1-20 of 620

Search Results for nonferrous castings

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005306
EISBN: 978-1-62708-187-0
... lead alloys nickel alloys non-ferrous alloys titanium alloys copper drossing softening desilvering CASTING OF NONFERROUS ALLOYS on a tonnage basis is dominated by aluminum, which is cast by ingot and continuous processes for primary mills and by all foundry (shape casting) processes...
Image
Published: 01 December 2008
Fig. 1 Nonferrous casting processes by tons poured. Source: From data of AFS 2002 survey. More
Image
Published: 15 June 2019
Fig. 1 Nonferrous casting processes by tons poured. Source: From data of American Foundry Society’s 2002 survey More
Image
Published: 01 December 2008
Fig. 5 U.S. nonferrous casting shipments from 1977 to 1986. Source: Ref 2 More
Image
Published: 01 December 2008
Fig. 9 Trends in production of nonferrous metal castings. Source: Ref 3 More
Book Chapter

By Thomas S. Piwonka
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003175
EISBN: 978-1-62708-199-3
... Abstract Aluminum alloys are primarily used for nonferrous castings because of their light weight and corrosion resistance. This article discusses at length the melting and metal treatment, structure control, sand casting, permanent mold casting, and die casting of aluminum alloys. It also...
Book Chapter

By Charles D. Nelson, Wayne Rasmussen, John Jorstad
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005249
EISBN: 978-1-62708-187-0
... Abstract This article discusses slurry molding that encompasses two distinct processes: plaster molding and ceramic molding. Plaster mold casting is a specialized casting process used to produce nonferrous castings that have greater dimensional accuracy, smoother surfaces, and more finely...
Book Chapter

By Sujoy Krishna Chaudhury
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005230
EISBN: 978-1-62708-187-0
... Abstract This article provides an overview of heat treatment processes, namely, solution heat treatment, quenching, natural aging, and artificial aging. It contains a table that lists the various heat treatment tempers commonly practiced for nonferrous castings. The article describes...
Book Chapter

By Randall Counselman
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005345
EISBN: 978-1-62708-187-0
... Abstract Repair welding is a necessary operation for most fabricators and can cost more than the price of the original component if performed improperly. This article provides a discussion on the repair welding of castings for ferrous and nonferrous materials. The discussion focuses...
Book Chapter

By Thomas S. Piwonka
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003170
EISBN: 978-1-62708-199-3
..., steering and suspension components, etc.), prosthetics, and gas turbine engine hardware. This introduction explains the steps involved in making a casting using a simplified flow diagram, and discusses the ferrous and nonferrous alloys used for metal casting. casting alloys ferrous alloys metal...
Book Chapter

By J.L. Jorstad
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005187
EISBN: 978-1-62708-187-0
... …  Investment All 2 NA Small to medium Outstanding  Replicast All 1 NA Medium to large … Centrifugal casting  Metal mold Nonferrous 3 Yes Small to medium …  Sand mold All 2 Yes Small to medium … Permanent mold and semipermanent mold  Gravity   Static top pour...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005186
EISBN: 978-1-62708-187-0
... Motor vehicles Metalworking machinery Other major markets include steel manufacturing, spring goods, heating and air conditioning, recreation equipment, industrial materials handling equipment, ships and boats, and aircraft and aerospace (a) Nonferrous castings Aluminum Auto and light...
Book Chapter

By Richard J. Fruehan, Prince N. Anyalebechi
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005192
EISBN: 978-1-62708-187-0
... Abstract This article reviews the solubilities of the common gases present in ferrous metals, such as cast irons, and nonferrous metals, such as aluminum, copper, magnesium, and their alloys. The kinetics of the relevant reactions, reactions during solidification, and possible methods...
Book Chapter

Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006250
EISBN: 978-1-62708-169-6
... growth. The article also describes the various types of solid-state transformations such as isothermal transformation and athermal transformation, resulting from the heat treatment of nonferrous alloys. It provides information on the homogenization of chemical composition within a cast structure...
Book Chapter

By Scott McIntyre
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005252
EISBN: 978-1-62708-187-0
... Abstract Shell molding is used for making production quantities of castings that range in weight from a few ounces to approximately 180 kg (400 lb), in both ferrous and nonferrous metals. This article lists the limitations or disadvantages of shell mold casting. It describes the two methods...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003276
EISBN: 978-1-62708-176-4
..., size and shape of the workpiece, specimen surface flatness and surface condition, and indent location. The article focuses on the selection for specific types of materials, such as steels, cast irons, nonferrous alloys, and plastics, and industrial applications, of hardness tests. hardness test...
Book Chapter

By Paul K. Trojan
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005193
EISBN: 978-1-62708-187-0
... the occurrence of inclusions in any cast metal. It presents a discussion on the inclusions in ferrous and nonferrous alloys, including steels, cast irons, aluminum alloys, copper alloys, and magnesium alloys. aluminum alloys cast irons copper alloys ferrous alloys magnesium alloys nonferrous alloys...
Book Chapter

Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005644
EISBN: 978-1-62708-174-0
... Abstract Weldability refers to the ease of welding a material under the imposed fabrication conditions to perform satisfactorily during service. This article is a comprehensive collection of tables that summarize the general weldability of cast irons, steels, nonferrous metals, and their alloys...
Book Chapter

By Yeou-Li Chu
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005292
EISBN: 978-1-62708-187-0
... Abstract High-pressure die casting is a fast method for the net shape manufacturing of parts from nonferrous alloys. This article reviews the automation technologies for the different stages or steps of the process. These steps include liquid metal pouring, injection, solidification, die open...
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005200
EISBN: 978-1-62708-187-0
... Abstract Vacuum induction melting (VIM) is often done as a primary melting operation followed by secondary melting (remelting) operations. This article presents the process description of VIM and illustrates potential processing routes for products, which are cast from VIM ingots or electrodes...