1-5 of 5 Search Results for

microregions

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003769
EISBN: 978-1-62708-177-1
... transformations. The article also describes specimen preparation procedures and examines the microstructure of several alloy samples. aluminum alloys macroexamination metallography microregions microstructure microstructure examination specimen preparation ALUMINUM ALLOYS encompass a wide range...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003765
EISBN: 978-1-62708-177-1
... with steadite, are white, while their interiors are almost black due to overetching the pearlitic-ferritic matrix. Figure 19 shows the same microstructure after etching with Klemm's I reagent. The microregions inside the eutectic cells with a lower phosphorus content are tinted a blue color, while the areas...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006342
EISBN: 978-1-62708-179-5
.... The cell boundaries, filled with steadite, are white, while their interiors are almost black due to overetching the pearlitic-ferritic matrix. Figure 23 shows the same microstructure after etching with Klemm’s I reagent. The microregions inside the eutectic cells with a lower phosphorus content...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006559
EISBN: 978-1-62708-290-7
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005950
EISBN: 978-1-62708-166-5
... there are a few studies that demonstrate the necessity of bidirectional coupling. Phase transformations alter the mechanical field due to transformation strains. During a phase transformation, a transforming microregion changes its volume and occasionally...