Published: 30 June 2023
Fig. 6 Potential in-process nondestructive testing and metrology inspection methods for defect detection in laser powder-bed fusion/directed-energy deposition. IR, infrared; CMM, coordinate measuring machine; GOM, 3D inspection software More
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003228
EISBN: 978-1-62708-199-3
... NDT methods. Additional information on the various types of NDT methods can be obtained from the American Society for Nondestructive Testing (Columbus, OH), Nondestructive Testing, Volume 03.03, published annually by ASTM (Philadelphia, PA), and in Nondestructive Evaluation and Quality Control...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003463
EISBN: 978-1-62708-195-5
... Abstract Mechanical and environmental loadings cause a variety of failure modes in composites, including matrix cracking, fiber-matrix debonding, delamination between plies, and fiber breakage. This article summarizes visual analysis and nondestructive testing methods for the failure analysis...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003237
EISBN: 978-1-62708-199-3
... laboratory testing, production testing, and structural testing. The article includes a section in which the characteristics of acoustic emission inspection are compared with other nondestructive testing methods. Further, it briefly reviews the key elements of the acoustic-emission instrumentation, which...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001473
EISBN: 978-1-62708-173-3
... Abstract This article describes the applications, methods, and limitations of five principal nondestructive test methods, namely, penetrant testing, magnetic-particle testing, eddy current testing, radiographic testing, and ultrasonic testing. The article also provides guidance for the method...
Image
Published: 01 August 2018
Fig. 8 Ground weld surface after visual inspection and prior to using a subsequent different nondestructive testing method. Courtesy of A. Antonatos More
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006438
EISBN: 978-1-62708-190-0
..., Welding of Pipelines and Related Facilities 7 ACI 349.3-02, Evaluation of Existing Nuclear Safety Related Concrete Structures 14 ACI 228, Nondestructive Test Methods for Evaluation of Concrete in Structures 15 International Atomic Energy Agency Guidebook on Nondestructive Testing...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006447
EISBN: 978-1-62708-190-0
... and Certification of NDT Personnel”). Basic Principles There are many definitions for VI, the shortest given by British Standards Institute’s standard BS EN 1330-10:2003, “Non-Destructive Testing. Terminology. Terms Used in Visual Testing,” as “visual testing method of nondestructive testing using...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005345
EISBN: 978-1-62708-187-0
... properties, such as tensile strength, yield strength, and elongation. This information is useful in selecting a welding process and filler metal for the repairs. If the size or configuration of the casting precludes the removal of specimens, then nondestructive methods and hardness testing may be used...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006445
EISBN: 978-1-62708-190-0
..., and gamma-ray density determination. The article also discusses the methods for automated nondestructive testing of pressed and sintered PM parts: acoustic methods-resonance testing, eddy current testing, magnetic bridge comparator testing, ultrasonic techniques, radiographic techniques, gamma-ray density...
Series: ASM Handbook
Volume: 24A
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.hb.v24A.a0006974
EISBN: 978-1-62708-439-0
... Abstract X-ray radiography and computed tomography (CT) are nondestructive testing (NDT) tools particularly well suited to additive manufacturing (AM). A brief overview of NDT for AM is presented in this article, including other NDT methods, followed by identifying the key advantages...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005857
EISBN: 978-1-62708-167-2
... material. The product and process are verified at specified frequency after each key process. The combination of nondestructive testing methods can help to guarantee the quality of induction heat treatment operations. The NDE techniques can be used to interrogate material properties during...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006479
EISBN: 978-1-62708-190-0
...-related documents can be found in Volume 03.03, Nondestructive Testing . Table 1 lists many ASTM International guides, practices, and test methods relevant to NDT. The most up-to-date information can be found on the ASTM International website ( Ref 1 ) and in Ref 2 . A selection of ASTM...
Series: ASM Handbook
Volume: 24A
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.hb.v24A.a0007023
EISBN: 978-1-62708-439-0
... Abstract This article covers defect formation and classification, followed by a brief description of the most common nondestructive testing (NDT) methods used for postbuild inspection. Descriptions of the established and emerging NDT techniques for in-process monitoring (IPM) and in-process...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006449
EISBN: 978-1-62708-190-0
... examination methods based on flaw type and product stage is presented in a table. The article also discusses in-service inspection of tubular products and presents an example that illustrates the importance of nondestructive testing (NDT) for welds in austenitic stainless steel tubing. tubular products...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003437
EISBN: 978-1-62708-195-5
... Abstract This article describes the characterization techniques, mechanical tests, and nondestructive evaluation methods that are commonly used for metal-matrix composites. It also tabulates typical methods of particle size and size distribution measurement, as well as mechanical test...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001478
EISBN: 978-1-62708-173-3
... and conformance to specifications. Brazing procedures should be qualified to meet specification requirements using both nondestructive and destructive inspection methods. Nondestructive Inspection Nondestructive inspection ( Ref 6 ) or testing techniques include visual, leak, radiographic, ultrasonic...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006336
EISBN: 978-1-62708-179-5
..., or number of these anomalies exceeds the maximum allowed by the purchaser. The nondestructive methods include visual inspection, dimensional inspection, liquid penetrant inspection, magnetic-particle inspection, eddy-current inspection, radiographic inspection, ultrasonic inspection, resonant testing...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006462
EISBN: 978-1-62708-190-0
... Abstract Both nondestructive testing (NDT) and nondestructive evaluation (NDE) use noninvasive measurement techniques to gain information about defects and various properties of materials, components, and structures. This article begins with a discussion on the historical development...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003240
EISBN: 978-1-62708-199-3
... Abstract Holography is basically a two-step process for creating a whole three dimensional image of a diffusely reflecting object having some arbitrary shape. This article discusses the advantages, disadvantages and applications of using the optical holography method in nondestructive...