1-15 of 15

Search Results for nonmechanical properties

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

By John Moylan
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003442
EISBN: 978-1-62708-195-5
... Abstract Characterization of nonmechanical properties is performed in the testing and certification of composite materials. This article focuses on the properties of composites that are commonly investigated. The properties include: per ply thickness; constituent content; density; coefficient...
Book Chapter

By Frederick T. Wallenberger
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003352
EISBN: 978-1-62708-195-5
... Abstract Reinforcing fibers are a key component of polymer-matrix composites (PMCs), ceramic-matrix composites (CMCs), and metal-matrix composites (MMCs). This article discusses the mechanical and nonmechanical properties of these composites. It presents an overview of PMC, CMC, and MMC...
Book Chapter

Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005174
EISBN: 978-1-62708-186-3
... Abstract This article focuses on the mechanical and nonmechanical cutting methods used in metal fabrication industries. The most prevalent equipment used for mechanical cutting includes shears, iron workers, nibblers, and band saws. Nonmechanical methods of cutting include gas cutting, electric...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001241
EISBN: 978-1-62708-170-2
.... The conventional wisdom is that the strength of a work material decreases with temperature and increases with strain rate, and that these two opposing effects have a minimal net effect on machining processes. However, this may not always be the case. Thermal properties are also of interest to the nonmechanical...
Book Chapter

By Greg Kress
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003392
EISBN: 978-1-62708-195-5
... restrictions Life cycle durability and damage tolerance Maintainability and reparability Nonmechanical properties, such as flammability and electrical properties From the prioritized design criteria, all of the engineering, material, process, and configuration options should be evaluated...
Book Chapter

By J.R. Davis
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001303
EISBN: 978-1-62708-170-2
... Abstract This article provides a brief review of the classification and characteristics of cast irons. It describes the processes used to clean iron castings, including mechanical cleaning and finishing and nonmechanical cleaning. The article discusses surface treatments used to extend casting...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001403
EISBN: 978-1-62708-173-3
... systems, and sheet metal. Material properties and welding processes that may be significant in meeting design goals are also described. aerospace systems automobiles buildings and bridges damage tolerance durability fabricability gas metal arc welding joinability joining laser beam welding...
Book Chapter

Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006335
EISBN: 978-1-62708-179-5
... is an important prerequisite of any coating process. Suitable levels of cleanliness and surface roughness are achieved by various mechanical and nonmechanical methods. If castings are heat treated before they are coated, the choice of heat treatment conditions can influence the properties of the coating...
Book Chapter

By Tom Duerig
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005658
EISBN: 978-1-62708-198-6
... Abstract This article focuses on the specific aspects of nitinol that are of interest to medical device designers. It describes the physical metallurgy, physical properties, and tensile properties of the nitinol. The article discusses the factors influencing superelastic shape memory effects...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003425
EISBN: 978-1-62708-195-5
... Abstract Advanced thermoplastic composites possess impact resistance, fracture toughness, and elevated temperature endurance properties due to their melt-fusible nature. This article presents the material options available for thermoplastic composites such as pseudothermoplastics, post...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006938
EISBN: 978-1-62708-395-9
... components are sourced externally, the specification process takes on more complexity. It is not unusual for materials and component parts to be specified based on a limited number of attributes that have provided utility in certain uses and can be an effective proxy for a wider range of properties. However...
Book Chapter

By George M. Goodrich
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005322
EISBN: 978-1-62708-187-0
... and the various metallurgical aspects, such as the composition, alloying element, solidification, and graphite morphologies, of different types of cast iron. It describes the physical properties for various cast irons and the influence of microstructure and chemical composition on each property. The article...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006545
EISBN: 978-1-62708-210-5
... features also are important factors in improving resistance to SCC without disturbing the high-performance mechanical properties of the material ( Ref 14 ). Microstructural aspects include precipitates in the grain boundaries, equilibrium precipitates along the grain boundary, and the precipitate-free zone...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.9781627083959
EISBN: 978-1-62708-395-9
Book Chapter

By W. R. Warke
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003553
EISBN: 978-1-62708-180-1
... tip, or some other nonmechanical factor. Fig. 4 Stress-corrosion crack growth. (a) Schematic diagram of typical crack-propagation rate as a function of crack-tip stress-intensity behavior illustrating the regions of stage 1, 2, and 3 crack propagation as well as identifying the plateau velocity...