1-20 of 80 Search Results for

movable furnaces

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005198
EISBN: 978-1-62708-187-0
... Abstract This article discusses the design parameters, operation, characteristics, properties, and advantages of various types of crucible furnaces, such as stationary, tilting, and movable furnaces. It also provides information on the application of the crucible furnaces. crucible...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006075
EISBN: 978-1-62708-175-7
... powders and the safe operation of continuous mesh belt sintering furnaces with combustible atmospheres. It also provides a comprehensive high-level overview of the safety-related issues and concerns related to the use of compacting presses in the manufacturing sector. compacting presses continuous...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005806
EISBN: 978-1-62708-165-8
... nitrocarburizing and austenitic nitrocarburizing. The article includes a discussion on the difficulties in specimen cleaning, importance of furnace purge, uses of pre and post oxidation, depassivation, or activation, and requirements for perfect nucleation in nitriding process. In nitriding, the successful...
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005199
EISBN: 978-1-62708-187-0
... or secondary steelmaking. The two most important primary steelmaking processes are the electric arc furnace (EAF) process and the basic oxygen furnace (BOF) process or Linz-Donawitz process. The EAF process has been increasingly used, gradually overtaking the BOF as the primary steelmaking furnace...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005957
EISBN: 978-1-62708-166-5
.... An overhead crane moves the load to and from the car bottom. The car furnace also is called a bogie hearth. The bottom (floor) of the furnace is constructed as an insulated movable car that is moved out of the furnace for loading and unloading. Car bottom furnaces can take days to complete a single load cycle...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003197
EISBN: 978-1-62708-199-3
... carburizing, commercially the most important variant of carburizing, the source of carbon is a carbon-rich furnace atmosphere produced either from gaseous hydrocarbons—for example, methane (CH 4 ), propane (C 3 H 3 ), and butane (C 4 H 10 )—or from vaporized hydrocarbon liquids. Carbon Sources Low...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005955
EISBN: 978-1-62708-166-5
..., and pusher-type systems have been adapted for transferring work loads inside these furnaces. For example, the hearth may be supported on wheels that are protected by movable heat baffles and that roll on rails installed below and outside the heated zone. The longitudinal motion may be supplied by a sealed...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006513
EISBN: 978-1-62708-207-5
... component design requires multiple cores, movable mold components, or complicated inner cavities and undercuts. Sand cores become necessary when the design prohibits drawing the core after the casting solidifies. When sand cores replace part of the metal mold, the process is called “semipermanent mold...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003199
EISBN: 978-1-62708-199-3
... Abstract Control of temperature and furnace atmospheres has become increasingly critical to successful heat treating. Temperature instrumentation and control systems used in heat treating include temperature sensors, controllers, final control elements, measurement instruments, and set-point...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006525
EISBN: 978-1-62708-207-5
... furnaces, transfer systems, and, by inclusion, the quality of the castings produced. Die casters are familiar with composition limits that prevent sludge formation. A common rule is: (Eq 2) Fe + 2 Mn + 3 Cr ≤ 1.7 This limit is arbitrary and inexact, it is often assigned values from 1.5...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003980
EISBN: 978-1-62708-185-6
... . The stock is positioned in the first (topmost) station of the stationary die of the machine. During the upset forging cycle, the movable die slides against the stationary die to grip the stock. The header tool, fastened in the header slide, advances toward and against the forging stock to spread...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005288
EISBN: 978-1-62708-187-0
... the complete process of melting, alloying, holding, and casting takes place in one self-contained furnace ( Ref 1 ). The Unicast furnace differs from the modern version only in that refractory brick insulation is used hout instead of low-thermal-mass insulation. The integrated melting, homogenizing...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005615
EISBN: 978-1-62708-174-0
... short, thus allowing the work to remain at the sufficient preheat temperature. Selection of heating method depends on the size and shape of the work and the preheat temperature; a combination of methods can be used. Torch and furnace heating are widely used; induction and infrared-radiation heating...
Book Chapter

Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005115
EISBN: 978-1-62708-186-3
... or on the bolster plate of a press, they can also be attached to the feed vertically, sideways, or upside-down. One common application is to mount two feeds on one die or special machine and process and assemble two different parts. Consider also the possibility of mounting an air feed on a movable platform...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005926
EISBN: 978-1-62708-166-5
... Abstract This article provides a detailed discussion on the types of furnace atmospheres required for heat treating. These include generated exothermic-based atmospheres, generated endothermic-based atmospheres, generated exothermic-endothermic-based atmospheres, generated dissociated-ammonia...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005928
EISBN: 978-1-62708-166-5
... Abstract The atmosphere within a furnace chamber is a basic factor in achieving the desired chemical reactions with metals during heat treating. This article presents the fundamentals of heat treating atmospheres, and describes two groups of atmosphere control, namely, furnace atmosphere...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006330
EISBN: 978-1-62708-179-5
... with a furnace. It provides a discussion on the dilatometer analysis that is generally used to measure linear displacement as a function of temperature for all types of materials, and the problems associated with volume-change measurements. The article presents a graphical representation of a consequence...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005904
EISBN: 978-1-62708-167-2
.... Extraction of Fumes A movable exhaust hood, in which the furnace cover is integrated, is installed on the furnace platform to extract fumes. These have meanwhile been developed to such an extent that they properly capture fumes in every operating state, namely during charging and melting, during holding...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003996
EISBN: 978-1-62708-185-6
... have programmable press operation, press load and operation monitoring and control, and press energy and press operation control systems. These systems, combined with automated handling and supporting equipment, such as reheat furnaces and trim presses, can be used to achieve full forging process...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003091
EISBN: 978-1-62708-199-3
... using movable throat armors are some of the developments in charged material management. High hot-blast temperatures of 1250 °C (2280 °F) are now commonly used in several blast furnaces around the world, which has a direct bearing on the coke rate of the furnace. The ability to use high blast...