Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006140
EISBN: 978-1-62708-175-7
... Abstract Prealloyed (PA) powder metallurgy is a technique where complex near-net shape titanium aircraft components are fabricated with low buy-to-fly ratios. This article describes the physical principle, mechanism, and simulation and modeling of metal can and hot isostatic pressing (HIP...
Image
Published: 30 September 2015
Fig. 2 Near-net shape O-30-grade beryllium mirror blank segment processed by hot isostatic pressing for the James Webb Space Telescope More
Image
Published: 30 September 2015
Fig. 12 Near-net shape aluminum-beryllium blanks consolidated by hot isostatic pressing More
Image
Published: 30 September 2015
Fig. 5 Example of a Foaminal near-net shape part More
Image
Published: 01 January 2005
Fig. 23 Near-net-shape alloy 718 turbine disk produced by a multistep hot-die forging process More
Image
Published: 30 September 2015
Fig. 3 Near-net shape powder metallurgy titanium alloy parts produced by die pressing and sintering. (a) Ti-6Al-4V prototype connecting rod. (b) Ti-6Al-4V aircraft component part. (c) Commercially pure (CP) titanium washers. (d) Ti-6Al-4V washers. (e) Ti-3Al-2.5V collars. (f) Nuts. Source More
Image
Published: 30 September 2015
Fig. 9 Complex PM hot isostatic pressed, near net shape housings from Ti-6Al-4V More
Image
Published: 01 January 2005
Fig. 10 Yield strength as a function of near-net-shape die temperature for numerous nickel-base alloys and a molybdenum alloy (TZM) More
Image
Published: 01 January 2005
Fig. 11 100 h stress rupture strength as a function of near-net-shape die temperature for selected nickel-base alloys More
Image
Published: 01 January 2005
Fig. 22 Complex near-net-shape IN 100 turbine disk produced using a two-step isothermal forge process More
Image
Published: 30 November 2018
Fig. 9 Example of Foaminal near-net shape part and foaming mold More
Image
Published: 31 December 2017
Fig. 20 Schematic of LENS (laser engineered near-net shaping) process illustrating synthesis of laser-assisted coating where coating material is deposited together with the laser beam. Source: Ref 93 More