Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003481
EISBN: 978-1-62708-195-5
... Abstract This article provides information on the potential applications of fiber-reinforced polymer (FRP) composites for maritime craft and offshore drilling platforms. The key benefits gained from using FRP materials together with an examination of the drawbacks and major issues impeding...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004108
EISBN: 978-1-62708-184-9
... offshore structures. Most stationary offshore oil industry platforms are not painted below the waterline, and most marine pipelines are factory coated with special proprietary coatings (see the articles “Corrosion in Petroleum Production Operations,” and “External Corrosion of Oil and Natural Gas...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004210
EISBN: 978-1-62708-184-9
... is also responsible for the external corrosion of offshore platforms and drilling rigs. In oil and gas production, highly stressed structural members are directly exposed to a corrosive, aerated seawater environment. This also makes localized corrosion and corrosion fatigue a particular concern...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001463
EISBN: 978-1-62708-173-3
... Underwater welding techniques are used primarily for the repair of offshore platforms, particularly after the normal 5 year inspection period. However, these techniques have also been very useful during the installation of new offshore structures and undersea pipelines, the installation of hot taps...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005601
EISBN: 978-1-62708-174-0
..., wheel rims, suspension components, and other parts. Small-diameter flux cored electrodes are used for automotive body repair. Gas-shielded flux cored wires are used in the fabrication of mining machinery, off-road equipment, earth-moving machinery, pipe and superstructures for offshore drilling...
Series: ASM Handbook
Volume: 24A
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.hb.v24A.a0006958
EISBN: 978-1-62708-439-0
... applications. VRT, virtual raster. Courtesy of Baker Hughes Companies within the O&G industry, as in many others, use a base of physical assets to operate their business. Examples of such assets include offshore platforms, land rigs, and refineries, which require regular maintenance...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005258
EISBN: 978-1-62708-187-0
..., tubes for the chemical processing industry, foundation piles, and building columns. Centrifugal casting is sometimes used to produce nonrotating gas turbine components of heat-resistant materials. Offshore petroleum production platforms in the oil and gas industry use centrifugally cast tubes in various...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001403
EISBN: 978-1-62708-173-3
...), and corrosive and erosive effects, especially for reentry into the atmosphere. Underwater Applications A wide variety of material properties are involved in the application of weldments under water. Corrosion resistance is frequently a major concern, especially in seawater. Ships and offshore drilling...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005565
EISBN: 978-1-62708-174-0
... for welding projects that require a number of welding arcs within close proximity to each other, such as large construction projects, power plant and chemical plant turnaround, large offshore drilling platforms, and so on. There are two systems in common use: Resistance grid Multiple dc positive...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004134
EISBN: 978-1-62708-184-9
... in designing systems with acceptable cold-climate corrosion performance. Topics include location, inappropriate measures, special factors, and ergonomics. Location Some of the highest marine corrosion rates in the world are found on offshore petroleum production platforms in Cook Inlet, AK, ( Ref 7...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003325
EISBN: 978-1-62708-176-4
... qualification, and the weld service assessment. The article describes two general types of measurements for residual stress in welds: locally destructive techniques and nondestructive techniques. Locally destructive techniques include hole drilling, chip machining, and block sectioning. Nondestructive...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001080
EISBN: 978-1-62708-162-7
... heaters, condensers, thin-walled tubing  Offshore installations Cooling equipment, condensers, heat exchangers, piping and tubing, flanges, deep-drilling riser pipes, flexible risers, desulfurizes, catalytic crackers, sour water strippers, regenerators, structural components Biomedical engineering...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004211
EISBN: 978-1-62708-184-9
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002395
EISBN: 978-1-62708-193-1
... a growing discipline over the past 30 years. Steel structures can cover a diverse number of markets, such as construction of bridges and buildings, pressure vessels, construction and mining equipment, and offshore platforms and ships. Both carbon, high-strength low-alloy (HSLA) and alloy steels are used...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006041
EISBN: 978-1-62708-172-6
... stadiums, water storage tanks, bridges, rail cars, offshore drilling platforms, and other assorted applications. Application techniques have included spray, brush, and rolling methods. These types of coatings can be applied at ambient temperatures with standard commercial spray equipment. The typical pot...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003806
EISBN: 978-1-62708-183-2
...-alloy steels are being considered around the world for the structural members of waste packages. Marine Applications Carbon and low-alloy steels are used for submerged or partly submerged structures—both in harbors for sea walls and piers, for example, and offshore for oil drilling platforms...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003516
EISBN: 978-1-62708-180-1
... reactors, offshore drilling platforms, and the like. The more knowledge and information one has at the beginning of the design process, the more quickly one can define the type of material to be used. This cannot be overstated. The designer must work with the engineer to define the anticipated use...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006022
EISBN: 978-1-62708-175-7
... parts may be turned, milled, drilled, tapped, and ground. Machinability depends on the density and the microstructure of the material. For a PM material of a given density and microstructure, the machinability will depend on the type of cutting operation being performed, the cutting tool material...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006433
EISBN: 978-1-62708-192-4
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003417
EISBN: 978-1-62708-195-5
... low flame, smoke, and toxicity protect passengers in the event of fire. The Channel Tunnel, or Chunnel, project (connecting England and France under the English Channel) utilized a tremendous amount of pultruded product for electrical cable support systems and other structural applications. Offshore...