1-1 of 1 Search Results for

nadic end-capped amic acid oligomer resin

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003365
EISBN: 978-1-62708-195-5
.... The article reviews the chemistry of several addition-type polyimides, including phenylethynyl-containing imide oligomers, nadic end-capped polyimides, and LARC RP46. It explains the preparation processes of nadic end-capped amic acid oligomer resin solutions, including the preparation of resin powder...