1-20 of 359 Search Results for

nace

Sort by
Image
Published: 30 September 2015
Fig. 3 NACE International surface finish weld comparator More
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006024
EISBN: 978-1-62708-172-6
... of the Society for Protective Coatings' (SSPC) standards and NACE International standards as well as the International Organization for Standardization (ISO) standards and International Concrete Repair Institute (ICRI) guidelines for surface cleanliness. blast cleaning extraction grinding wheels...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004113
EISBN: 978-1-62708-184-9
.... These data are collected from predesign site assessments, tank electrical characteristics, and soil-resistivity measurements. The article addresses NACE Standard RP0169, which gives requirements and desired characteristics for coating in conjunction with CP. It also explains the methods of protecting...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003650
EISBN: 978-1-62708-182-5
.... The ASTM International and NACE International standards that are directly or indirectly applicable to simulated service corrosion testing in water are tabulated. The article also describes the effects of variable concentrations of dissolved carbonates, such as calcium, magnesium, and/or sodium, in water...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003653
EISBN: 978-1-62708-182-5
... process. Resistance and hydrogen probes monitor on-line corrosion in reactor cooling waters, oil pipelines, and refineries ( Ref 1 , 2 ). The location and monitoring of these probes are critical for obtaining meaningful data. NACE Standard, RP0189-95 discusses such methods for on- line monitoring...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003656
EISBN: 978-1-62708-182-5
... relative flow rates. Anode 0 and anode 1 are redundant, and zero resistance ammeter (ZRA) can be switched to either anode. Adapted from Ref 24 , with permission from the National Association of Corrosion Engineers (NACE) International This method has been tested for localized corrosion monitoring...
Image
Published: 01 January 2005
; NACE, NACE International; PWRI, Public Works Research Institute; JASPP, Japan Association for Steel Pipe Piles; JACC, Japan Association of Corrosion Control More
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003700
EISBN: 978-1-62708-182-5
... into the horizontal section of the overhead vapor line; however, many variations exist. Details of refinery inhibitor injections are difficult to generalize due to the uniqueness and variety of each situation. Numerous publications exist, including a NACE International Technical Committee Report that details...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004108
EISBN: 978-1-62708-184-9
... of organic coating systems. Surface cleanliness and proper surface profile are both important. Surface preparation frequently accounts for two-thirds of total painting costs for offshore structures. The Society for Protective Coatings (formerly the Steel Structures Painting Council, SSPC), NACE...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003608
EISBN: 978-1-62708-182-5
...,” Paper 592, presented at Corrosion/93 (Houston, TX), NACE International, Inc. , March 1993 2. Perry F.A. , “A Review of Stray Current Effects on a Gas Transmission Main in the Boston, Massachusetts Area,” Paper 590, presented at Corrosion/94 (Houston, TX), NACE International, Inc...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004134
EISBN: 978-1-62708-184-9
... in the spring. When thermal insulation is soaked, the pipes can suffer from corrosion under insulation ( Ref 15 , 16 ). The designer should specify immersion-service coatings for external piping surfaces used in underground utilidors to limit these effects, in accordance with NACE International recommended...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003637
EISBN: 978-1-62708-182-5
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003694
EISBN: 978-1-62708-182-5
..., and mill scale. NACE International and the former Steel Structures Painting Council (SSPC) have jointly issued a series of surface preparation standards that are used widely throughout North America. The SSPC is now known as SSPC: The Society for Protective Coatings. Similar standards issued...
Image
Published: 01 January 2003
Fig. 3 Calcareous deposits in the tidal region of an offshore platform. Courtesy of NACE International More
Image
Published: 01 January 2003
Fig. 4 Schematic diagram of a coupled multielectrode system for localized corrosion studies. Source: Ref 33 , with permission from NACE International More
Image
Published: 01 January 2003
Fig. 5 Schematic diagram of a coupled multielectrode array sensor for localized corrosion. Adapted from Ref 38 , with permission from NACE International More
Image
Published: 15 January 2021
Fig. 13 Deep caustic gouging beneath heavy insulating deposits. Steam forming under the insulating deposit escapes and concentrates caustic capable of dissolving metal. Courtesy of NACE International More
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003714
EISBN: 978-1-62708-182-5
... of Electrochemistry) www.ise-online.org/ Japanese Society of Corrosion Engineering www.jcorr.or.jp/ Korean Institute of Metals and Materials www.kim.or.kr/ Materials Research Society www.mrs.org/ Mexican Society of Electrochemistry (SMEQ) www.sm-electroquimica.org NACE International www.nace.org...
Image
Published: 15 January 2021
Fig. 8 Increase in corrosion rate for steel treated with a corrosion inhibitor in carbon-dioxide-saturated 3% saline solution with addition of acetate. Source: Ref 52 . Reprinted with permission from NACE International More
Image
Published: 01 January 2003
Fig. 2 Crevice cell system. (a) Cross section of crevice assembly. (b) Schematic diagram of crevice assemblies galvanically coupled to stainless steel (SS) cathode. Source: Ref 27 , with permission from NACE International More