Skip Nav Destination
Close Modal
Search Results for
metallurgical control
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 1294
Search Results for metallurgical control
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006310
EISBN: 978-1-62708-179-5
... structure with freedom from carbides. The article describes the methods of magnesium treatment, control of magnesium content, and inoculation. It concludes with a discussion on the metallurgical controls of ductile iron production. carbides ductile iron ductile iron castings ductile metallic matrix...
Abstract
Unlike gray iron, which contains graphite flakes, ductile iron has an as-cast structure containing graphite particles in the form of small, rounded, spheroidal nodules in a ductile metallic matrix. This article discusses the raw materials that are used for ductile iron production and outlines the most common and important requirements for controlling the composition of ductile iron. Treatment to produce ductile iron involves the addition of magnesium to change the form of the graphite, followed by or combined with inoculation of a silicon-containing material to ensure a graphitic structure with freedom from carbides. The article describes the methods of magnesium treatment, control of magnesium content, and inoculation. It concludes with a discussion on the metallurgical controls of ductile iron production.
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001003
EISBN: 978-1-62708-161-0
... Abstract This article discusses the compositions, properties, and typical applications for ductile irons that are defined by U.S. and international standards . It describes the various methods used to test and inspect the metallurgical control processes in ductile iron production. The article...
Abstract
This article discusses the compositions, properties, and typical applications for ductile irons that are defined by U.S. and international standards . It describes the various methods used to test and inspect the metallurgical control processes in ductile iron production. The article discusses the effect of composition, graphite shape, and section size on the properties of ductile iron. The article also describes the mechanical properties of ductile iron at elevated temperatures. The heat treatment of ductile iron castings produces a significant difference in mechanical properties from as-cast ductile iron. A ductile iron generally has higher hardenability than a eutectoid steel with comparable alloy content. The article also discusses the physical properties of ductile iron, including density, thermal conductivity, electrical conductivity, electrical resistivity, and magnetic properties. Ductile iron has been chosen in many instances on the basis of significantly lower machining costs, which resulted in lower overall cost of the part.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003110
EISBN: 978-1-62708-199-3
... Abstract Malleable iron is a type of cast iron that has most of its carbon in the form of irregularly shaped graphite nodules. This article tabulates the typical composition of malleable iron and specifications, and applications of malleable iron castings. It discusses the metallurgical control...
Abstract
Malleable iron is a type of cast iron that has most of its carbon in the form of irregularly shaped graphite nodules. This article tabulates the typical composition of malleable iron and specifications, and applications of malleable iron castings. It discusses the metallurgical control of malleable irons with emphasis on its composition and heat treatment. The article provides information on the specifications and mechanical properties of different types of malleable irons, such as ferritic, pearlitic, and martensitic malleable irons.
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003995
EISBN: 978-1-62708-185-6
... on the key stages of deformation, and the required metallurgical information at each of these stages. austenite steel controlled rolling conventional hot rolling deformation ferrous alloys grain refinement high strength low alloy steel hot working hot-rolled steel metal forming microalloy...
Abstract
Thermomechanical processing (TMP) refers to various metal forming processes that involve careful control of thermal and deformation conditions to achieve products with required shape specifications and good properties. This article describes TMP methods in producing hot-rolled steel and reviews how improvements in the strength and toughness depend on the synergistic effect of microalloy additions and on carefully controlled thermomechanical conditions. It discusses TMP variables and the general distinctions between conventional hot rolling and common types of controlled-rolling schedules. The article describes the metallurgical processes in grain refinement of austenite steel by hot working, such as recovery and recrystallization and strain-induced transformation. The grain refinement in high strength low alloy steel by alloy addition is also discussed. The article provides an outline on the key stages of deformation, and the required metallurgical information at each of these stages.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003108
EISBN: 978-1-62708-199-3
... Abstract This article provides information on the general characteristics, composition, uses, applications and specifications for standard grades of ductile iron. It describes the manufacturing and metallurgical process control procedures, including testing and inspection, and heat treatment...
Abstract
This article provides information on the general characteristics, composition, uses, applications and specifications for standard grades of ductile iron. It describes the manufacturing and metallurgical process control procedures, including testing and inspection, and heat treatment. The article also talks about the effects of composition, graphite shape, and section size on the mechanical properties of ductile iron. Tables and graphs provide helpful information on the tensile properties, compressive properties, torsional properties, damping capacity, impact properties, fracture toughness, fatigue strength, and elevated-temperature properties of ductile iron.
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005925
EISBN: 978-1-62708-166-5
... Abstract Temperature control in heat treating is of paramount importance in maintaining the quality and achieving the desired metallurgical results. This article provides a detailed account of the factors affecting temperature control in heat treating furnaces, with information on temperature...
Abstract
Temperature control in heat treating is of paramount importance in maintaining the quality and achieving the desired metallurgical results. This article provides a detailed account of the factors affecting temperature control in heat treating furnaces, with information on temperature control systems, including contact sensors, noncontact sensors, controllers, energy-flow regulators, measurement instruments, and set-point programmers. Common contact sensors include temperature scales, thermocouples, and resistance temperature detectors, whereas optical pyrometers and on-line radiation thermometers fall under the noncontact type. The article describes two types of instrumentation used in heat treating: field test instruments for temperature-uniformity surveys and system-accuracy tests; and controlling, monitoring, and recording instruments for digital instrumentation.
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005903
EISBN: 978-1-62708-167-2
... Abstract Interplays of metallurgical factors, such as dissolved oxygen, carbon, and silicon content, that control the molten metal from melting to pouring, have a decisive influence on the quality of the castings. This article focuses on the magnesium treatment and desulfurization carried out...
Abstract
Interplays of metallurgical factors, such as dissolved oxygen, carbon, and silicon content, that control the molten metal from melting to pouring, have a decisive influence on the quality of the castings. This article focuses on the magnesium treatment and desulfurization carried out during inoculation and nucleation of molten cast iron, assisting in the formation of cast iron. The different types of cast irons are gray cast iron, nodular cast iron, compacted graphite iron, malleable cast iron, and alloyed cast iron. The article provides an overview of the melt treatment processes carried out in cast steel, wrought and cast aluminum, and copper materials.
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001034
EISBN: 978-1-62708-161-0
... Abstract This article aims to survey the factors controlling the weldability of carbon and low-alloy steels in arc welding. It discusses the influence of operational parameters, thermal cycles, and metallurgical factors on weld metal transformations and the susceptibility to hot and cold...
Abstract
This article aims to survey the factors controlling the weldability of carbon and low-alloy steels in arc welding. It discusses the influence of operational parameters, thermal cycles, and metallurgical factors on weld metal transformations and the susceptibility to hot and cold cracking. The article addresses the basic principles that affect the weldability of carbon and low-alloy steels. It outlines the characteristic features of welds and the metallurgical factors that affect weldability. It describes the common tests to determine steel weldability. There are various types of tests for determining the susceptibility of the weld joint to different types of cracking during fabrication, including restraint tests, externally loaded tests, underbead cracking tests, and lamellar tearing tests. Weldability tests are conducted to provide information on the service and performance of welds. The major tests that are discussed in this article are weld tension test, bend test, the drop-weight test, the Charpy V-notch test, the crack tip opening displacement test, and stress-corrosion cracking test.
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006838
EISBN: 978-1-62708-329-4
... and fabrication sources of failure, addresses the key factors in production and quality control, and explains failure analysis of AM parts. binder jet sintering directed energy deposition failure analysis metal products metallurgical characteristics powder bed fusion quality assurance ADDITIVE...
Abstract
This article provides an overview of metal additive manufacturing (AM) processes and describes sources of failures in metal AM parts. It focuses on metal AM product failures and potential solutions related to design considerations, metallurgical characteristics, production considerations, and quality assurance. The emphasis is on the design and metallurgical aspects for the two main types of metal AM processes: powder-bed fusion (PBF) and directed-energy deposition (DED). The article also describes the processes involved in binder jet sintering, provides information on the design and fabrication sources of failure, addresses the key factors in production and quality control, and explains failure analysis of AM parts.
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001021
EISBN: 978-1-62708-161-0
... requirements for metallurgical integrity, mechanical properties, and dimensional accuracy. It can also provide for identification and certification of the forging so that it can be traced throughout processing and in service. Responsibility for material control is subject to agreement between the purchaser...
Abstract
Forgings are classified in various ways, beginning with the general classifications open die and closed die. They are also classified according to how they are made; such as hammer upset forgings, ring-rolled forgings, and multiple-ram press forgings; and in terms of the close-to-finish factor or amount of stock that must be removed to satisfy the dimensional and detail requirements of the finished part. In addition to types and classifications, the article discusses critical design factors and ways to ensure that the resulting forgings measure up to metallurgical, mechanical property, and dimensional accuracy requirements. The responsibility for design verification is vested in material control, which depends on the proper application of drawings, specifications, manufacturing process controls, and quality assurance programs. The article addresses each of these areas as well as related topics; including stress-induced fatigue failure, tolerances, machining allowances; and the fundamentals of hammer and press forgings, hot upset forgings, and hot extrusion forgings.
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006286
EISBN: 978-1-62708-169-6
... Abstract Quenching is a widely used technique to strengthen titanium alloys. This article presents the metallurgical and structural background underlying the specific techniques applied in the quenching of various titanium alloys, and the ways to control and reduce residual stresses induced...
Abstract
Quenching is a widely used technique to strengthen titanium alloys. This article presents the metallurgical and structural background underlying the specific techniques applied in the quenching of various titanium alloys, and the ways to control and reduce residual stresses induced from quenching or other thermal or mechanical processes. It discusses the types and microstructures of titanium alloys, namely, alpha, alpha-beta, and beta alloys, and describes the general effects of the various heat treatments. The article provides information on quenching media, quenching rate, section size, and martensitic transformation in quenched titanium alloys. It shows how residual stresses in titanium alloys are evaluated and controlled. Finally, the article describes the stress-relief treatments used to reduce residual stresses.
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005967
EISBN: 978-1-62708-166-5
... Abstract Of the various thermal processing methods for steel, heat treating has the greatest overall impact on control of residual stress and on dimensional control. This article provides an overview of the effects of material- and process-related parameters on the various types of failures...
Abstract
Of the various thermal processing methods for steel, heat treating has the greatest overall impact on control of residual stress and on dimensional control. This article provides an overview of the effects of material- and process-related parameters on the various types of failures observed during and after heat treating of quenched and tempered steels. It describes phase transformations of steels during heating, cooling of steel with and without metallurgical transformation, and the formation of high-temperature transformation products on the surface of a carburized part. The article illustrates the use of carbon restoration on decarburized spring steels. Different geometric models for carbide formation are shown schematically. The article also describes the different microstructural features such as grain size, microcracks, microsegregation, and banding.
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003510
EISBN: 978-1-62708-180-1
... Abstract This article provides an overview of the effects of various material- and process-related parameters on residual stress, distortion control, cracking, and microstructure/property relationships as they relate to various types of failure. It discusses phase transformations that occur...
Abstract
This article provides an overview of the effects of various material- and process-related parameters on residual stress, distortion control, cracking, and microstructure/property relationships as they relate to various types of failure. It discusses phase transformations that occur during heat treating and describes the metallurgical sources of stress and distortion during heating and cooling. The article summarizes the effect of materials and the quench-process design on distortion and cracking and details the effect of cooling characteristics on residual stress and distortion. It also provides information on the methods of minimizing distortion and tempering. The article concludes with a discussion on the effect of heat treatment processes on microstructure/property-related failures.
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005591
EISBN: 978-1-62708-174-0
..., wherein an external gas is supplied to shield the arc, and molding shoes are used to confine the molten weld metal for vertical-position welding. This article describes the fundamentals, temperature relations, consumables, metallurgical and chemical reactions, and process development of ESW. The problems...
Abstract
Electroslag welding (ESW) involves high energy input relative to other welding processes, resulting generally in inferior mechanical properties and specifically in lower toughness of the heat-affected zone. Electrogas welding (EGW) is a method of gas metal or flux cored arc welding, wherein an external gas is supplied to shield the arc, and molding shoes are used to confine the molten weld metal for vertical-position welding. This article describes the fundamentals, temperature relations, consumables, metallurgical and chemical reactions, and process development of ESW. The problems, quality control, and process applications of ESW and EGW are also discussed.
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002165
EISBN: 978-1-62708-188-7
... Abstract This article discusses the use of a shaped electrode for electrical discharge machining (EDM). It describes the operational methodology of the EDM. Topography, metallurgical and chemical effects, and surface integrity of the EDM surface are reviewed. The article provides information...
Abstract
This article discusses the use of a shaped electrode for electrical discharge machining (EDM). It describes the operational methodology of the EDM. Topography, metallurgical and chemical effects, and surface integrity of the EDM surface are reviewed. The article provides information on the characteristics of electrodes and the process features of electrode manufacturing. Functions of the dielectric fluids and applications of the EDM are discussed. The article reviews the advancement in EDM such as no-wear EDM and computer numerically controlled vertical EDM. It analyzes the applications and process of the traveling wire EDM. Health and safety measures for the EDM process are also discussed.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003633
EISBN: 978-1-62708-182-5
... Abstract Stress-corrosion cracking (SCC) is a phenomenon in which time-dependent crack growth occurs when the necessary electrochemical, mechanical, and metallurgical conditions exist. This article provides an overview of the environmental phenomenon, mechanisms, and controlling parameters...
Abstract
Stress-corrosion cracking (SCC) is a phenomenon in which time-dependent crack growth occurs when the necessary electrochemical, mechanical, and metallurgical conditions exist. This article provides an overview of the environmental phenomenon, mechanisms, and controlling parameters of SCC. It describes the phenomenological and mechanistic aspects of the initiation and propagation of SCC. The article includes a phenomenological description of crack initiation and propagation that describes well-established experimental evidence and observations of stress corrosion. Discussions on mechanisms describe the physical process involved in crack initiation and propagation. The article also includes information on dissolution models and mechanical fracture models.
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006574
EISBN: 978-1-62708-290-7
... Abstract Ultrasonic additive manufacturing (UAM) is a solid-state hybrid manufacturing technique that leverages the principles of ultrasonic welding, mechanized tape layering, and computer numerical control (CNC) machining operations to create three-dimensional metal parts. This article begins...
Abstract
Ultrasonic additive manufacturing (UAM) is a solid-state hybrid manufacturing technique that leverages the principles of ultrasonic welding, mechanized tape layering, and computer numerical control (CNC) machining operations to create three-dimensional metal parts. This article begins with a discussion on the process fundamentals and process parameters of UAM. It then describes metallurgical aspects in UAM. The article provides a detailed description of a wide range of mechanical characterization techniques of UAM, namely tensile testing, peel testing, and pushpin testing. The article ends with information on sensor embedding.
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001404
EISBN: 978-1-62708-173-3
... Abstract This article presents in-depth metallurgical information about the response of carbon and low-alloy steels to welding conditions and micro-structural evolution in the weld heat-affected zone. It discusses the fabrication weldability and service weldability of carbon and low-alloy...
Abstract
This article presents in-depth metallurgical information about the response of carbon and low-alloy steels to welding conditions and micro-structural evolution in the weld heat-affected zone. It discusses the fabrication weldability and service weldability of carbon and low-alloy steels. The article describes six general classes of the metal: low-carbon steels, high-strength low-alloy steels, quenched-and-tempered steels, heat-treatable low-alloy steels, thermal-mechanical-controlled processing steels, and chromium-molybdenum steels. It concludes with an illustration of steels' susceptibility to hydrogen-assisted cold cracking relative to carbon content and carbon equivalent.
Book: Powder Metallurgy
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006110
EISBN: 978-1-62708-175-7
... various stages of the sintering process and the physical, chemical, and metallurgical phenomena occur within the mass of metal powder particles. It discusses the four advantages of high-temperature sintering of various ferrous PM materials: improved mechanical properties, improved physical properties...
Abstract
High-temperature sintering of ferrous components continues to be important in the powder metallurgy (PM) industry. Improvements in both production rates and properties are possible as sintering temperatures increase above 1120 deg C. This article provides an overview of the different various stages of the sintering process and the physical, chemical, and metallurgical phenomena occur within the mass of metal powder particles. It discusses the four advantages of high-temperature sintering of various ferrous PM materials: improved mechanical properties, improved physical properties, development of liquid phase, and ability to sinter active elements in alloy steels. The article also provides information on three sources of process control requirements, namely, the powder blend, green density, and sintering conditions.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003637
EISBN: 978-1-62708-182-5
... most often reported as being affected by microbiological corrosion are listed, along with the organisms usually implicated in the attack. The article explains that the influence of organisms can be addressed successfully for a corrosion control program by using four types of evidence: metallurgical...
Abstract
This article focuses on the effects of microscopic organisms and the by-products they produce on the electrochemical corrosion of metals. The general characteristics of the microorganisms that facilitate their influence on the electrochemistry of corrosion are discussed. The industries most often reported as being affected by microbiological corrosion are listed, along with the organisms usually implicated in the attack. The article explains that the influence of organisms can be addressed successfully for a corrosion control program by using four types of evidence: metallurgical, microbiological, chemical, and electrochemical. It provides information on the microbiologically influenced corrosion (MIC) of irons and steels, passive alloys (austenitic stainless steels), aluminum alloys, copper alloys, and composites. The article reviews the formation of microbial biofilms and macrofouling films. It also describes the general approaches taken to prevent MIC.
1