Skip Nav Destination
Close Modal
Search Results for
open-mold casting
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 524 Search Results for
open-mold casting
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005286
EISBN: 978-1-62708-187-0
... required by downstream manufacturing processes. This article starts with a review of the different forms of ingot and the molten-metal processing techniques involved in ingot casting. It then describes the open-mold casting and direct chill (DC) ingot casting processes. The process variations...
Abstract
Ingot casting is the vital conduit between molten metal provided by primary production and recycling and the manufacture of aluminum and aluminum alloy products. A number of ingot casting processes have been developed to ensure the soundness, integrity, and homogeneity required by downstream manufacturing processes. This article starts with a review of the different forms of ingot and the molten-metal processing techniques involved in ingot casting. It then describes the open-mold casting and direct chill (DC) ingot casting processes. The process variations and solidification in the DC process are summarized. The article explains continuous processes, namely, twin-roll strip casting, slab casting, and wheel-belt processes. It concludes with information on postsolidification processes, including stress relief and scalping, and a discussion of safety practices for ingot casting.
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006485
EISBN: 978-1-62708-207-5
... the molten metal processing and ingot casting process in terms of open-mold casting and direct chill process. The article examines the continuous processes that provide commercial alternatives to conventional ingot casting. It reviews the postsolidification processes in terms of stress relief, homogenization...
Abstract
Ingot casting is the vital conduit between molten metal provided by primary production and recycling, and the manufacture of aluminum and aluminum alloy products. This article discusses various ingot forms, such as remelt ingot, billets, ingots for rolling, fabricating ingot, and particle ingot and powder. It describes the molten metal processing and ingot casting process in terms of open-mold casting and direct chill process. The article examines the continuous processes that provide commercial alternatives to conventional ingot casting. It reviews the postsolidification processes in terms of stress relief, homogenization, and scalping. The article concludes with a discussion on safety limited to ingot casting.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005261
EISBN: 978-1-62708-187-0
... metal up through a narrow-diameter fill (stalk) tube from a furnace usually residing below the casting machine (although there is a version using electromagnetic forces to lift metal into the mold, and then the furnace may be an open hearth located beside the casting machine). The process can...
Abstract
This article provides an overview of conventional low-pressure casting and describes types of furnaces, tooling, and cores. It discusses the casting cycle steps, advantages, mechanical properties, and considerations of counterpressure casting. The article describes the vacuum riserless/pressure riserless casting process for casting aluminum.
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006519
EISBN: 978-1-62708-207-5
...Abstract Abstract Investment casting, in which molten metal is poured into hot molds, allows for the production of aluminum parts with extremely thin sections, knife edges and sharp detail. This article describes the various steps in the investment casting process, including patternmaking...
Abstract
Investment casting, in which molten metal is poured into hot molds, allows for the production of aluminum parts with extremely thin sections, knife edges and sharp detail. This article describes the various steps in the investment casting process, including patternmaking and dimensioning, the design and manufacture of shell molds, melting and casting methods, and postcasting operations such as knockout, core removal, and cleaning. It also addresses a wide range of design considerations, discusses casting defects, and provides several design examples.
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009072
EISBN: 978-1-62708-177-1
... or casting resin and corresponds to clamped samples used in automated polishing heads. It details that cavity molds involve mounting the composite specimens using a casting resin in a preset mold. The article also discusses the mounting of composite materials for hand polishing. automated polishing...
Abstract
This article describes how composite specimens are sectioned, documented, and labeled during sample preparation. The mounting procedures for the specimen are summarized. The article explains sample clamping, which involves not mounting the specimens using an adhesive or casting resin and corresponds to clamped samples used in automated polishing heads. It details that cavity molds involve mounting the composite specimens using a casting resin in a preset mold. The article also discusses the mounting of composite materials for hand polishing.
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006513
EISBN: 978-1-62708-207-5
... during opening of the mold, and ejected by the withdrawal of the retaining core or cores. It is important that the casting remain in the correct mold half until ejection. For castings that have similar geometry in both mold halves, a spring-loaded, push-off mechanism in one mold half might be needed...
Abstract
Aluminum casting in steel and iron permanent molds is used widely throughout industry, and the vast majority of permanent mold castings are made of aluminum and its alloys. There are several methods used to cast aluminum in permanent molds. This article focuses on permanent mold casting with molten aluminum fed by gravity, low pressure, vacuum and centrifugal pressure, and squeeze casting. It discusses the major variables that affect the life of permanent molds, including pouring temperature, casting shape, cooling methods, heating cycles, storage, and cleaning. The article reviews the basic components of mold coatings: refractory fillers, binder, and carrier. Casting defects and suggested corrective actions for permanent mold casting are summarized in a table. The article concludes with a discussion on thin-wall permanent-mold castings.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005265
EISBN: 978-1-62708-187-0
...) An interlock between the melt and the casting chambers is opened, the melt is moved into the casting chamber, and the fill pipe is submerged in the melt. (c) Argon pressure is applied to the casting chamber, causing metal to fill the mold. The mold chamber may or may not be pressurized to achieve the desired...
Abstract
This article discusses the general principles and advantages of countergravity mold filling. It details several production implementations that use differential pressure countergravity mold filling methods, namely the countergravity low-pressure air process, countergravity low-pressure vacuum process, countergravity low-pressure inert atmosphere process, countergravity pressure vacuum process, supported shell technique, loose sand vacuum process, and countergravity centrifugal casting process.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005255
EISBN: 978-1-62708-187-0
... molds and cores, detailing the binders and other materials used, as well as the formulation and control of slurries. Methods for pattern removal, mold firing, melting, casting, postcasting treatment, and inspection are explained. After presenting design recommendations for investment castings...
Abstract
This article reviews the pattern materials used in investment casting, which can be loosely grouped into waxes and plastics. The patternmaking process, pattern tooling, and pattern and cluster assembly are described. The article also describes the manufacture of ceramic shell molds and cores, detailing the binders and other materials used, as well as the formulation and control of slurries. Methods for pattern removal, mold firing, melting, casting, postcasting treatment, and inspection are explained. After presenting design recommendations for investment castings, the article concludes with information on applications and special versions of the investment casting process.
Book Chapter
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0009016
EISBN: 978-1-62708-187-0
... temperature range or freezing interval. Solid shrinkage: The solid casting cools from its solidification temperature to room temperature. Solid shrinkage, also called patternmaker's shrinkage, is accommodated by making the pattern and, therefore; the mold cavity, somewhat larger than the desired...
Abstract
The role of an engineer in designing risers is to make sure that risers provide the feed metal in the right amount, at the right place, and at the right time. This article addresses feed metal volume, riser location, and duration of liquid feed metal. It discusses the three types of feeding systems used in riser design: riser sleeves, topping compounds, and breaker cores.
Book Chapter
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005251
EISBN: 978-1-62708-187-0
.... The mold halves are opened and the pattern removed. Metal is poured into the cavity. The mold is broken and the casting removed. Tons 1–5° 635 25 All $800–4000 Samples: 2–6 weeks Production: 2–6 weeks after approval Investment (lost wax) A metal mold makes wax replicas surrounded...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005352
EISBN: 978-1-62708-187-0
... traditionally have been transferred to a mold or casting unit by tapout or lip pouring by using an intermediate ladle. Traditional metal transfer from the molten-metal supply to the mold is done with open-top ladles ranging from hand held to multiton, crane-supported, mechanized tilt ladles. Underpouring from...
Abstract
This article discusses various molten-metal treatments, namely fluxing, degassing, and molten-metal filtration. It focuses on various molten-metal handling systems for transporting, holding, or delivering molten metal to the mold/die system. These include launders, tundishes, holding furnaces or transport crucibles, molten-metal transfer pumps, teeming ladles, and dosing and pouring furnaces.
Book Chapter
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0009019
EISBN: 978-1-62708-187-0
...Abstract Abstract Cores are separate shapes, of sand, metal, or plaster, that are placed in the mold to provide castings with contours, cavities, and passages. Cored holes should be designed simply as the intended function of the casting permits. This article describes the designing of casting...
Abstract
Cores are separate shapes, of sand, metal, or plaster, that are placed in the mold to provide castings with contours, cavities, and passages. Cored holes should be designed simply as the intended function of the casting permits. This article describes the designing of casting for the use of sand cores and to eliminate cores, with illustrations. It provides general rules for designing cored holes in investment castings. The article discusses the general principles of coremaking with illustrations. It concludes with a comparison between coring and drilling.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005295
EISBN: 978-1-62708-187-0
... directly into the top opening of an ingot mold until the mold is full, as shown in Fig. 1 . Pouring is normally done through a nozzle at the bottom of the ladle, but lip pouring by tilting the ladle is also done in small operations. The flow of steel from the bottom of a ladle is controlled by a stopper...
Abstract
When a heat of steel is melted and refined, it is necessary to solidify it into useful forms for further processing or final use. Ingot casting remains the preferred method for certain specialty, tool, forging, and remelted steels. This article discusses the methods, equipment, and theory for pouring, solidifying, and stripping steel ingots. It describes two basic types of pouring methods, top pouring and bottom pouring, and provides information on equipment such as hot tops, ingot molds, and stools. The design of the ingot is dictated by the application and type of steel involved. The article concludes with information on the applications of solidification simulation.
Book Chapter
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003508
EISBN: 978-1-62708-180-1
... molds. It presents the international classification of common casting<