1-20 of 1210

Search Results for mill products

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

By Jack W. Bray
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001059
EISBN: 978-1-62708-162-7
... Abstract Aluminum mill products are those that have been subjected to plastic deformation by hot- and cold-working mill processes such as rolling, extruding, and drawing, either singly or in combination. Microstructural changes associated with the working and with any accompanying thermal...
Image
Published: 30 November 2018
Fig. 2 Flow chart for an aluminum rolling-mill production line More
Book Chapter

By S. Lampman
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001081
EISBN: 978-1-62708-162-7
... Abstract This article discusses the wrought product forms of titanium and titanium-base alloys, which include forgings and the typical mill products with tabulations for various specifications, and compares specifications for pure titanium, titanium alloys for mechanical, physical properties...
Book Chapter

By D.U. Furrer, S.L. Semiatin
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003999
EISBN: 978-1-62708-185-6
... Abstract Forging of nickel-base alloys results in geometries that reduce the amount of machining to obtain final component shapes and involves deformation processing to refine the grain structure of components or mill products. This article discusses the heating practice, die materials...
Book Chapter

Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002140
EISBN: 978-1-62708-188-7
... Abstract Thread milling is a method of cutting screw threads with a milling cutter in a thread mill. This article discusses the operational procedures of thread milling machines, namely, universal thread mills, production thread mills, planetary thread mills, and numerical control machines...
Book Chapter

By Rodney R. Boyer
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003141
EISBN: 978-1-62708-199-3
..., including all operations that convert ingot into general mill products, such as billet, bar, plate, sheet, strip, tube, and wire. The section on secondary fabrication describes processes such as die forging, extrusion, hot and cold forming, machining, chemical milling, and joining. The article presents...
Book Chapter

By Derek E. Tyler
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001066
EISBN: 978-1-62708-162-7
... Abstract Wrought copper and copper alloys are produced in various mill-product forms for a variety of applications due to their high electrical conductivity, corrosion resistance, ease of fabrication, and good heat-transfer properties. This article describes the manufacturing processes used...
Book Chapter

Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006708
EISBN: 978-1-62708-210-5
... Abstract The 6xxx series aluminum alloys are used across end applications including all forms of transportation, electronics, and building and construction. This article contains tables that list standard specifications for 6xxx series aluminum alloys and select specialty mill products...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003125
EISBN: 978-1-62708-199-3
... shapes; forgings; and impacts. The article provides information on product economics, design and selection, including product dimension and dimension tolerances, and design and use of wrought product capabilities. Finally, it tabulates the specifications and standards for aluminum mill products...
Book Chapter

By Jay W. Larson
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003804
EISBN: 978-1-62708-183-2
..., and agriculture. These products include bars, rods, wires, hot and cold rolled sheets, strip plates, tin mill products, steel tubes, castings, and forgings. The article also provides information on the methods used to prevent or control the rusting of ferrous materials, namely, alloying, coating, and covering...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001103
EISBN: 978-1-62708-162-7
..., including consolidation, hot rolling, heat treating, and the fabrication of mill products. It also discusses the nominal composition and microstructure of commercial ODS alloys, including nickel, iron, and aluminum-base systems, and provides detailed information on their mechanical, physical, oxidation...
Book Chapter

Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006598
EISBN: 978-1-62708-210-5
... Abstract This datasheet provides information on key alloy metallurgy, mill product specifications, processing effects on physical and mechanical properties, and applications of high-strength aerospace alloys 2024 and Alclad 2024. It contains tables that list values of tensile property limits...
Book Chapter

Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006596
EISBN: 978-1-62708-210-5
... Abstract This datasheet provides information on key alloy metallurgy, fabrication characteristics, mill-product specifications, processing effects on physical properties, and applications of high-strength alloy 2014. It contains tables that list values of tensile property limits for alloy 2014...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006695
EISBN: 978-1-62708-210-5
... Abstract This datasheet provides information on composition limits, mill product specifications, fabrication characteristics, processing effects on physical and mechanical properties, and applications of packaging and general-construction alloys 5052 and 5252. aluminum alloy 5052...
Book Chapter

Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006693
EISBN: 978-1-62708-210-5
... Abstract Alloy 5005, available as architectural sheet and components, was introduced in 1935 to fill the need of the mobile-home industry for a lightweight, inexpensive, workable, corrosion-resistant siding material. This datasheet provides information on composition limits, mill product...
Image
Published: 30 September 2015
Fig. 17 Pilot- and production-sized vibratory mills More
Image
Published: 01 January 1989
Fig. 15 Common forms of production milling operations More
Book Chapter

Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005125
EISBN: 978-1-62708-186-3
... Abstract This article discusses the mill products most often formed by the three-roll forming process. It schematically illustrates some of the shapes commonly produced from flat stock by the three-roll forming process. The article describes the two basic types of three-roll forming machines...
Book Chapter

By Howard A. Kuhn
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003269
EISBN: 978-1-62708-176-4
... Abstract This article reviews the common methods of shear and multiaxial testing for the evaluation of engineering components such as fasteners and mill products. It discusses shear test methods, including through-thickness tests, in-plane shear tests, and double-notched shear test. The article...
Book Chapter

Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006703
EISBN: 978-1-62708-210-5
... Abstract This datasheet provides information on composition limits, mill product specifications, fabrication characteristics, processing effects on physical and mechanical properties, and applications of high-strength Al-Mg-Mn-Cr alloy 5456. aluminum alloy 5456 aluminum mill products...