Published: 01 January 2006
Fig. 2 Selected scanning electron micrography (SEM) micrographs of retrieved modular connections from different orthopedic implants showing evidence of corrosion attack. (a) SEM of head taper near the free surface (top). Note the machining lines at the top near the exterior of the device More
Image
Published: 01 December 2004
Fig. 24 Scanning electron micrography image of aluminum dendrites in the fractured surface of a tensile test bar of an A356.0 alloy More
Image
Published: 01 June 2012
Fig. 2 Selected scanning electron micrography (SEM) micrographs of retrieved modular connections from different orthopaedic implants showing evidence of corrosion attack. (a) SEM of head taper near the free surface (top). Note the machining lines at the top near the exterior of the device More
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009076
EISBN: 978-1-62708-177-1
... is ready to be analyzed by microscopy techniques. Standard texts on microscopy should be consulted to obtain and interpret the images recorded by micrography ( Ref 5 , 6 , 7 , 8 , 9 , 10 , 11 , 12 ). Changes in heat and the type of stress the material has seen in use or during testing may...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003727
EISBN: 978-1-62708-177-1
... in Fig. 24 . Fig. 23 Typical dendrites in an A356 alloy in a computer-processed image. Etchant: modified Poulton reagent (60% HCl, 30% HNO 3 , 5% HF, 5% H 2 O) Fig. 24 Scanning electron micrography image of aluminum dendrites in the fractured surface of a tensile test bar of an A356.0...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005653
EISBN: 978-1-62708-198-6
... heads ( Ref 30 , 33 ). Fig. 2 Selected scanning electron micrography (SEM) micrographs of retrieved modular connections from different orthopaedic implants showing evidence of corrosion attack. (a) SEM of head taper near the free surface (top). Note the machining lines at the top near...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004206
EISBN: 978-1-62708-184-9
... Selected scanning electron micrography (SEM) micrographs of retrieved modular connections from different orthopedic implants showing evidence of corrosion attack. (a) SEM of head taper near the free surface (top). Note the machining lines at the top near the exterior of the device and the corrosion evident...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006940
EISBN: 978-1-62708-395-9
... interference measurements ( Ref 81 ), it is inferred that a crack initiates and propagates in glassy polymers under certain conditions through a single craze. Optical micrography, on the other hand, shows that a few ( Ref 3 ) or myriad ( Ref 82 ) crazes precede FCI. The common denominator in each...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003752
EISBN: 978-1-62708-177-1