Skip Nav Destination
Close Modal
Search Results for
noble metal alloys
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 254 Search Results for
noble metal alloys
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003620
EISBN: 978-1-62708-182-5
..., and noble metal alloys dealloying. The current-potential behavior of a binary alloy undergoing selective dissolution is reviewed. The article highlights the four mechanisms required for the formation of porous metals: ionization-redeposition, surface diffusion, volume diffusion, and percolation model...
Abstract
Dealloying is a corrosion process in which one or more elements are selectively dissolved, leaving behind a porous residue of the remaining elements. This article describes the dealloying in various systems, namely, dezincification, graphitic corrosion, dealuminification, and noble metal alloys dealloying. The current-potential behavior of a binary alloy undergoing selective dissolution is reviewed. The article highlights the four mechanisms required for the formation of porous metals: ionization-redeposition, surface diffusion, volume diffusion, and percolation model of selective dissolution.
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005670
EISBN: 978-1-62708-198-6
... discussion on the ancient history of noble and precious metal use in dentistry is provided. The article discusses the use of direct gold dental filling materials, direct silver dental filling materials, traditional amalgam alloys, high-copper amalgam alloys, and gallium alloys in biomedical applications...
Abstract
This article focuses on the use of noble and precious metals for biomedical applications. These include gold, platinum, palladium, ruthenium, rhodium, iridium, and osmium. The physical and mechanical properties of noble and precious metals are presented in tables. A brief discussion on the ancient history of noble and precious metal use in dentistry is provided. The article discusses the use of direct gold dental filling materials, direct silver dental filling materials, traditional amalgam alloys, high-copper amalgam alloys, and gallium alloys in biomedical applications. It also provides information on gold coatings and iridium oxide coatings for stents.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004181
EISBN: 978-1-62708-184-9
... resistance of various metals and alloys in HCl, including carbon and alloy steels, austenitic stainless steels, standard ferritic stainless steels, nickel and nickel alloys, copper and copper alloys, corrosion-resistant cast iron, zirconium, titanium and titanium alloys, tantalum and its alloys, and noble...
Abstract
Hydrochloric acid (HCl) may contain traces of impurities that will change the aggressiveness of the solution. This article discusses the effects of impurities such as fluorides, ferric salts, cupric salts, chlorine, and organic solvents, in HCl. It describes the corrosion resistance of various metals and alloys in HCl, including carbon and alloy steels, austenitic stainless steels, standard ferritic stainless steels, nickel and nickel alloys, copper and copper alloys, corrosion-resistant cast iron, zirconium, titanium and titanium alloys, tantalum and its alloys, and noble metals. The article illustrates the effect of HCl on nonmetallic materials such as natural rubber, neoprene, thermoplastics, and reinforced thermoset plastics. It also tabulates the corrosion of various metals in dry hydrogen chloride.
Book: Corrosion: Materials
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003834
EISBN: 978-1-62708-183-2
... control: noble metal clad systems, corrosion barrier systems, sacrificial metal systems, transition metal systems, complex multilayer systems, and clad diffusion alloys. cladding corrosion control sacrificial metal systems clad metals noble metal clad systems corrosion barrier systems...
Abstract
This article describes the principal cladding processes and methods for calculating properties of clad metals. It reviews the designing processes of clad metals to achieve specific requirements. The article discusses six categories of clad metal systems designed for corrosion control: noble metal clad systems, corrosion barrier systems, sacrificial metal systems, transition metal systems, complex multilayer systems, and clad diffusion alloys.
Book: Corrosion: Materials
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003808
EISBN: 978-1-62708-183-2
...Abstract Abstract From the standpoint of corrosion protection of iron and steel, metallic coatings can be classified into two types: noble coatings and sacrificial coatings. This article focuses on hotdipped zinc, aluminum, zinc-aluminum alloy and aluminum-zinc alloy coatings. It discusses...
Abstract
From the standpoint of corrosion protection of iron and steel, metallic coatings can be classified into two types: noble coatings and sacrificial coatings. This article focuses on hotdipped zinc, aluminum, zinc-aluminum alloy and aluminum-zinc alloy coatings. It discusses the Sendzimir process and the Cook-Norteman process, which are the two commercial processes that are used for almost all hot-dip galvanized sheet steel in the United States. The article provides a discussion on the aqueous corrosion and atmospheric corrosion of galvanized steel and aluminized steel, as well as the intergranular corrosion of galvanized steel.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003616
EISBN: 978-1-62708-182-5
... current density ( i corr ) as illustrated ( Fig. 6 ). Alloy systems ennobled in this fashion are relatively uncommon and often require very system-specific alloying additions, habitually noble metals (e.g., platinum, gold, palladium, etc.). Frequently, ennoblement is achieved only after enrichment...
Abstract
The corrosion behavior of a metal or alloy is determined by its composition and structural features, the environment and stresses to which it is exposed, and the behavior of any corrosion products generated. This article provides a detailed discussion on the fundamentals of pure metals, impure metals, and alloys. It highlights the ways in which the metallurgical variables, namely, composition and structure, influence the corrosion properties of metals and alloys in aqueous environment.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004209
EISBN: 978-1-62708-184-9
... been used. The gold-base alloys contain silver and copper as principal alloying elements, with smaller additions of palladium, platinum, zinc, indium, and other noble metals as grain refiners. The silver-base alloys contain palladium as a major alloying element, with additions of copper, gold, zinc...
Abstract
This article describes dental alloy compositions and its properties. It discusses the safety and efficacy considerations of dental alloy devices. The article defines and compares interstitial fluid and oral fluid environments. Artificial solutions developed for the testing and evaluation of dental materials are summarized. The article examines the effects of restoration contact on electrochemical parameters and reviews the concentration cells developed by dental alloy-environment electrochemical reactions. The composition and characterization of biofilms, corrosion products, and other debris that deposit on dental material surfaces are discussed. The article evaluates the types of alloys available for dental applications, including direct filling alloys, crown and bridge alloys, partial denture alloys, porcelain fused to metal alloys, wrought wire alloys, soldering alloys, and implant alloys. The effects of composition and microstructure on the corrosion of each alloy group are also discussed. The article concludes with information on the tarnishing and corrosion behavior of these alloys.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003607
EISBN: 978-1-62708-182-5
... dissimilar metals or alloys causes electron flow between them when they are electrically coupled in a conductive solution. The direction of electron flow, and therefore the galvanic behavior, depends on which metal or alloy is more active. The more active metal or alloy becomes anodic, and the more noble...
Abstract
This article describes the various factors that affect the extent of corrosion resulting from galvanic coupling. The factors include galvanic series, polarization behavior, and geometric relationship of metals and alloys. The article briefly discusses the various modes of attack that lead to galvanic corrosion of anodic members. It also explains the three electrochemical techniques of screening tests for predicting galvanic corrosion. The electrochemical techniques comprise of potential measurements, current measurements, and polarization measurements. The article provides a detailed discussion on the performance of alloy groupings. It concludes with information on various control methods that reduce or eliminate galvanic-corrosion effects.
Book: Thermal Spray Technology
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005709
EISBN: 978-1-62708-171-9
... attack of the substrate. Exclusion of oxygen sometimes can cause crevice corrosion. Fig. 1 Galvanic series of selected metals and alloys in seawater showing their corrosion potentials. Adapted from Ref 4 Cathodic or Noble Coatings Anodic or Sacrificial Coatings Application...
Abstract
Corrosion of marine- and land-based infrastructure is of major concern and its control forms an important objective. Thermal spray coatings (TSCs) are widely used for corrosion protection. This article focuses on two types of TSCs: cathodic or noble coatings and anodic or sacrificial coatings. It describes the factors affecting the performance of sacrificial TSCs in atmospheric and immersion environments. The article provides information on the applications of sacrificial TSCs, non-sacrificial coatings, and sealants/top coats, and exemplifies the use of sacrificial TSCs on structures for corrosion protection.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004170
EISBN: 978-1-62708-184-9
... are primarily based on their electrical, magnetic, and optical properties, ranging from noble metals such as gold and silver to more reactive metals such as aluminum and its alloys. Table 1 shows typical applications of conductors and contact materials ( Ref 18 ). The functionality of devices requires...
Abstract
This article discusses the influence of the materials, design, package type, and environment on corrosion in microelectronics. It describes the common sources and mechanisms of corrosion in microelectronics, including anodic, cathodic, and electrolytic reactions resulting in uniform corrosion, galvanic corrosion, pitting corrosion, creep corrosion, dendrite growth, fretting, stress-corrosion cracking, and whisker growth. The article presents effective measures for minimizing the moisture retention in hermetic packages and/or moisture ingress in plastic packages. It concludes with information corrosion tests.
Book: Thermal Spray Technology
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005735
EISBN: 978-1-62708-171-9
... and the noble coating with an electrolyte will result in a rapid attack of the ferrous metal, that is, the substrate. Unsealed areas of the coating, stress fractures, or other inadvertently exposed edges will, unfortunately, ensure such exposure. Generally, the removal of the coating by such corrosion is rapid...
Abstract
This article focuses on noble and neutral coatings and the requirements necessary to achieve successful industrial applications. These include corrosion and wear control and repair applications in processing and chemical industries, and valve and downhole drilling applications in the petrochemical industry. The article also discusses substrate chemistry and preparation; coating selection process and microstructure; sealing by chemical, post-heat treatments, and laser processing; and thermal spray process alternatives.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001260
EISBN: 978-1-62708-170-2
... being developed. This article is focused mainly on the science and engineering of multiple-layer metallic alloys with nanometer-scale modulation wavelengths, because these are the materials that have gained the most attention for surface engineering. Throughout this chapter a solidus, or virgule...
Abstract
Multiple-layer alloy electrodeposition involves the formation of an inhomogeneous alloy consisting of lamellae of different composition. This article reviews the process description, engineering parameters, characterization, and applications of multiple-layer alloys. Pulsed-current plating and pulsed-potential plating are also discussed.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001296
EISBN: 978-1-62708-170-2
..., potentials are listed for these metals under different conditions. As can be seen, the order of the different metals changes. For corrosion processes, such tables indicate which metal of a pair in contact is more noble or less noble. Factors influencing the actual potential values are temperature...
Abstract
This article focuses on the testing and typical corrosion behavior of coating-substrate systems in aqueous solutions and humid aggressive atmospheres. It includes a short review of the fundamentals of corrosion, followed by a discussion of specific system behavior, electrochemical and laboratory accelerated tests, and simulated service tests. The article also contains examples of different types of corrosion damage and presents guidelines for improving corrosion resistance.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003158
EISBN: 978-1-62708-199-3
... cost, and great versatility of application. Thermocouples are grouped into two broad categories, namely, standard thermocouples, including five base-metal thermocouples and three noble-metal thermocouples that have been given letter designations, and nonstandard thermocouples, including iridium-rhodium...
Abstract
Thermocouple devices are the most widely used devices for measurement of temperature in the metals industry. Favorable characteristics of these devices include good accuracy, suitability over a wide temperature range, fast thermal response, ruggedness, high reliability, low cost, and great versatility of application. Thermocouples are grouped into two broad categories, namely, standard thermocouples, including five base-metal thermocouples and three noble-metal thermocouples that have been given letter designations, and nonstandard thermocouples, including iridium-rhodium, platinum-molybdenum, platinel, and tungsten-rhenium thermocouples. This article discusses the basic principles, classification, and properties of thermocouples, and the techniques for insulating and protecting thermocouple wires from the operating environment.
Book Chapter
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
... by metal dissolution or oxidation. The more cathodic material is more corrosion resistant (i.e., more noble). Fig. 3 Galvanic series of metals and alloys in seawater. Alloys are listed in order of the potential they exhibit in flowing seawater; those indicated by the black rectangle were tested...
Abstract
This article addresses the forms of corrosion that contribute directly to the failure of metal parts or that render them susceptible to failure by some other mechanism. It describes the mechanisms of corrosive attack for specific forms of corrosion such as galvanic corrosion, uniform corrosion, pitting and crevice corrosion, intergranular corrosion, and velocity-affected corrosion. The article contains a table that lists combinations of alloys and environments subjected to selective leaching and the elements removed by leaching.
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
... galvanic cell are prone to corrode by metal dissolution or electrochemical oxidation. The more cathodic material is more corrosion resistant (i.e., more noble). Fig. 3 Galvanic series of metals and alloys in seawater. Alloys are listed in order of the potential they exhibit in flowing seawater...
Abstract
Corrosion is the electrochemical reaction of a material and its environment. This article addresses those forms of corrosion that contribute directly to the failure of metal parts or that render them susceptible to failure by some other mechanism. Various forms of corrosion covered are galvanic corrosion, uniform corrosion, pitting, crevice corrosion, intergranular corrosion, selective leaching, and velocity-affected corrosion. In particular, mechanisms of corrosive attack for specific forms of corrosion, as well as evaluation and factors contributing to these forms, are described. These reviews of corrosion forms and mechanisms are intended to assist the reader in developing an understanding of the underlying principles of corrosion; acquiring such an understanding is the first step in recognizing and analyzing corrosion-related failures and in formulating preventive measures.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003687
EISBN: 978-1-62708-182-5
... be pore free and flaw free. It is very difficult to obtain impervious coatings of more noble metals on steel or zinc alloys. Substantial metal thicknesses, usually 25 μm (1 mil) or more, are required. With some of these metallic deposits, particularly the noble metals, thinner coatings applied by pulse...
Abstract
This article discusses the various factors that affect the corrosion performance of electroplated coatings. It describes the effects of environment and the deposition process on substrate coatings. The article provides a discussion on the electrochemical techniques capable of predicting the corrosion performance of a plated part. It reviews the designs of coating systems for optimal protection of the substrate. The article also discusses controlled weathering tests and accelerated tests used to predict and determine the relative durability of the coating.
Book: Corrosion: Materials
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003822
EISBN: 978-1-62708-183-2
..., as discussed in a subsequent section of this article. In all cases, the basic remedy aims at maintaining creviced metal surfaces at sufficiently noble potentials where titanium alloy passivity is assured ( Ref 20 ). Crevice Corrosion Testing Crevice corrosion testing of titanium alloys generally aims...
Abstract
Titanium alloys are often used in highly corrosive environments because they are better suited than most other materials. The excellent corrosion resistance is the result of naturally occurring surface oxide films that are stable, uniform, and adherent. This article offers explanations and insights on the most common forms of corrosion observed with titanium alloys, including general corrosion, crevice corrosion, anodic pitting, hydrogen damage, stress-corrosion cracking, galvanic corrosion, corrosion fatigue, and erosion-corrosion. It also provides practical strategies for expanding the useful application range for titanium and includes a comprehensive overview of available corrosion data.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003614
EISBN: 978-1-62708-182-5
... attributed to the fine grain size and enrichment of alloying and trace elements in the layer, most notably magnesium. Noble intermetallic particles such as Al 3 Fe dispersed throughout the layer are believed to be important in triggering electrochemical activity of the layer by forming microgalvanic couples...
Abstract
Filiform corrosion has been observed to occur under a wide range of organic coatings and proceeds with the same general characteristics on steel, aluminum, and magnesium. This article describes the standard tests for filiform corrosion, characteristics and mechanisms of filiform corrosion in steels, as well as coated aluminum and magnesium. It concludes with information on the prevention and mitigation of filiform corrosion accomplished through the adjustment of the environment and changes in the substrate and coating systems.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003142
EISBN: 978-1-62708-199-3
... group includes noble metals such as platinum, palladium, and rhodium. The second includes nickel, molybdenum, and tungsten. The third group includes zirconium, tantalum, chromium, and possibly molybdenum. Considerable work has been done on the use of noble metals as alloying additions in titanium...
Abstract
This article discusses corrosion resistance of titanium and titanium alloys to different types of corrosion, including galvanic corrosion, crevice corrosion, stress-corrosion cracking (SCC), erosion-corrosion, cavitation, hot salt corrosion, accelerated crack propagation, and solid and liquid metal embrittlement. A short section discusses the addition of alloys that can improve the corrosion resistance of titanium.