Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006269
EISBN: 978-1-62708-169-6
... information on the wear and fatigue properties and corrosion resistance of nitrided titanium alloys, as well as the effect of nitriding on the biocompatibility of titanium. It also compares plasma-nitrided titanium alloys with alloy steels. It concludes with a short discussion on the effect of nitriding on...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003090
EISBN: 978-1-62708-199-3
... and nitrides. These steels have very low strength, but are used to produce components that are difficult or impossible to form from other steels. Very-low-carbon, fully ferritic steels (0.001% C) are now being manufactured for automotive components that harden during the paint-curing cycle. These...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006273
EISBN: 978-1-62708-169-6
..., tempering (a) Calculated with thermodynamic values from Ref 2 . Source: Ref 3 Fig. 1 Typical thickness and hardness of nitrided layers on steels as well as titanium and aluminum alloys. PZ, precipitation zone; NL, nitride layer (compound layer). Source: Ref 2 Table 2...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003197
EISBN: 978-1-62708-199-3
... depth measurement methods case hardening cyaniding nitriding nitrocarburizing steel CARBURIZING is a case-hardening process in which carbon is dissolved in the surface layers of a low-carbon steel part at a temperature sufficient to render the steel austenitic...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001306
EISBN: 978-1-62708-170-2
... (electrical steels). This article provides a detailed discussion on the various surface treatments, including cleaning, nitriding, carburizing, coating, and plating, performed on specialty steels. carburizing case hardening cleaning coating corrosion resistance deburring electrical steels ferrous...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005927
EISBN: 978-1-62708-166-5
... tempering tool steel FLUIDIZED-BED TECHNIQUES are not new to the metalworking industry. They were first developed in the 1960s to 1970s for the treatment of metals. As the understanding of fluidization fundamentals improves, several major technological innovations have occurred since then: The use...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001305
EISBN: 978-1-62708-170-2
... implantation and laser surface processing. Surface hardening techniques, namely, nitriding, carburizing, boriding, and flame hardening, performed to improve the resistance of stainless steel alloys are also reviewed. acid cleaning acid descaling alkaline cleaning boriding buffing carburizing...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003246
EISBN: 978-1-62708-199-3
... carbides, graphite, martensite, and a variety of intermetallic phases, nitrides, and nonmetallic inclusions. The article further describes the two-phase constituents including, tempered martensite, pearlite, and bainite and nonmetallic inclusions in steel that consist of two or more phases. common...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005955
EISBN: 978-1-62708-166-5
... and devices for measuring thermal and electrical conductivity. The article also describes the applications of the vacuum heat treating process, namely, vacuum nitriding and vacuum carburizing. Finally, it reviews the heat treating process of tool steels, stainless steels, Inconel 718, and titanium and...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005956
EISBN: 978-1-62708-166-5
... hardening. This article provides a model-based description of the development of residual stresses during case hardening. It also describes the influence and effects of residual stresses and distortion in hardening, carburizing, and nitriding processes of the steel. axial stress carbon content...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003821
EISBN: 978-1-62708-183-2
..., and corrosion by molten salts. Applications where the corrosion properties of nickel alloys are important factors in materials selection include the petroleum, chemical, and electrical power industries. Most nickel alloys are much more resistant than the stainless steels to reducing acids, such as...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003188
EISBN: 978-1-62708-199-3
... alloys cubic boron nitride cutting tool materials high-speed tool steels machining applications material grade selection polycrystalline diamond SELECTING THE PROPER CUTTING TOOL MATERIAL for a specific machining application can provide substantial advantages, including increased productivity...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001320
EISBN: 978-1-62708-170-2
... Abstract The classes of tool materials for machining operations are high-speed tool steels, carbides, cermets, ceramics, polycrystalline cubic boron nitrides, and polycrystalline diamonds. This article discusses the expanding role of surface engineering in increasing the manufacturing...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001231
EISBN: 978-1-62708-170-2
..., and it is generally true that today's precision engineering will be tomorrow's general engineering. At present, the highest spindle speeds in conventional lathes are 2200 to 2400 rpm. For precision finishing cuts on steel and materials with similar properties, the highest spindle speeds should range...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006787
EISBN: 978-1-62708-295-2
... the results obtained at 650 °C (1200 °F) ( Ref 77 ), where AISI 347 and 310 stainless steels, Incoloy 800H (IN-800H), and Inconel 625 (IN-625) were tested in eutectic 34.42wt%NaCl-65.58wt%LiCl under a nitrogen atmosphere. Table 3 lists the chemical compositions of the alloys tested. The high current...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001312
EISBN: 978-1-62708-170-2
..., silicon carbide, silica sand, and steel grit are satisfactory media for mechanical descaling. Periodic replacement of used media may be required to avoid excessive working of the surfaces by dull particulates. Roughening of exposed surface areas occurs from grit or shot impingement, depending on the grit...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003842
EISBN: 978-1-62708-183-2
... generally high stiffness and low density of ceramic materials also reduce dynamic forces in high-speed components such as bearing balls. Hybrid ceramic bearings using silicon nitride rolling elements and steel races are capable of significantly higher speeds than comparable all-steel bearings under oil...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003059
EISBN: 978-1-62708-200-6
... Abstract This article provides crystallographic and engineering data for single oxide ceramics, zirconia, silicates, mullite, spinels, perovskites, borides, carbides, silicon carbide, boron carbide, tungsten carbide, silicon-nitride ceramics, diamond, and graphite. It includes data on crystal...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003091
EISBN: 978-1-62708-199-3
... Abstract This article presents a detailed account on the process flow, composition, alternative sources, and the advancement of ironmaking, steelmaking and secondary steelmaking practices. Some steels, such as bearing steels, heat-resistant steels, ultrahigh strength missile and aircraft steels...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003114
EISBN: 978-1-62708-199-3
... Abstract This article discusses the characteristics, composition limits, and classification of wrought tool steels, namely high-speed steels, hot-work steels, cold-work steels, shock-resisting steels, low-alloy special-purpose steels, mold steels, water-hardening steels, powder metallurgy tool...