1-20 of 31 Search Results for

multidisciplinary optimization

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002446
EISBN: 978-1-62708-194-8
... and provides some background on how these algorithms make decisions when searching for the optimal design. It also provides information on structural optimization, topology optimization, materials processing optimization, multidisciplinary optimization, and global optimization. design optimization...
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005534
EISBN: 978-1-62708-197-9
... , Science , Vol 288 ( No. 5468 ), 1997 , p 993 – 998 3. Koch P.N. , Simpson T.W. , Allen J.K. , and Mistree F. , Statistical Approximations for Multidisciplinary Optimization: The Problem of Size , J. Aircraft , Vol 36 ( No. 1 ), 1999 , p 275 – 286 10.2514/2.2435 4...
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005505
EISBN: 978-1-62708-197-9
... P.N. , McMillan M. , and Chiang W.-S. , “A Distributed, Component-Based Integration Environment for Multidisciplinary Optimal and Quality Design,” AIAA-2002-5476, Ninth AIAA/ISSMO Symposium on Multidisciplinary Analysis and Optimization ( Atlanta, GA ) 4. Runyan J...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003971
EISBN: 978-1-62708-185-6
.... Srivatsa S.K. , Application of Multidisciplinary Optimization (MDO) Techniques to the Manufacture of Aircraft-Engine Components , Handbook of Workability and Process Design , Dieter G.E. , Kuhn H.A. , and Semiatin S.L. , Ed., ASM International , 2003 , Chap. 24 Metalworking...
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005513
EISBN: 978-1-62708-197-9
... optimization: This blends computational mechanics with multidisciplinary optimization to emulate the essence of in situ process control in the computer. It is ex situ because it must be performed in advance of the deposition due to its computational needs. The “measurements” are data in the thermomechanics...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002457
EISBN: 978-1-62708-194-8
... the viewpoint of the user (customer). Value analysis is applied to problems as diverse as automobile engines and gall bladder operations. It works whenever a product or process performs a function and costs money. While the method is often used to improve on present products, its greatest power is in optimizing...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003087
EISBN: 978-1-62708-199-3
... and more companies are forming multidisciplinary project teams to ensure that all needed input is obtained concurrently. This is reflected by the increasing use of “concurrent” or “simultaneous” engineering methods ( Ref 6 , 7 ). Thus material and process selection is a progressive process...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002443
EISBN: 978-1-62708-194-8
... as needed. The ability to model subtle changes in geometry permits the optimization of size, shape, or form to obtain minimum weight or maximum performance. Table 1 summarizes the many engineering problems addressed by the finite element method. Because the method was originally developed...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005425
EISBN: 978-1-62708-196-2
... is effective and is readily used for metallurgical understanding of tensile property control and optimization ( Ref 15 ). However, the grain size is not the only microstructural feature that can influence the yield strength. Additional models are required to describe contributions from solid-solution...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002379
EISBN: 978-1-62708-193-1
... mechanics is a multidisciplinary engineering topic that has foundations in both mechanics and materials science. This article summarizes the microstructural aspect of fracture resistance in structural materials. It provides a discussion on basic fracture principles and schematically illustrates...
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005528
EISBN: 978-1-62708-197-9
...)90006-6 33. Oyane M. , Criteria of Ductile Fracture Strain , Jpn. Soc. Mech. Eng. , Vol 15 ( No. 90 ), 1972 , p 1507 – 1513 34. Kubli W. , Maurer M. , and Reissner J. , The Use of FE Process Simulation in Tool and Machine Optimization of the Fine Blanking...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006465
EISBN: 978-1-62708-190-0
... conditions and methods, robust enough to be predictive, and accessible enough to be applicable ( Ref 15 ). This is an enormous task and an area of active multidisciplinary research ( Ref 8 ). At this point, the uncertainty and variability, even from machine to machine, prohibits broad application to critical...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.9781627081948
EISBN: 978-1-62708-194-8
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006753
EISBN: 978-1-62708-295-2
... and other life-prolonging activities can be optimized. Diligence in Use of Terminology Communicating technical information accurately is of paramount importance in all engineering areas, including failure analysis. The choice of technical descriptors, nomenclature, and even what may be considered...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003500
EISBN: 978-1-62708-180-1
... life-prolonging activities can be optimized. Diligence in Use of Terminology Communicating technical information is of paramount importance in all engineering areas, including failure analysis. The choice of technical descriptors, nomenclature, and even what might be considered technical jargon...
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005530
EISBN: 978-1-62708-197-9
...-24112 05-39) 109. Röhl P.J. , He B. , and Finningan P. , “A Collaborative Optimization Environment for Turbine Engine Development,” American Institute of Aeronautics and Astronautics Paper AIAA-1998-4734, Seventh AIAA/USAF/NASA/ISOO Symposium on Multidisciplinary Analysis...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.9781627081863
EISBN: 978-1-62708-186-3
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005636
EISBN: 978-1-62708-174-0
... Parameter Estimation , Academic Press , New York , 1974 124. Dennis J. and Schnabel R. , Numerical Methods for Unconstrained Optimizations and Non-Linear Equations , Prentice Hall , 1983 125. Tikhonov N. , Soviet Math. Dokl. , Vol 4 , 1963 , p 1035 – 1038 126...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005426
EISBN: 978-1-62708-196-2
... A. and Lam J. , Role of CFD in Analysis and Optimization of the Continuous Casting Processes , First MIT Conference on Computational Fluid and Solid Mechanics , June 12–15, 2001 ( Cambridge, MA ), 2001 , p 912 – 916 66. Ha J. , Cleary P. , Alguine V. , and Nguyen T...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006370
EISBN: 978-1-62708-192-4
... model wear tool material die material METAL FORMING TRIBOLOGY is a multidisciplinary topic, generally involving solid mechanics, fluid mechanics, heat transfer, chemistry, and materials science. Metal forming presents extremely demanding applications of tribology. Elevated temperatures, high...