... Abstract This article addresses the types, properties, forms, and applications of fibers that are available for use in fiber-reinforced polymeric matrix composites, including glass, graphite, carbon, aramid, boron, silicon carbide, ceramic, continuous oxide and discontinuous oxide fibers. It...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003357
EISBN: 978-1-62708-195-5
... Abstract This article focuses on the production methods, properties, and applications of two main types of commercially available continuous-length ceramic fibers, namely, oxide fibers based on the alumina-silica system and on alpha-alumina, and nonoxide fibers based primarily on beta-phase...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003359
EISBN: 978-1-62708-195-5
... Abstract For the reinforcement of metal-matrix composites, four general classes of materials are commercially available: oxide fibers based primarily on alumina and alumina silica systems, nonoxide systems based on silicon carbide, boron fibers, and carbon fibers. This article discusses the key...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003352
EISBN: 978-1-62708-195-5
... reinforcing fibers. The article describes cost-considered value-in-use of the ultimate-use temperature of selected fibers in three fiber categories: metal fibers or wires, oxide ceramic fibers, and non-oxide ceramic fibers. reinforcing fibers polymer-matrix composites ceramic-matrix composites metal...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003353
EISBN: 978-1-62708-195-5
... Abstract This article discusses the types, oxide composition, as well as mechanical and physical properties of general-purpose and special-purpose glass fibers. It describes the glass melting and fiber forming processes and provides information on important commercial products such as...
Book Chapter

By Paul J. Walsh
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0009241
EISBN: 978-1-62708-195-5
... not melt or soften with heat, allowing them to be used in such high temperature applications as rocket nozzles and aircraft brakes. In fact, their strength actually increases with temperature in non-oxidizing atmospheres. These unique properties are the result of the fiber microstructure, in both the...
Book Chapter

By Karl K. Chang
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0009242
EISBN: 978-1-62708-195-5
... Abstract The chemical composition of Kevlar aramid fiber is poly para-phenyleneterephthalamide. Para-aramid fibers belong to a class of materials known as liquid crystalline polymers. This article discusses the manufacture of aramid fibers and the major fiber forms, such as continuous filament...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003031
EISBN: 978-1-62708-200-6
... Abstract This article discusses the types, properties, and uses of continuous-fiber-reinforced composites, including glass, carbon, aramid, boron, continuous silicon carbide, and aluminum oxide fiber composites. While polyester and vinyl ester resins are the most used matrix materials for...