Skip Nav Destination
Close Modal
Search Results for
metallizing
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 9127 Search Results for
metallizing
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003022
EISBN: 978-1-62708-200-6
... Abstract The process of coating plastics with metals for functional purposes is called metallizing of plastics. This article discusses the metallizing of plastics, provides information on its history, and gives a short note on applications and adhesion properties of metallic coatings. It also...
Abstract
The process of coating plastics with metals for functional purposes is called metallizing of plastics. This article discusses the metallizing of plastics, provides information on its history, and gives a short note on applications and adhesion properties of metallic coatings. It also discusses the selection of plastics for plating. This article also describes metallizing techniques, including plating (electrolytic or electroplating), vacuum metallizing and thermal spraying, and environmental considerations. The article discusses the quality assurance procedures for metallized plastic parts which include tests that assess the quality of the finish, coating thickness, adhesion, and corrosion resistance, and gives a short note on service performance, which includes service condition classifications.
Image
Published: 01 November 1995
Fig. 2 Common methods of metallizing ceramics. (a) Vacuum evaporation. (b) Sputtering. (c) Screen printing
More
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001348
EISBN: 978-1-62708-173-3
... Abstract This article reviews quantifying adhesion, bonding, and interfacial characterization and strength in a solid-state welding process. It discusses metal-metal configurations and provides information on experimental work carried out in measuring the mechanical properties of interfaces...
Abstract
This article reviews quantifying adhesion, bonding, and interfacial characterization and strength in a solid-state welding process. It discusses metal-metal configurations and provides information on experimental work carried out in measuring the mechanical properties of interfaces based on theoretical analysis. A discussion on the properties affecting adhesion is also provided.
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003554
EISBN: 978-1-62708-180-1
... Abstract Metal-induced embrittlement is a phenomenon in which the ductility or fracture stress of a solid metal is reduced by surface contact with another metal in either liquid or solid form. This article summarizes the characteristics of solid metal induced embrittlement (SMIE) and liquid...
Abstract
Metal-induced embrittlement is a phenomenon in which the ductility or fracture stress of a solid metal is reduced by surface contact with another metal in either liquid or solid form. This article summarizes the characteristics of solid metal induced embrittlement (SMIE) and liquid metal induced embrittlement (LMIE). It describes the unique features that assist in arriving at a clear conclusion whether SMIE or LMIE is the most probable cause of the problem. The article briefly reviews some commercial alloy systems where LMIE or SMIE has been documented. It also provides some examples of cracking due to these phenomena, either in manufacturing or in service.
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006786
EISBN: 978-1-62708-295-2
... Abstract Metal-induced embrittlement is a phenomenon in which the ductility or the fracture stress of a solid metal is reduced by surface contact with another metal in either the liquid or solid form. This article summarizes some of the characteristics of liquid-metal- and solid-metal-induced...
Abstract
Metal-induced embrittlement is a phenomenon in which the ductility or the fracture stress of a solid metal is reduced by surface contact with another metal in either the liquid or solid form. This article summarizes some of the characteristics of liquid-metal- and solid-metal-induced embrittlement. This phenomenon shares many of these characteristics with other modes of environmentally induced cracking, such as hydrogen embrittlement and stress-corrosion cracking. The discussion covers the occurrence, failure analysis, and service failures of the embrittlement. The article also briefly reviews some commercial alloy systems in which liquid-metal-induced embrittlement or solid-metal-induced embrittlement has been documented and describes some examples of cracking due to these phenomena, either in manufacturing or in service.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005192
EISBN: 978-1-62708-187-0
... Abstract This article reviews the solubilities of the common gases present in ferrous metals, such as cast irons, and nonferrous metals, such as aluminum, copper, magnesium, and their alloys. The kinetics of the relevant reactions, reactions during solidification, and possible methods...
Abstract
This article reviews the solubilities of the common gases present in ferrous metals, such as cast irons, and nonferrous metals, such as aluminum, copper, magnesium, and their alloys. The kinetics of the relevant reactions, reactions during solidification, and possible methods of control or removal of the dissolved gases are discussed. The most common method for removing hydrogen from aluminum, copper, and magnesium is inert gas flushing. The article provides information on techniques to overcome gas porosity in ferrous and nonferrous metals.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003086
EISBN: 978-1-62708-199-3
... Abstract Material properties are the link between the basic structure and composition of the material and the service performance of a part or component. This article describes the most significant properties that must be considered when choosing a metal for a given application, namely physical...
Abstract
Material properties are the link between the basic structure and composition of the material and the service performance of a part or component. This article describes the most significant properties that must be considered when choosing a metal for a given application, namely physical properties (mass characteristics and thermal, electrical, magnetic, radiation, and optical properties), chemical properties (corrosion and oxidation resistance) and mechanical properties (tensile and yield strength, elongation, toughness, hardness, creep, and fatigue). The article also contains tables that list room-temperature physical properties, vapor pressures, and mechanical properties for various metals.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003371
EISBN: 978-1-62708-195-5
... Abstract Metallic matrices are essential constituents for the fabrication of metal-matrix composites (MMCs). This article describes three different classes of aluminum alloys, namely, commercial aluminum alloys, low-density and high-modulus alloys, and high temperature alloys. It presents...
Abstract
Metallic matrices are essential constituents for the fabrication of metal-matrix composites (MMCs). This article describes three different classes of aluminum alloys, namely, commercial aluminum alloys, low-density and high-modulus alloys, and high temperature alloys. It presents typical tensile properties and fracture toughness of the selected heat treatable aluminum alloys in a table. Titanium alloys are very attractive for MMC applications, due to their higher strength and temperature capability compared to aluminum alloys. The article tabulates the effect of heat treatment on room-temperature properties and tensile properties of Ti-25Al-17Nb alloy sheet.
Book Chapter
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001087
EISBN: 978-1-62708-162-7
... Abstract Precious metals are of inestimable value to modern civilization. This article discusses the resources and consumption, trade practices, and special properties of precious metals and its alloys, including ruthenium, rhodium, palladium, silver, osmium, iridium, platinum, and gold...
Abstract
Precious metals are of inestimable value to modern civilization. This article discusses the resources and consumption, trade practices, and special properties of precious metals and its alloys, including ruthenium, rhodium, palladium, silver, osmium, iridium, platinum, and gold, and tabulates the industrial applications of precious metals. It provides information on the commercial forms (wire, rod, sheet, strip, ribbon, and foil) and uses of precious metals, including semifinished products, precious metal powders, industrial uses, coatings, and jewelry.
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001119
EISBN: 978-1-62708-162-7
... Abstract Metal contamination of the environment reflects both natural sources and industrial activity, affecting human health. This article begins with a discussion on the level of metal exposure resulting in toxicological effects, the factors influencing toxicity of metals, and carcinogenicity...
Abstract
Metal contamination of the environment reflects both natural sources and industrial activity, affecting human health. This article begins with a discussion on the level of metal exposure resulting in toxicological effects, the factors influencing toxicity of metals, and carcinogenicity of metal compounds. It discusses some commonly used chelating agents for treating metal intoxication, and clinical effectiveness in treating poisoning by different metals. The metals discussed are grouped into four categories: (1) major toxic metals with multiple effects, including arsenic, beryllium, cadmium, chromium, lead, mercury, and nickel; (2) essential metals with potential for toxicity, including cobalt, copper, iron, manganese, molybdenum, selenium, and zinc; (3) metals with toxicity related to medical therapy, including aluminum, bismuth, gallium, gold, lithium, and platinum; and (4) minor toxic metals, including antimony, barium, indium, magnesium, silver, tellurium, thallium, tin, titanium, uranium, and vanadium. The main factors included in the discussion are their disposition, toxicity, biological factors and treatment.
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001095
EISBN: 978-1-62708-162-7
... Abstract Metallic glasses can be prepared by solidification of liquid alloys at cooling rates sufficient to suppress the nucleation and growth of competing crystalline phases. This article presents a historical survey of the study of metallic glasses and other amorphous metals and alloys...
Abstract
Metallic glasses can be prepared by solidification of liquid alloys at cooling rates sufficient to suppress the nucleation and growth of competing crystalline phases. This article presents a historical survey of the study of metallic glasses and other amorphous metals and alloys. This includes a discussion of synthesis and processing methods, structure and morphology, and a description of the electronic, magnetic, thermodynamic, chemical, and mechanical properties of metallic glasses. In addition, the article describes the development of metallic glasses as materials for technical applications.
Book: Powder Metallurgy
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006093
EISBN: 978-1-62708-175-7
... describes the four process groups for the production of open- and closed-pore metal foams. It discusses the principles of the foaminal process with the description of various foaming agents, solidified metal foam, and geometries and derived structures of metal foams. The use of syntactic metal foam...
Abstract
Cellular or foam structures can be described by means of two broader cases: foams in which the pores are all connected to each other and with the environment (open-pore foams) and foams in which every single pore is completely enclosed by the matrix (closed-pore foams). This article describes the four process groups for the production of open- and closed-pore metal foams. It discusses the principles of the foaminal process with the description of various foaming agents, solidified metal foam, and geometries and derived structures of metal foams. The use of syntactic metal foam in various fields is included. The article reviews the mechanical properties of closed-pore metal foams, details the machining and joining procedures of the metal foams, and presents the applications of the metal foam.
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003776
EISBN: 978-1-62708-177-1
... Abstract This article explains how to prepare precious metal test samples for metallographic examination. It discusses cutting, mounting, grinding, polishing, and etching and addresses some of the challenges of working with small, relatively soft specimens. It includes dozens of example...
Abstract
This article explains how to prepare precious metal test samples for metallographic examination. It discusses cutting, mounting, grinding, polishing, and etching and addresses some of the challenges of working with small, relatively soft specimens. It includes dozens of example micrographs, comparing and contrasting the microstructural features of gold, platinum, iridium, palladium, and ruthenium-base alloys. It examines pure gold, intermetallic gold compounds, gold and platinum jewelry alloys, platinum-containing shape memory alloys, and alloys consisting of platinum, aluminum, and copper.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005224
EISBN: 978-1-62708-187-0
... Abstract Semisolid metal (SSM) processing is a special die casting process, where partially solidified metal slurry is injected into a die cavity to form die cast components. This article discusses the flow behavior of an SSM slurry with emphasis on viscosity, rheological behavior, and yield...
Abstract
Semisolid metal (SSM) processing is a special die casting process, where partially solidified metal slurry is injected into a die cavity to form die cast components. This article discusses the flow behavior of an SSM slurry with emphasis on viscosity, rheological behavior, and yield stress. It illustrates the microstructural formation of semisolids under forced convection. The article concludes with an illustration that compares two SSM processes, namely, thixocasting and rheocasting.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005351
EISBN: 978-1-62708-187-0
... the factors that influence the formation of inclusions. The article describes the three basic methods of mechanically removing or separating inclusions from molten metal. The methods include sedimentation, flotation, and positive filtration. The article provides a discussion on the types of molten-metal...
Abstract
In the handling of molten aluminum, it is fairly common to use filters as a part of the melting unit and in the gating and/or riser system. This article describes the methods of in-furnace and in-mold filtration, with an emphasis on the filtration of molten aluminum. It discusses the factors that influence the formation of inclusions. The article describes the three basic methods of mechanically removing or separating inclusions from molten metal. The methods include sedimentation, flotation, and positive filtration. The article provides a discussion on the types of molten-metal filters, including bonded-particle filters, cartridge filters, and ceramic foam filters. It lists the factors that are important in achieving optimum performance of any in-furnace filtering application. The article concludes with information on filtered metal quality and the methods of evaluation.
Book Chapter
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003721
EISBN: 978-1-62708-177-1
... Abstract This article provides information on the general structural features and origins of metals. The characteristic structural features of single-phase metals and alloys, such as grain structure and substructure, are discussed. The article also describes the major types of multiphase...
Abstract
This article provides information on the general structural features and origins of metals. The characteristic structural features of single-phase metals and alloys, such as grain structure and substructure, are discussed. The article also describes the major types of multiphase structures and macrostructure of metals and alloys.
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002189
EISBN: 978-1-62708-188-7
... Abstract This article focuses on the machining of reactive metals which refer collectively to the elements titanium, hafnium, and zirconium. It provides guidelines for machining titanium and titanium alloys and describes machining operations, such as turning, milling, drilling, tapping, reaming...
Abstract
This article focuses on the machining of reactive metals which refer collectively to the elements titanium, hafnium, and zirconium. It provides guidelines for machining titanium and titanium alloys and describes machining operations, such as turning, milling, drilling, tapping, reaming, grinding, and sawing, performed on titanium and its alloys. The article also provides information on electrochemical machining (ECM), chemical milling (CHM), and laser beam machining (LBM) for titanium and titanium alloys. Guidelines for machining zirconium alloys and hafnium are also provided. The article provides a short description of turning, milling, and drilling operations performed on zirconium alloys and hafnium. It also discusses health and safety considerations related to zirconium and hafnium.
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002190
EISBN: 978-1-62708-188-7
... Abstract This article describes various machining techniques of refractory metals, namely, niobium, molybdenum, tantalum, and tungsten. These include turning, boring, trepanning, reaming, milling, tapping, drilling, and sawing. Parameters for the machining of the refractory metals are also...
Abstract
This article describes various machining techniques of refractory metals, namely, niobium, molybdenum, tantalum, and tungsten. These include turning, boring, trepanning, reaming, milling, tapping, drilling, and sawing. Parameters for the machining of the refractory metals are also tabulated. In addition, the article provides information on cutting fluids and tools that are used in machining of the refractory metals as well as on the safety precautions to be followed in the machining process.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003181
EISBN: 978-1-62708-199-3
... Abstract This article provides a detailed account on forming operations (blanking, piercing, press-brake forming, contour rolling, deep drawing, cold forming, and hot forming) of various nonferrous metals, including aluminum alloys, beryllium, copper and its alloys, magnesium alloys, nickel...
Abstract
This article provides a detailed account on forming operations (blanking, piercing, press-brake forming, contour rolling, deep drawing, cold forming, and hot forming) of various nonferrous metals, including aluminum alloys, beryllium, copper and its alloys, magnesium alloys, nickel alloys, titanium alloys, and platinum metals. It discusses the formability, equipment and tooling, and lubricants used in the forming operations of these nonferrous metals.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003150
EISBN: 978-1-62708-199-3
... Abstract Precious metals include gold, silver, and six platinum-group metals, namely, platinum, palladium, ruthenium, rhodium, osmium, and iridium. This article focuses on the consumption, trade practices, properties, product forms, and applications of these metals and their alloys. gold...
1