T. Wolfe
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006391
EISBN: 978-1-62708-192-4
... materials, namely, iron-base overlays, chromium carbide-based overlays, nickel- and cobalt-base alloys, and tungsten carbide-based metal-matrix composite overlays. It discusses the types of hardfacing processes, such as arc welding processes, and laser cladded, oxyacetylene brazing and vacuum brazing...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003208
EISBN: 978-1-62708-199-3
... specimens, 6.40 ± 0.13 mm (0.252 ± 0.005 in.) in diameter. (b) Elongation in approximately 25 mm (1 in.) Oxyacetylene Braze Welding Oxyacetylene braze welding is a method of OFW capable of joining many base metals, but it is used primarily on steel and cast iron with a copper alloy filler...
Book Chapter

By William Ballis
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001372
EISBN: 978-1-62708-173-3
..., and are caused to flow together and solidify without the application of pressure to the parts being joined. The most important source of heat for OFW is the oxyacetylene welding (OAW) torch. The simplest and most frequently used OFW system consists of compressed gas cylinders, gas pressure regulators, hoses...
Book Chapter

By D.P. Sekulic
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006529
EISBN: 978-1-62708-207-5
... Abstract Brazing technology is continually advancing for a variety of metals including aluminum and its alloys and nonmetals. This article discusses the key physical phenomena in aluminum brazing and the materials for aluminum brazing, including base metals, filler metals, brazing sheet...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006079
EISBN: 978-1-62708-175-7
... Abstract Metals and alloy powders are used in welding, hardfacing, brazing, and soldering applications, which include hardface coatings, the manufacturing of welding stick electrodes and flux-cored wires, and additives in brazing pastes or creams. This article reviews these applications...
Book Chapter

By Charles White
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006301
EISBN: 978-1-62708-179-5
... welding, oxyfuel welding, and braze welding. The article discusses various special techniques, such as groove-face grooving, studding, joint design modifications, and peening, for improving the strength of a weld or its fitness for service. The article describes other fusion welding methods...
Book Chapter

By Mel M. Schwartz
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001345
EISBN: 978-1-62708-173-3
... Abstract This article describes the physical principles of brazing with illustrations and details elements of the brazing process. The elements of brazing process include filler-metal flow, base-metal characteristics, filler-metal characteristics, surface preparation, joint design and clearance...
Book Chapter

By E.B. Gempler
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001455
EISBN: 978-1-62708-173-3
... assemblies. Torch brazing is similar to oxyfuel gas welding in that the heat to effect the joint is applied locally. Oxyacetylene, oxyhydrogen, and oxy-natural gas are used in commercial torch brazing applications. Close temperature control is needed when using the typical BAlSi-3 and BAlSi-4 filler metals...
Book Chapter

By Robert W. Messler, Jr.
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005552
EISBN: 978-1-62708-174-0
...; and fusion welding with directed energy sources, such as laser welding, electron beam welding. The article reviews the different types of nonfusion welding processes, regardless of the particular energy source, which is usually mechanical but can be chemical, and related subprocesses of brazing and soldering...
Book Chapter

Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005647
EISBN: 978-1-62708-174-0
... bonding; dip brazing DBTT ductile-to-brittle transition temperature dc direct current DCEN direct current, electrode negative DCEP direct current, electrode positive DFB diffusion brazing DFW diffusion welding diam diameter DIN Deutsche Industrie-Normen (German Industrial...
Book Chapter

By Matthew J. Lucas, Jr.
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001452
EISBN: 978-1-62708-173-3
... with a silver brazing filler metal for use in a high vacuum atmosphere system Brazing was conducted with a manually manipulated oxyacetylene torch and a strong reducing flame. The assembly shown in Fig. 1 could have been brazed in a furnace or by induction, but production was small and did not justify...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005712
EISBN: 978-1-62708-171-9
..., and vacuum brazing. The article provides information on the selection of overlays and materials such as chromium-carbide-base overlays and tungsten carbide metal-matrix composites. gas metal arc welding high-velocity oxyfuel thermal spray coating material selection oil sand protective overlays...
Book Chapter

Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006556
EISBN: 978-1-62708-210-5
... Excellent Good Polishing Excellent Excellent Good Gas welding Fair Fair Excellent Arc welding Fair Fair Excellent Brazing … … No Heat treating Yes Yes No Anodized appearance Very good Very good Gray brown Electroplating Excellent Excellent Very good Casting...
Book Chapter

By Thomas W. Eagar
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001332
EISBN: 978-1-62708-173-3
..., both in terms of process variations (such as fastening, adhesive bonding, soldering, brazing, arc welding, diffusion bonding, and resistance welding) and in the disciplines needed for problem solving (such as mechanics, materials science, physics, chemistry, and electronics). An engineer with unusually...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0005663
EISBN: 978-1-62708-173-3
...DOI: 10.31399/asm.hb.v06.a0005663 Abbreviations and Symbols A austenite; ampere B bainite DFB diffusion brazing bal balance DFW diffusion welding A angstrom bcc body-centered cubic DHC delayed hydride cracking bct body-centered tetragonal diam diameter AA Aluminum Association c edge length...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003116
EISBN: 978-1-62708-199-3
..., hardening, and stress relieving. Stainless steels are commonly joined by welding, brazing, and soldering. The article lists the procedures and precautions that should be instituted during welding to ensure optimum corrosion resistance and mechanical properties in the completed assembly. forging...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003205
EISBN: 978-1-62708-199-3
... Abstract This article discusses different types of joining processes, including welding, brazing, soldering, mechanical fastening, and adhesive bonding. It examines two broad classes of welding: fusion welding and solid-state welding. The article discusses the process selection considerations...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003162
EISBN: 978-1-62708-199-3
... alloys are either iron-, nickel-, or cobalt-base. Several welding processes are used to apply the hardfacing materials. They range from the traditional (for example, oxyacetylene torch) to more recently developed processes like plasma-transferred arc. To accommodate these different overlay processes...
Book Chapter

Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005646
EISBN: 978-1-62708-174-0
... metal by a blast of air. the addition of ller metal. brazing ller metal or ux due to lack of wet- arc blow The de ection of an electric arc from automatic welding Welding with equipment ting of the base metal. its normal path because of magnetic forces. that performs the welding operation without...
Book

Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.9781627081733
EISBN: 978-1-62708-173-3