..., University of Missouri Research Reactor A.D. Krawitz, Department of Mechanical and Aerospace Engineering, University of Missouri~olumbia General Uses Size: 1 to 10 cm3 for powder structure determination, single crystals of 0.5 to several Determination of atomic arrangements (for hundred mm 3. Law...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002349
EISBN: 978-1-62708-193-1
..., University of Missouri-Columbia, Columbia, MO, 1986 26. Bouse G.K. , Bernstein I.M. , and Stone D.H. , Role of Alloying and Microstructure on the Strength and Toughness of Experimental Rail Steels , in STP 644, ASTM , 1978 , p 145 – 161 27. Fowler G.J. and Tetelman...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006562
EISBN: 978-1-62708-290-7
Series: ASM Handbook
Volume: 24A
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.hb.v24A.a0006973
EISBN: 978-1-62708-439-0
Image
Published: 01 December 2008
Fig. 4 Completed expanded polystyrene pattern assemblies ready for ceramic coating. Courtesy of Missouri Precision Castings More
Image
Published: 01 December 2008
drive sprocket for armored personnel carrier. The part is 510 mm (20 in.) in outside diameter, 114 mm (4 1 2 in.) thick, and weighs 28 kg (62 lb). Sprocket teeth are used as-cast, resulting in a significant savings in machining costs. Courtesy of Missouri Precision Castings More
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005256
EISBN: 978-1-62708-187-0
... in.) in outside diameter, 114 mm (4 1 2 in.) thick, and weighs 28 kg (62 lb). Sprocket teeth are used as-cast, resulting in a significant savings in machining costs. Courtesy of Missouri Precision Castings Process Details The Replicast process has two variations: Replicast FM (full mold...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005302
EISBN: 978-1-62708-187-0
... Specialty Company in Missouri, where foundry trials confirmed that aluminum-boron master alloys were good refiners. However, the added boron reacted with dissolved titanium to produce a sludge in holding furnaces. Also, boron apparently reacted with strontium, since boron additions resulted in a loss...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001078
EISBN: 978-1-62708-162-7
.... (g) By agreement between the purchaser and the supplier, bismuth levels up to 0.150% may be allowed. (h) Arsenic, antimony, and tin each at 0.001% max. (i) Chemical lead designates the undesilverized lead produced from southeastern Missouri ores. (j) Copper-bearing lead is made by adding...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006272
EISBN: 978-1-62708-169-6
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003502
EISBN: 978-1-62708-180-1
... involve the interaction of various materials in an assembly or with the environment. An articulated tractor and low-loading trailer was being driven through some hilly country in Missouri after delivery of a bulldozer to a construction site. The driver noticed that his rear trailer brakes had started...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003146
EISBN: 978-1-62708-199-3
... of southeastern Missouri, which contain small amounts of copper and silver. The copper content significantly improves corrosion resistance and mechanical strength, making chemical lead the next most frequently used grade after corroding lead. The silver content also improves corrosion resistance in some...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005186
EISBN: 978-1-62708-187-0
... centrifugal casting to remove gases and was the first to pour two or more metals into a single rotating mold. The centrifugal casting of steel was first attempted in 1898 at the plant of the American Steel Foundries in St. Louis, Missouri. Railroad car wheels were spun cast in 1901 at a rotation speed of 620...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005978
EISBN: 978-1-62708-168-9
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006814
EISBN: 978-1-62708-329-4
..., in general, are associated with many failures. Notable failures involving connections include riveted connections (the molasses spill in Boston, 1919), eye-bar connections (the Silver Bridge in West Virginia, 1967), bolted connections (Kemper Arena in Missouri, 1979), O-ring joints (the Challenger explosion...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002463
EISBN: 978-1-62708-194-8
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002403
EISBN: 978-1-62708-193-1
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006287
EISBN: 978-1-62708-169-6
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006509
EISBN: 978-1-62708-207-5
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006524
EISBN: 978-1-62708-207-5